0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Formula | Oxide Interaction | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Toxicity

Common sense can be applied to the safe use of ceramic materials. The obvious dangers are breathing the dust and inhaling the fumes they produce during firing. Here is a round-up of various materials and their obvious hazards.

Key phrases linking here: toxicity - Learn more

Details

Are you getting suspicious that lawyers write most of the labels that now appear on material packages? Do all the labels look the same? How does one pick out the materials that are the most dangerous when materials thought to be safe are labelled in the same way as the toxic ones? Warnings have lost much of their impact, at times to the point of being ridiculous.

Material Safety Datasheets that outline hazards associated with coming into contact with the material itself, and while these have the same general format, there is a tremendous variety with reference to the information they volunteer, the hazards detail provided, and the degree of harmony between like materials. The average user is overwhelmed by all of these sheets, and reading them tends to make us cynical about how real the warnings are. In addition, these sheets have nothing to do with the safety issues surrounding the functional use of glazes made using the materials.

In recent years the subject of material safety and possible safety issues surrounding the functional use of glazed ware with food and drink have become a hot topic on the Internet, in the press, and within educational institutions. There are people putting their heart and soul into trying to educate us about the hazards of many ceramic materials. At the same time, there are many, including authors and people of repute, paying absolutely no attention and making glazes from whatever materials and whatever proportions they please. And firing them in unventilated kilns in confined work areas! There are some who argue strenuously to defend the use of known poisons and carcinogens because we can't come up with hard data to prove that anyone is being affected by them. There are others campaigning against ceramics in schools and universities, claiming it is just too dangerous.

Surely there is some middle ground we can reach. I feel the position is best expressed by Monona Rossol, an author, chemist, potter, and activist who summarized two decades of selfless dedication to this issue on many levels by calling herself an 'industrial hygienist for the arts, crafts, and theatre'. She speaks of the 'ethical' use of materials and formulations. This approach strikes a chord with many who have seen so many cases where the supposed know-it-alls claim total understanding of things and kick down "caution signs" under the banner that no one can produce hard data to justify their existence. Ethical use of materials means we err on the side of safety and the prevailing common sense, and are less swayed by those with hidden agendas and conflicts of interest. If a material like barium, for example, is surrounded in controversy, then glazes that employ it are 'controversial' glazes. Do you suppose anyone would buy your ware if there was a hang-tag on it explaining that industry experts are currently embroiled in heated disputes over an ingredient's safety?

Finished Product Quality

Is the user of your pottery in danger from food or drink dissolving toxic compounds from the glaze surface, from micro-organisms that the glaze surface might provide a home for, or from actually swallowing a chip of the glaze that has flaked off the surface? This site has lots of information to help you make your products safe for the end-user, it does not require an engineer. There are some really bad glazes out there, we can help you recognize them.

Is Your Working Space Safe?

Silica is likely the most dangerous material used in ceramics since silicosis is the most common ceramic material-related health-effect in production workers. Workers in the industry are routinely screened for lung function for this specific danger. Silica itself is clearly not a poison, you can eat it with no problems. But quartz crystals can lodge themselves deeply in the air pocket of the lungs so breathing a lot of it is obviously not good. But remember, quartz is the most abundant mineral in nature. Gravel, concrete, asphalt, garden soil, etc are all loaded with quartz. So the minimization of dust is a key component to a safe workplace.

Kiln fumes are also obviously potentially hazardous, they need to be vented outside or kilns need to be in a separate room. Many materials can produce fumes that are toxic, the danger increases exponentially with firing temperature. Be most wary of decomposing metal oxides (e.g. manganese, cobalt), generally, the use of ceramic stains is much safer.

Material Safety

There are many articles on material safety on this website. You can find a list of all of these by searching for the word "toxicity" or "safety" (on the home page or in the glossary or articles section).

As a quick overview, the following are some general comments. Keep in mind that when I say a material is not generally harmful, I mean in the quantities a person would be exposed to in a clean typical working environment. Also, this page is not dealing with the contribution any material might make to a glaze containing (leaching hazard of toxins into food and drink), that is a matter to understand at the glaze chemistry level (unbalanced glazes that release toxic metals can be made from any materials).

Related Information

A practical dust box may be better than a dust hood


A dust removal box

This picture has its own page with more detail, click here to see it.

An example of a custom-made dust collection hood in our repackaging and lab recipe mixing area. The slots along the front suck particles into the duct directly away from the operator's face. Suction comes from a centrifugal exhaust fan downstream where the pipe exits the building, it is driven by a 3/4hp motor (these fans are best at sucking, not blowing, so they need to be located at the exit). About 40 feet of 8-inch heating pipe connects from the hood to a fitting that expands to 12 inches going into the fan. The sliding damper above the hood enables stopping all airflow (to prevent heat loss during cold days). Notice it is located above the scale and heat sealer where most dust is generated during weighing and packaging.

Frits instead of raw zinc, lithium, barium, strontium


zinc, lithium, barium, strontium oxide powders

This picture has its own page with more detail, click here to see it.

Raw material sources of zinc, lithium, barium, strontium have issues (e.g. precipitates in glaze slurries, toxicity, high drying shrinkage and carbon burnoff that affect laydown and fired surface defects like pinholes, blisters, orange peeling, crystallization). Yet the oxides that these materials supply to the glaze melt - ZnO, Li2O, BaO and SrO, can be sourced from frits which melt much better and remove most of the problems. Consider examples made by Fusion:
-Frit F-493 has 11% Li2O
-F-403 has 35% BaO
-F-581 has 39% SrO
-FZ-16 has 15% ZnO
These frits source other oxides but such are common in most glazes and glaze calculation can be used to retain the overall chemistry. Although these are expensive, the benefits are game changers. But there is a problem: Potters can't get these. Therefore they have difficulty creating the dazzling visual effects of many commercial glazes.

Sedimentary clays are a whos-who of the periodic table


This picture has its own page with more detail, click here to see it.

These are the results of a detailed elemental composition analysis of a sedimentary clay. The first column of numbers is ppm (parts per million), divide them by 10,000 to get percent. The Fe here, for example, is 50,868 or 5.1%. The second column is +/- error. Notice that this test does not detect boron or lithium, they require a different method. By contrast, the chemical analysis shown on the data sheet of a typical ceramic material shows only the principle ceramic oxides (less than a dozen), but all of these trace elements will still be present.

N95 Particulate Respirator mask


This picture has its own page with more detail, click here to see it.

This designation is an international standard for a general purpose respirator to filter out respirable quartz particles (which cause silicosis). Use one of these when working in a area where ventilation is insufficient to remove all of the dust. Use it also in circumstances where there is temporary generation of large quantities of dust. Do not wear this as a substitute for keeping floors and working areas clean.

Stains are better in black DIY glazes

Use 5% stain instead of 15% metal oxides


Make your own black glaze

This picture has its own page with more detail, click here to see it.

Consider the hazards and hassles before choosing a black matte or gloss recipe that has high individual or combined percentages of manganese dioxide, cobalt or nickel.

Gloss blacks: These are super popular as the base for layering of reactive glazes. DIY dipping versions thus make a lot of sense. They make even more sense when they don’t turn to jelly in the bucket because of the high percentage of red iron oxide in all blacks made using metal oxide colorants. And when the total percentage of pigment is as high, or higher than 15%. And when the pigments cause crystallization (especially when overloaded).

Matte blacks: The human eye can detect even slight differences in the degree of matteness (which is very difficult to keep consistent). Raw metal oxides affect the matteness, especially when overloaded with pigment. They are prone to cutlery marking if too matte. By using stains, manufacturers and even potters have learned to tune recipes (lower left) and firing schedules to achieve consistency and functionality (even tourist souvenirs (lower right) feature them now). With stains, only one material is producing the color, its percentage (which can be as low as 4%) can be tuned.

Links

Glossary Leaching
Ceramic glazes can leach heavy metals into food and drink. This subject is not complex, there are many things anyone can do to deal with this issue
Hazards Manganese in Clay Bodies
Manganese is used to stain clays (using black) and to impart fired speckling (as a decorative effect). It is dangerous?
Hazards Overview of Material Safety by Gavin Stairs
Toxicology and ceramic materials is a complex subject, what materials and methods pose the greatest dangers, which are the safest?
Articles Crazing and Bacteria: Is There a Hazard?
A post to a discussion on the clayart group by Gavin Stairs regarding the food safety of crazed ware.
Articles Attack on Glass: Corrosion Attack Mechanisms
Max Richens outlines the various mechanisms by which acids and bases can dissolve glass and glazes. He provides some information on stabilizing glazes against attack.
Articles Is Your Fired Ware Safe?
Glazed ware can be a safety hazard to end users because it may leach metals into food and drink, it could harbor bacteria and it could flake of in knife-edged pieces.
Articles Are Your Glazes Food Safe or are They Leachable?
Many potters do not think about leaching, but times are changing. What is the chemistry of stability? There are simple ways to check for leaching, and fix crazing.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 