Alumina Toxicology | Ammonia and Latex Toxicity | Antimony Oxide | Are colored porcelains hazardous? | Arsenic Oxide | Asbestos Toxicity | Ball Clay | BARIUM and COMPOUNDS Toxicology | Barium Carbonate in Clay Bodies | Barium Carbonate in Glazes | Bentonite Toxicity | Beryllium Monoxide Toxicology | Bismuth Trioxide Toxicology | Boron Compounds and Their Toxicity | Brown Stain | Cadmium Toxicity | Calcium Carbonate Toxicology | Carbon Monoxide Toxicity | Cesium Toxicology | Chromium Compounds Toxicology | Clay Toxicity | Cobalt Oxide and Carbonate | Cobalt Toxicology | Copper Compounds Toxicology | Copper Oxide and Carbonate | Cristobalite Toxicity | Cryolite and Ceramics | Dealing With Dust in Ceramics | Diatomaceous Earth Toxicology | Dioxins in Clays | Epsom Salts | Eye Injuries Due to Radiation | Feldspar | Fighting Micro-Organisms in Ceramics | Fluorine Gas | Fumes from gas kilns | Gallium Oxide Toxicology | Hafnium Oxide Toxicty | Hydrofluoric Acid Toxicity | Iron oxide and Hematite | Lead Chromate | Lead in Ceramic Glazes | Lead Toxicology | Lithium Carbonate Toxicity | Lithium Toxicology | Man-Made Vitreous Fibers (MMVF) Toxicology | Man-Made Vitreous Fibers Safety Update | Manganese and Parkinsons by Jane Watkins | Manganese in Clay Bodies | Manganese Inorganic Compounds Toxicology | Manganese Toxicity by Elke Blodgett | Manganese: Creativity and Illness by Dierdre O'Reilly | Molybdenum Compounds Toxicology | Nickel Compounds Toxicity | Niobium Oxide Toxicity | Occupational Dermatoses | Overview of Material Safety by Gavin Stairs | Paraffin Toxicology | Perlite Toxicity | Plant Ash Toxicity | Potassium Carbonate Toxicity | Pregnancy and Ceramics | Propane Toxicology | Quartz Toxicity | Quartz Toxicity on Clayart | Rare Earth Compounds Toxicity | Rubidium and Cesium Toxicology | Rutile Toxicology | Silicosis and Screening | Silver Compounds Toxicology | Sodium Azide Toxicology | Sodium Carbonate Toxicology | Sodium Silicate Powder Toxicology | Stannous Chloride Toxicity | Strontium Carbonate Toxicity Note | Sulfur Dioxide Toxicity | | Talc Toxicology | Thallium Oxide Toxicology | Thorium Dioxide Toxicity | Tin Inorganic Compounds | Titanium Dioxide Toxicology | Toxicological Assessment of Zeolites | Tungsten Compounds Toxicology | Understanding Acronyms on MSDS's | Uranium and Ceramics | Vanadium and Compounds Toxicology | Vermiculite | Zinc Compounds Toxicology | Zirconium Compounds Toxicity | Zirconium Encapsulated Stains Toxicity

Talc Hazards Overview

Health concerns about talc revolve mainly around the non-platiform content, the extent to which these are asbestos, and how high the aspect ratio (length:width ratio) of non-platy particles need to be to make them a hazard. In ceramics, the platy form is used, so fibrous talc particles are considered a contaminant of that. In recent years (since 2020) litigation has shut down a number of talc suppliers in the US, it is not clear how closely this relates to the actual hazard of talc. Ceramic body manufacturers are evaluating how to substitute talc for other materials (especially in low fire whites where talc raises the thermal expansion to make glaze fit easier).

ACGIH TLV and OSHA PEL: 2 mg/cubic meter, 8 hr. TWA, Respirable Dust (talc containing no asbestos fibers).
CAS: 71949-90-1
Chlorite (typical 3%) ACGIH TLV: 10 mg/cubic meter 8 hr. TWA
CAS: 14808-60-7 Silica: (typical 2%) ACGIH TLV & OSHA PEL: 0.1 mg/cubic meter 8 hr. TWA, Respirable Dust

Wilson039;s RISK Scale of Material Hazards
(1-4 higher numbers are increased hazard)

May cause irritation to upper respiratory tract.

Pre-existing lung disease may be aggravated by exposure to dust. Prolonged over exposure can cause Talcosis (a pulmonary fibrosis of the lungs). Although talc is a fibrous magnesium silicate as is asbestos, it does not have the same effect on the lungs. The two minerals are closely associated, and most commercial talcs do contain some asbestos.

Talc is not characterized as a carcinogen by NTP, IARC, ACGIH or OSHA.

Talc may contain extremely small amounts (less than 2 ppm) of substances regulated under drinking water regulations: e.g. arsenic, beryllium, cadmium, chromium, lead, mercury, nickel.

Phsyical Data:

References

  1. An excellent discussion of talc hazards can be found in 039;Documentation of the Threshold Limit Values and Biological Exposure Indices039; from the American Conference of Industrial Hygienists, Cincinnati, OH
  2. 039;Patty039;s Industrial Hygiene and Toxicology039;, John Wiley & Sons has information on asbestosis and talcosis.

By Tony Hansen
Follow me on

Related Information

Links

Materials 4392 Rosa Blanca
Materials Glacier 200 Talc
Materials I.T. Talc
Materials Luzenac Talc 00S
Materials Noor Talc
Materials Roudnice Talc
Materials Sierralite Talc
Materials VanTalc
Materials FinnTalc
Materials Desertalc
Materials CT-30 Talc
Materials Cimcoat 325 Talc
Materials Nytal Talc
Materials Talc
A source of MgO for ceramic glazes, a flux or thermal expansion additive in clay bodies, also used in the manufacture of cordierite.
Materials Suzorite 325-PE
Materials Amtalc-C98
Materials Pioneer 2661 Talc
Materials Caltalc
Materials Ceramitalc 10A
Materials Ceramitalc No. 1
Oxides Sm2O3 -
URLs https://insight-live.com/insight/share.php?z=P8uThTnFoY
Replace Talc with Nepheline Syenite in low temperature white bodies
This is a development project at Plainsman Clays. It is in response to Texas talc no longer being available in North America.
URLs https://www.ncbi.nlm.nih.gov/search/research-news/8551/
$4.69 billion verdict against Johnson & Johnson's talcum powder
To 22 women who alleged the powder caused their ovarian cancer.
URLs https://www.asbestos.com/news/2021/05/04/canada-talc-restrictions/
Canada moves toward increased talc restrictions, but not in ceramics
Health Canada issued an official advisory in April 2021, concluding that loose talc products (in body powder) can cause serious lung problems. However the final assessment found there were no health concerns from pressed-powder products (e.g. talc in paper, paint, ceramics, plastics or putties).
URLs http://www.ilo.org/public/english/protection/safework/cis/products/icsc/dtasht/_icsc00/icsc0014.htm
Asbestos at ilo.org
URLs http://en.wikipedia.org/wiki/Asbestos
Asbestos at Wikipedia
URLs https://www.lawsuit-information-center.com/2-billion-verdict-in-missouri-motivates-jj-to-settle-talcum-powder-lawsuits.html
Lawsuit Information Center - Talcum powder pending cases almost 60K
The Talcum powder MDL added 146 new cases in Nov 2024, bringing the total to 58,198.
Hazards Asbestos Toxicity
Hazards Talc Toxicology

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy