Alumina Toxicology | Ammonia and Latex Toxicity | Antimony Oxide | Are colored porcelains hazardous? | Arsenic Oxide | Asbestos Toxicity | Ball Clay | BARIUM and COMPOUNDS Toxicology | Barium Carbonate in Clay Bodies | Barium Carbonate in Glazes | Bentonite Toxicity | Beryllium Monoxide Toxicology | Bismuth Trioxide Toxicology | Boron Compounds and Their Toxicity | Brown Stain | Cadmium Toxicity | Calcium Carbonate Toxicology | Carbon Monoxide Toxicity | Cesium Toxicology | Chromium Compounds Toxicology | Clay Toxicity | Cobalt Oxide and Carbonate | Cobalt Toxicology | Copper Compounds Toxicology | Copper Oxide and Carbonate | Cristobalite Toxicity | Cryolite and Ceramics | Dealing With Dust in Ceramics | Diatomaceous Earth Toxicology | Dioxins in Clays | Epsom Salts | Eye Injuries Due to Radiation | Feldspar | Fighting Micro-Organisms in Ceramics | Fluorine Gas | Fumes from gas kilns | Gallium Oxide Toxicology | Hafnium Oxide Toxicty | Hydrofluoric Acid Toxicity | Iron oxide and Hematite | Lead Chromate | Lead in Ceramic Glazes | Lead Toxicology | Lithium Carbonate Toxicity | Lithium Toxicology | Man-Made Vitreous Fibers (MMVF) Toxicology | Man-Made Vitreous Fibers Safety Update | Manganese and Parkinsons by Jane Watkins | Manganese in Clay Bodies | Manganese Inorganic Compounds Toxicology | Manganese Toxicity by Elke Blodgett | Manganese: Creativity and Illness by Dierdre O'Reilly | Molybdenum Compounds Toxicology | Nickel Compounds Toxicity | Niobium Oxide Toxicity | Occupational Dermatoses | Overview of Material Safety by Gavin Stairs | | Perlite Toxicity | Plant Ash Toxicity | Potassium Carbonate Toxicity | Pregnancy and Ceramics | Propane Toxicology | Quartz Toxicity | Quartz Toxicity on Clayart | Rare Earth Compounds Toxicity | Rubidium and Cesium Toxicology | Rutile Toxicology | Silicosis and Screening | Silver Compounds Toxicology | Sodium Azide Toxicology | Sodium Carbonate Toxicology | Sodium Silicate Powder Toxicology | Stannous Chloride Toxicity | Strontium Carbonate Toxicity Note | Sulfur Dioxide Toxicity | Talc Hazards Overview | Talc Toxicology | Thallium Oxide Toxicology | Thorium Dioxide Toxicity | Tin Inorganic Compounds | Titanium Dioxide Toxicology | Toxicological Assessment of Zeolites | Tungsten Compounds Toxicology | Understanding Acronyms on MSDS's | Uranium and Ceramics | Vanadium and Compounds Toxicology | Vermiculite | Zinc Compounds Toxicology | Zirconium Compounds Toxicity | Zirconium Encapsulated Stains Toxicity

Paraffin Toxicology

INDENTIFICATION :

CAS number : 8002-74-2

MAIN SYNONYMS :

French names :
Paraffine, cire de (fumées)
CIRE DE PARAFFINE
FUMEE DE PARAFFINE
English names :
Paraffin wax, fume
HARD PARAFFIN

USES AND SOURCES OF EMISSION :

Manufacture of cosmetics, as a sealing agent, in ceramics

HYGIENE ET SAFETY :

I. Appearance :

Solid, colourless to white, odourless

II. Physical and Chemical Properties :

Odor : None
Physical state : Solid at 25 °C
Vapor pressure : < 0.01 at 25 °C
Vapor density (air =1) : > 5
Boiling point : > 300 °C
Solubility in water (20°C) : < 0.1%
Evaporation rate (Butyl Acetate =1) : < 0.01
Freezing point : Not applicable
Volatiles (By volume) : < 1.0%
Specific density (25°C) : 0.90-0.93
Melting point : 45-100 °C
III. Inflammability and Explosiveness :
A. Inflammability :
This product is flammable under the following conditions : it can ignite if it is strongly heated and in the presence of a source of ignition.
B. Data on fire hazards :
Flash point : 199,00 °C, closed cup
T° of auto-ignition : 245 °C.
C Sensitivity to shocks :
This product is not sensitive to shocks.
D. Techniques and means of extinction :
Means of extinction:
- carbon dioxide
- foam
- dry chemical powder
- sprayed water
- alcohol foam
E. Additional information :
Cool the containers exposed to fire with water.
F. Special techniques :
Wear an autonomous respiratory apparatus.
G. Products of dangerous decomposition :
Carbon monoxide, carbon dioxide and other products such as aldehydes and ketones according to the oxidation state, aldehydes being able to be very irritating.

PREVENTION :

I. Storage :
Store in a cool place, away from any source of ignition, sheltered from oxidizing materials, acids and bases.

II. Exposure Control/Personal Protection :
This material will be used in the molten form. Protective clothing against splashes, thermal gloves, and ocular protection must be worn to prevent wounds.
Use the melted material in well ventilated sectors. While working in confined areas, use suitable respiratory protection.

III. Leaks :
Handle as a thermoplastic product. At the time of leaking of the melted material, allow the product to solidify and cool. Keep the material out of sewers and rivers by diking. Recover and place in suitable containers for re-use or disposal, according to local laws.

IV. Waste Disposal :
Consult local authorities.

TOXICOLOGY :

I. Experimental Toxicology :
In the rat, chronic ingestion showed its accumulation in certain target organs, such as the liver and spleen, associated with nonspecific immune response.

II. Absorption :
This product is absorbed by the respiratory tract.

III. Acute Effects :

A. Inhalation :
If heated it emits paraffin wax fumes :
- possible irritation of the eyes and the respiratory tract, more particularly in sensitive
individuals
- nausea.
B. Skin :
Contact with molten wax can cause serious burns.
C. Eyes :
Direct ocular contact of the melted product with the eyes can cause thermal burns and ocular lesions. Fumes and vapors coming from the thermal decomposition of paraffin wax can cause irritation of the eyes.
D. Ingestion :
This product is primarily inert and non poisonous. However, one must handle it carefully, do not ingest or put some in your mouth.

IV. Chronic Effects :
Inhalation of aerosols (if heated) :
- cough
- sputum production
- exertional shortness of breath
- possibility of pulmonary damage (lipoidic pneumonia)
- alveolitis and interstitial fibrosis.

V. Pregnancy :

A. Effects on development :
No data concerning antenatal development was found in the consulted documentary sources.
B Effects on the reproduction :
No data concerning reproduction was found in the consulted documentary sources.
C Data on the mother's milk :
There is no data concerning excretion or detection in mother's milk.

VI. Carcinogenic Effects :
The available data do not make it possible to make an adequate evaluation of the carcinogenic effect.

VII. Mutagenic Effects :
No data concerning a mutagenic in vivo or in vitro effect on cells of mammals was found in the consulted documentary sources.

FIRST AID :

I. Inhalation :
In the event of inhalation of fumes or vapors, bring the person into a well ventilated place. If he does not breathe, give him artificial respiration. Call a doctor.

II. Eyes :
Exposure to fumes and vapors of overheated paraffin can cause irritation of the eyes. Direct contact with molten paraffin wax can cause ocular damage and burns. At the time of the handling of molten wax, one should carry ocular protection at any time. If an accident occurs, wash the eyes with plenty of water during at least 15 minutes, call a doctor to take care of the wound.

III. Skin :
Exposure to fumes and vapors coming from the thermal degradation of the product can cause irritation of the skin. Direct contact with the molten product can cause burns. In the case of burns, wash the affected area with large amounts of water for 15 minutes. Do not try to remove the material fixed on the skin. Call a doctor to take care himself of the wound.

IV. Ingestion :
Is not an acute poison by ingestion. In the event of ingestion, do not induce vomiting, call a doctor.

EXPOSURE LIMIT IN QUEBEC :

Valeur d'Exposition Moyenne Pondérée (VEMP) :
2 mg/m³ (Fumes)

References :
1. Chemical Hazards of the Workplace, Proctor & Hughes, 4th edition.
2. Clinical Environmental Health and Toxic Exposures, Sullivan & Krieger; second edition.
3. CSST-Québec, Répertoire Toxicologique.
4. Occupational Medicine, Zenz C., third edition.
5. Sax's Dangerous Properties of Industrial Materials, Lewis C., 10th edition.
6. The International Group, MSDS, Paraffin.
7. Toxicologie Industrielle et Intoxications Professionnelles, Lauwerys R.R., 4th edition.

By Edouard Bastarache

Related Information

Links

Materials Paraffin Wax
Typecodes Article by Edouard Bastarache
Edouard Bastarache is a well known doctor that has written many articles on the subject of toxicity of ceramic materials and books on technical aspects of ceramics. He writes in both English and French.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy