Alumina Toxicology | Ammonia and Latex Toxicity | Antimony Oxide | Are colored porcelains hazardous? | Arsenic Oxide | Asbestos Toxicity | Ball Clay | BARIUM and COMPOUNDS Toxicology | Barium Carbonate in Clay Bodies | Barium Carbonate in Glazes | Bentonite Toxicity | Beryllium Monoxide Toxicology | Bismuth Trioxide Toxicology | Boron Compounds and Their Toxicity | Brown Stain | Cadmium Toxicity | Calcium Carbonate Toxicology | Carbon Monoxide Toxicity | Cesium Toxicology | Chromium Compounds Toxicology | Clay Toxicity | Cobalt Oxide and Carbonate | Cobalt Toxicology | Copper Compounds Toxicology | Copper Oxide and Carbonate | Cristobalite Toxicity | Cryolite and Ceramics | | Diatomaceous Earth Toxicology | Dioxins in Clays | Epsom Salts | Eye Injuries Due to Radiation | Feldspar | Fighting Micro-Organisms in Ceramics | Fluorine Gas | Fumes from gas kilns | Gallium Oxide Toxicology | Hafnium Oxide Toxicty | Hydrofluoric Acid Toxicity | Iron oxide and Hematite | Lead Chromate | Lead in Ceramic Glazes | Lead Toxicology | Lithium Carbonate Toxicity | Lithium Toxicology | Man-Made Vitreous Fibers (MMVF) Toxicology | Man-Made Vitreous Fibers Safety Update | Manganese and Parkinsons by Jane Watkins | Manganese in Clay Bodies | Manganese Inorganic Compounds Toxicology | Manganese Toxicity by Elke Blodgett | Manganese: Creativity and Illness by Dierdre O'Reilly | Molybdenum Compounds Toxicology | Nickel Compounds Toxicity | Niobium Oxide Toxicity | Occupational Dermatoses | Overview of Material Safety by Gavin Stairs | Paraffin Toxicology | Perlite Toxicity | Plant Ash Toxicity | Potassium Carbonate Toxicity | Pregnancy and Ceramics | Propane Toxicology | Quartz Toxicity | Quartz Toxicity on Clayart | Rare Earth Compounds Toxicity | Rubidium and Cesium Toxicology | Rutile Toxicology | Silicosis and Screening | Silver Compounds Toxicology | Sodium Azide Toxicology | Sodium Carbonate Toxicology | Sodium Silicate Powder Toxicology | Stannous Chloride Toxicity | Strontium Carbonate Toxicity Note | Sulfur Dioxide Toxicity | Talc Hazards Overview | Talc Toxicology | Thallium Oxide Toxicology | Thorium Dioxide Toxicity | Tin Inorganic Compounds | Titanium Dioxide Toxicology | Toxicological Assessment of Zeolites | Tungsten Compounds Toxicology | Understanding Acronyms on MSDS's | Uranium and Ceramics | Vanadium and Compounds Toxicology | Vermiculite | Zinc Compounds Toxicology | Zirconium Compounds Toxicity | Zirconium Encapsulated Stains Toxicity

Dealing With Dust in Ceramics

Indoor air pollution of all types is considered one of the most important health hazards of our time. The dramatic rise in the incidence of Asthma is said to be evidence of this. Ceramic arts, crafts, production and lab testing can generate significant dust if it is not managed properly. Ceramic educational programs can come under scrutiny because of dust concerns. Here are suggestions to reduce your exposure and make your workplace safe.

Common Sense

Did You Know?

Good Habits

Workarea Improvements

Other Suggestions:

Success? Gauge your progress by turning out the lights and shining a strong flashlight across the room. Or by how many times your air quality monitor triggers.


By Tony Hansen
Follow me on

Related Information

Chronic exposure to this causes silicosis


This picture has its own page with more detail, click here to see it.

It is high-level exposure to this kind of dust for many years without adequate protection that causes silicosis. The levels of dust in a typical well-maintained and clean pottery studio come nowhere close to this.

A material storage rack


This picture has its own page with more detail, click here to see it.

This material storage area employs a rack to keep pails off the floor so the area can be hosed down easily. The materials in each pail are sealed in plastic bags or the pail is covered with a lid.

A practical dust box may be better than a dust hood


A dust removal box

This picture has its own page with more detail, click here to see it.

An example of a custom-made dust collection hood in our repackaging and lab recipe mixing area. The slots along the front suck particles into the duct directly away from the operator's face. Suction comes from a centrifugal exhaust fan downstream where the pipe exits the building, it is driven by a 3/4hp motor (these fans are best at sucking, not blowing, so they need to be located at the exit). About 40 feet of 8-inch heating pipe connects from the hood to a fitting that expands to 12 inches going into the fan. The sliding damper above the hood enables stopping all airflow (to prevent heat loss during cold days). Notice it is located above the scale and heat sealer where most dust is generated during weighing and packaging.

N95 Particulate Respirator mask


This picture has its own page with more detail, click here to see it.

This designation is an international standard for a general purpose respirator to filter out respirable quartz particles (which cause silicosis). Use one of these when working in a area where ventilation is insufficient to remove all of the dust. Use it also in circumstances where there is temporary generation of large quantities of dust. Do not wear this as a substitute for keeping floors and working areas clean.

Crystalline silica warning on a box of clay:

React instead of overreacting.


Crystalline silica warning on a box of clay

This picture has its own page with more detail, click here to see it.

Like any dirt, clays contain quartz. Quartz particles are all around us, the mineral makes up about 12 percent of the land surface and about 20 percent of the Earth's crust. It is impossible to get away from quartz particles (e.g. road and street dust are common sources). Farmers and construction workers are constantly exposed to it. Quartz inhalation is a hazard when:
1. Inhaled particles are just the right size to block the tiny air passages in the lungs.
2. Chronic exposure over a long period occurs (or shorter exposure to high concentrations).
Since you don't know the particle size of any dust, it is only sensible to take precautions against #2. We do know that respirable particles that can get stuck in the lungs are <5 microns. Clay powders used in ceramics are typically ground to 75 microns, far larger. However, that processing does produce lots of finer sizes also, so there is good reason to keep dust down. Specifics about the hazards of powders used in ceramics are available on SDSs (Safety Data Sheets).

Links

Materials Silica
Silica, sold as a white powder, is pure quartz mineral. Quartz is pure SiO2 silicon dioxide. It is the most abundant mineral on earth and most used in ceramics.
Materials Ball Clay
A fine particled highly plastic secondary clay used mainly to impart plasticity to clay and porcelain bodies and to suspend glaze, slips and engobe slurries.
URLs https://www.consumernotice.org/environmental/silica-dust/
Silica Dust information from consumernotice.org, a site created by legal professionals, accomplished medical providers, product safety specialists and patient advocates.
URLs https://www.amazon.ca/Quality-Monitor-Detector-Readings-Pollution/dp/B08M6F57PN
Air quality monitoring device on Amazon
Measures tiny particulate in micron respirable sizes.
URLs https://www.amazon.ca/ABEST-Portable-Airbrush-Painting-Extension/dp/B01HZ1HDF6
Portable airbrush spray booth on Amazon
For possible use as a dust box or dust hood in a ceramic studio.
Minerals Quartz
Quartz is the most abundant mineral on earth, it is the main crystalline mineral form of silica (SiO
Glossary Powder Processing
An entire industry is dedicated to the science, materials and equipment associated with the creation, processing and handling of powders.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy