Alumina Toxicology | Ammonia and Latex Toxicity | Antimony Oxide | Are colored porcelains hazardous? | Arsenic Oxide | Asbestos Toxicity | Ball Clay | BARIUM and COMPOUNDS Toxicology | | Barium Carbonate in Glazes | Bentonite Toxicity | Beryllium Monoxide Toxicology | Bismuth Trioxide Toxicology | Boron Compounds and Their Toxicity | Brown Stain | Cadmium Toxicity | Calcium Carbonate Toxicology | Carbon Monoxide Toxicity | Cesium Toxicology | Chromium Compounds Toxicology | Clay Toxicity | Cobalt Oxide and Carbonate | Cobalt Toxicology | Copper Compounds Toxicology | Copper Oxide and Carbonate | Cristobalite Toxicity | Cryolite and Ceramics | Dealing With Dust in Ceramics | Diatomaceous Earth Toxicology | Dioxins in Clays | Epsom Salts | Eye Injuries Due to Radiation | Feldspar | Fighting Micro-Organisms in Ceramics | Fluorine Gas | Fumes from gas kilns | Gallium Oxide Toxicology | Hafnium Oxide Toxicty | Hydrofluoric Acid Toxicity | Iron oxide and Hematite | Lead Chromate | Lead in Ceramic Glazes | Lead Toxicology | Lithium Carbonate Toxicity | Lithium Toxicology | Man-Made Vitreous Fibers (MMVF) Toxicology | Man-Made Vitreous Fibers Safety Update | Manganese and Parkinsons by Jane Watkins | Manganese in Clay Bodies | Manganese Inorganic Compounds Toxicology | Manganese Toxicity by Elke Blodgett | Manganese: Creativity and Illness by Dierdre O'Reilly | Molybdenum Compounds Toxicology | Nickel Compounds Toxicity | Niobium Oxide Toxicity | Occupational Dermatoses | Overview of Material Safety by Gavin Stairs | Paraffin Toxicology | Perlite Toxicity | Plant Ash Toxicity | Potassium Carbonate Toxicity | Pregnancy and Ceramics | Propane Toxicology | Quartz Toxicity | Quartz Toxicity on Clayart | Rare Earth Compounds Toxicity | Rubidium and Cesium Toxicology | Rutile Toxicology | Silicosis and Screening | Silver Compounds Toxicology | Sodium Azide Toxicology | Sodium Carbonate Toxicology | Sodium Silicate Powder Toxicology | Stannous Chloride Toxicity | Strontium Carbonate Toxicity Note | Sulfur Dioxide Toxicity | Talc Hazards Overview | Talc Toxicology | Thallium Oxide Toxicology | Thorium Dioxide Toxicity | Tin Inorganic Compounds | Titanium Dioxide Toxicology | Toxicological Assessment of Zeolites | Tungsten Compounds Toxicology | Understanding Acronyms on MSDS's | Uranium and Ceramics | Vanadium and Compounds Toxicology | Vermiculite | Zinc Compounds Toxicology | Zirconium Compounds Toxicity | Zirconium Encapsulated Stains Toxicity

Barium Carbonate in Clay Bodies

MSDS sheets indicate that barium (CAS: 7440-39-3) is poison and toxic if ingested. MSDS sheets also claim that barium is an irritant for inhalation and skin contact. Excessive amounts can cause violent diarrhea, convulsive tremors, and muscular paralysis. Barium is known to affect the heart and nervous system.

In ceramics, barium is most commonly inhaled as a fine dust or absorbed through cuts or lesions on the hands of people who handle compounds containing the material. However, some authorities quote inhalation exposure limits that are less restrictive than those for silica (e.g. ACGIH lists a Threshold Limit Value (TLV) at 0.5 mg/cubic meter for barium while quartz is 0.05). OSHA, on the other hand, lists quartz as 10.0 and barium as 0.5.

Almost all raw clay materials (including kaolins) contain soluble impurities (i.e. iron-stained calcium/magnesium sulphates). When a raw piece of clay is dried, these impurities come to the surface with the water as it evaporates. During firing, this leaves an unsightly glassy discoloration on the surface (in some cases even a glaze-like surface). In structural products, this is called "efflorescence". Such surfaces are highly prized in sculpture bodies because they highlight textures and contours. Of course, in functional pottery and structural products, these salts are not wanted. Even after a clay is fired, the salts can come to the surface if the clay is non-vitreous and is rewetted often (as is the case with red terra cotta brick). These surface deposits can affect melting patterns of overlying glaze layers. Fused solubles on the surface can also stick ware together or to kiln shelves and can seal the surface, causing premature bloating during firing.

Clay supply companies commonly add barium carbonate to clay bodies and raw products (0.1-0.6%) to mitigate this problem. The barium chemically reacts with the sulphates to precipitate insoluble products. In the reaction, very slightly soluble barium carbonate and soluble calcium sulphate convert to insoluble barium sulphate and calcium carbonate. Thus, both remain within the body and do not concentrate on the surface during drying. It is possible to measure the amount of solubles in a clay body and calculate the minimum amount of barium needed to precipitate them. However, in practical term,s this does not work because different types and even shipments of barium vary in their effectiveness and the natural salt content within the clays varies even more. If the fired surface is monitored closely companies can continuoiusly adjust to use just enough barium to precipitate all the soluble, but no more (barium is expensive and industry obviously does not want to use more than is necessary).

The presence of barium in clay bodies is sometimes thought to be a health hazard for hypersensitive people. But it is difficult to even demonstrate its solubility, and therefore bioavailability, in a simple lab experiment (MSDS sheets may even list it as insoluble). However, it does precipitate the dissolved calcium and magnesium salts in the clays, which proves that part of it is dissolving. In addition lab tests to deduce barium carbonate content in aged pugged clay bodies have shown a much lesser quantity of unreacted barium than the slight solubility suggests is possible. An MSDS from BassTech International classifies barium as moderately toxic on inhalation, non-toxic on contact or skin absorption, an eye irritant and toxic if ingested at 57mg per kg of body weight (this would be over 1 kg of pugged clay containing the highest proportion of barium normally used). If there is a hazard, then the most likely would be breathing in the dust and swallowing part of it. Obviously, it would be impossible to breathe in enough to be harmful.

Leaching Hazard When Used in Clay Bodies?

The practice of adding barium to clay bodies is questioned by some as a leaching hazard in functional ware made from the clay. However, one must consider:

The US Food and Drug Administration does not have a leaching requirement for barium. However, the US EPA has a standard for drinking water of 2 mg/liter or less. This standard was set to protect the population most at risk for heart effects - adult men. Testing can be done at Elemental Research Lab, 309-267 West Esplanade, North Vancouver, B.C. Canada V7M 1A5 604-985-0445 (they test many metals). Also at Kirby Health Center Lab, 71 North Franklin Street, Wilkes-Barre, PA 18701 717-822-4278.


By Tony Hansen
Follow me on

Related Information

How bad can efflorescence on terra cotta be?


Soluble salts on terra cotta cup

This picture has its own page with more detail, click here to see it.

Like this! This terra cotta clay matures to good strength around 1950F. Notice how the soluble salts have concentrated on the outer and most visible surface. The piece was dried upside down so, of course, all the water had to escape through that route. A complicating factor is how handling of the piece at the leather hard stage has made it even more unsightly. This problem is common in many terra cotta materials but can also surface in others. A tiny addition of barium carbonate can precipitate the salts inside the clay matrix so they do not come to the surface on drying.

The magic of a small barium carbonate addition to a clay body


This picture has its own page with more detail, click here to see it.

Two bisqued terracotta mugs demonstrate efflorescence. The clay on the right has 0.35% added barium carbonate (it precipitated the natural soluble salts dissolved in the clay and prevented them from coming to the surface with the water and being left there during drying). The process is called efflorescence and is the bane of the brick and terra cotta tile industries. The one on the left is the natural clay. The unsightly appearance is fingerprints from handling the piece in the leather-hard state, the salts have concentrated in these areas (the other piece was also handled).

Soluble salts on cone 04 terra cotta clay bodies


This picture has its own page with more detail, click here to see it.

Low temperature clays are far more likely to have this issue. And if present, it is more likely to be unsightly. The salt-free specimens have 0.35% added barium carbonate.

A typical DFAC drying disk of an iron stoneware clay


This picture has its own page with more detail, click here to see it.

The center portion was of this DFAC test disk was covered and so it lagged behind during drying, setting up stresses that caused the disk to crack. This test is such that most pottery clays will exhibit a crack. The severity of the crack becomes a way to compare drying performances. Notice the test also shows soluble salts concentrating around the outer perimeter, they migrated there from the center section because it was not exposed to the air.

Cone 10R stoneware clay with and without barium carbonate


This picture has its own page with more detail, click here to see it.

0.35% barium added to the one of the left makes the amazing difference on the bases of these two stoneware mugs. The slightly soluble barium precipitates the soluble sulphates in the body, leaving them insoluble within the matrix. Notice that not only has the brown glassy scum at the edges been removed but the whole body surface is actually less vitreous.

Links

Materials Barium Carbonate
A pure source of BaO for ceramic glazes. This is 77% BaO and has an LOI of 23% (lost at CO2 on firing).
Materials Barium Sulfate
Glossary Sulfates
Soluble sulfates in clay produce efflorescence, an unsightly scum that mars the fired surface of structural and functional ceramic products.
Glossary Efflorescence
A common problem with dry and fired ceramic. It is evident by the presence of a light or dark colored scum on the dry or fired surface.
Articles Soluble Salts in Minerals: Detailed Overview
There are a wide range of soluble materials that can be in clay, this article enumerates them, provides procedures on identifying and measuring them and outlines what to do about the problem.
Minerals Gypsum
Gypsum is hydrated calcium sulphate, CaSO4 2H2O. It is the crystalline mineral from which plaster is
Hazards Understanding Acronyms on MSDS's
Understanding the meaning and purpose of acronyms used on materials safety data sheets for ceramic minerals and materials
Hazards BARIUM and COMPOUNDS Toxicology
Hazards Barium Carbonate in Glazes
Oxides BaO - Barium Oxide, Baria

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy