0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Formula | Oxide Interaction | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Wood Ash Glaze

Common washed wood ash can supply important ceramic oxides when melted, so it can comprise significant percentages in a recipe. Plus it can produce unique visual effects.

Key phrases linking here: wood ash glazes, wood ash glaze, ash glazes, ash glaze - Learn more

Details

A glaze that employs organic ash (e.g. paper, wood) as a supplier of basic oxides (especially CaO, K2O, Na2O). Ashes are generally flaky and fibrous and cannot be screened well, this consistency contributes to variegation in the color and texture of the fired surface. Without large batches of consistent ash to draw on repeatability is poor, so this type of glaze is mostly most suitable for potters who are willing to develop and tune recipes for each batch of ash.

Many pottery books and websites deal with the preparation (washing) of wood ash. It can be difficult to separate the ash from the unburned material so it may be necessary to calcine or even ball mill it. Most practitioners consider ash glazes decorative and do not use them on functional ware, they thus are prepared to tolerate poor working properties and inconsistent results. However, our approach is to use enough ash to get an earthy appearance but not so much that a glaze is no longer functional or easily usable.

Many recipes online call for "wood ash". But there is a problem with this. The chemistry of different organic ash types varies dramatically. But also for different batches of the same wood. And, more often than not, the type of wood is not even known. Or, it is a mix. If a recipe only calls for a small percentage of wood ash (e.g. less than 10%) this might not be a problem. But for larger percentages, the chances of your recipe firing the same as the pictures shown is very low.

The unique nature of ash compared to ceramic materials requires a different approach to glaze making. Generally, the aim is to develop a recipe using the highest practical percentage of a batch of ash that you have accumulated, blended and processed (the larger the batch the better). Ash is most often high in CaO, so it makes little sense to employ calcium carbonate or wollastonite in the recipe. At the chemistry level, a typical ash contains no Al2O3 and little SiO2, the two most important oxides in a glaze. The most common ceramic materials that supply these are kaolin and feldspar so they are the natural companions in a recipe. In the past, it was common to also add Gerstley Borate to help melting and suspension, but it has almost no Al2O3 or SiO2 - it is thus better to use a balanced frit that supplies both (meaning Ferro Frit 3134 is not suitable). The higher the ash percentage the thicker the slurry will be and the more water it will require (and the more the problem with drying shrinkage and cracking) - a conservative approach might be to settle for a lower percentage of ash in the recipe (e.g. 35-40%). A higher kaolin percentage should produce a better slurry rheology. Adding CMC gum can also help with adherence and drying issues. Some ashes have significant Na2O, this will be evident if the glaze crazes - in these cases substitute as much of the feldspar for a frit as possible. The only case where silica should be needed is if a combination of over-melting and crazing happens.

All of the pieces shown here were made by Tony Hansen, they demonstrate what is possible in formulating ash glaze recipes. This can be a very rewarding experience, especially when you learn to recognize what material(s) need to be added or substituted to improve the appearance or performance.

Related Information

A starter recipe for a brown wood ash glaze for cone 6


A basic brown wood ash glaze for cone 6

This picture has its own page with more detail, click here to see it.

It makes sense to maximize the percentage of wood ash. This glaze was the product of preparing a large ash batch and a project to develop a glaze specifically from it (this is important because every batch of ash is different). This recipe contains ~2% iron oxide. Wood ash generally contains very little Al2O3, a critical oxide needed for stable glass development. I thus added 20% EP kaolin (any kaolin should work), it supplies the Al2O3 and suspends the slurry. The ash usually contains lots of fluxing oxides, but it still needs help to melt a glaze at cone 6 (so add 30% feldspar, it also supplies more of the critical Al2O3). For better melting consider substituting some of the feldspar with an Al2O3-containing borax frit (like Ferro frit 3195, even better, frit 3249 since it will prevent crazing). To ease development it is often easier to add more powdered materials to an existing slurry (e.g. it is likely that more frit will be needed), this will push down the total percentage of ash possible in the recipe - thus I often end of with 40% ash.

Cone 6 bowl demonstrates a starter wood ash glaze recipe


Basic wood ash glaze recipe

This picture has its own page with more detail, click here to see it.

A wood ash glaze is not generally something you mix from a recipe. It is something you develop from a batch of ash (see the article below for more information). This ash glaze contains no iron but does have a little cobalt (about 0.25%). The ash is about 50%, with 20% EP kaolin, 20% Custer feldspar and a little rutile (2-4%). If your attempted glaze does not melt well enough consider substituting some of the feldspar for balanced boron frit. If it melts too much and crazes add some silica at the expense of the feldspar.

Plainsman M332 vase with a wood ash glaze fired at cone 6.


Wood ash glazed vase

This picture has its own page with more detail, click here to see it.

The pattern was painted using wax resist, and the glaze was applied by pouring. This recipe was the product of multiple previous versions and experience in learning how to process wood ash to a finer particle size and host it in a recipe that melted to the right degree. This glaze fired to such a good surface that it was suitable for functional ware. These were among Tony's earliest successes in formulating glazes, hundreds of pieces grew from this. M332 is a coarse-particled clay body and most glazes pinhole on it if not slow-cooled. Yet these ash glazes produced defect-free surfaces (albeit with plenty of variegation from the impurities intrinsic to the material). Electric kilns began taking pottery by storm in the 1970s and he often tested them with the largest possible pieces.

Cone 6 oxidation wood ash glazed vase


This picture has its own page with more detail, click here to see it.

I always put the emphasis on ash glazes with functional surfaces, well melted, uncrazed and resistant to staining or cutlery marking. This version gets its color only from rutile. The glaze creates a more decorative surface when applied thinner (like the inside of this small vase). When thicker the surface is functional (like the outside surface). Ash glazes can be very stable (resistant to running during firing) if they contain enough Al2O3 (mainly from the kaolin) but also from the feldspar.

Cone 8 oxidation wood ash glazed planter by Tony Hansen


This picture has its own page with more detail, click here to see it.

H463 with a wood ash glaze. This cone 6 glaze was fired to cone 8 to make these pieces. The higher temperature produced more melt fluidity and variegation in this rutile and cobalt version of a wood ash recipe. A thicker application on the outside caused cracking during drying, that produced crawling that added to the aesthetic.

Inbound Photo Links



Pottery made from cremation ash, increasingly popular!

Links

Materials Rice Straw Ash
A type of plant ash sometimes used as an ingredient in pottery glazes.
Materials Rice Husk Ash
A type of plant ash used as an ingredient in pottery glazes.
Materials Pine Wood Ash
A type of wood ash used as an ingredient in pottery glazes.
Materials Oakwood Ash
A type of wood ash used as an ingredient in pottery glazes.
Materials Hardwood Ash
A type of wood ash used as an ingredient in pottery glazes.
Materials Eucalyptus Ash
A type of wood ash used as an ingredient in pottery glazes.
Materials Applewood Ash
A type of wood ash used as an ingredient in pottery glazes.
Materials Wood Ash
For centuries, pottery glazes have been made from ash mostly mixed with clay and feldspar.
Materials Volcanic Ash
Powdered volcanic ash is used to make ceramic glazes, some varieties have a chemistry similar enough to glaze that high percentages can be employed.
Materials Soft Wood Ash
A type of wood ash used as an ingredient in pottery glazes.
Glossary Ceramic Glaze
Ceramic glazes are glasses that have been adjusted to work on and with the clay body they are applied to.
Hazards Plant Ash Toxicity
The hazards of using plant and wood ash in ceramic glazes
Articles Chemistry vs. Matrix Blending to Create Glazes from Native Materials
Is it better to do trial and error line and matrix blending of materials to formulate glazes or is it better to use glaze chemistry right from the start?

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy