1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Plaster

Alternate Names: Gypsum, Selenite

Description: Potter's Plaster

Notes

There are many different types of plaster, they vary mainly in setting time, strength, and absorbency. Manufacturers provide instruction booklets on how to mix and use their materials. For example, common precautions with reference to pottery plaster are: Don't stack pallets 3 high to avoid hard chunks, use before the shelf life of 120 days expires (if longer then extend mixing time), don't mix at higher than 105 degrees for proper set. The shelf life precautions are especially important in wet climates or where stock is being kept in damp warehouses (in dry climates plaster can be stored much longer).

USG Pottery #1 (2000 psi) is an example of a general-purpose material for high water absorption. It is normally mixed at a 70 consistency (70 water to 100 plaster). Of course, this ratio can be compromised by adding more water (for greater absorbency), but that comes at the cost of mold life and surface durability. Puritan plaster is similar but emphasizes hardness at the cost of porosity, it is used in production applications where molds must be more durable (e.g. for use in jiggering machines).

Jiggering benefits from a plaster with more surface hardening additives (i.e. USG's "Puritan" 66:100 water:plaster). For carving USG "Moulding Plaster" works well. USG Ultracal (5000 psi) and Hyrdostone (10,000 psi) are very hard materials and ideal for case molds where "hardness at the expense of absorbency" are required (they require much less water).

Manufacturers have excellent mixing instructions on their websites. They emphasize proper water-to-plaster ratio for the right durability absorbency compromise. Manufacturers recommend weighing the water, adding the plaster to the water, soaking for 2-3 minutes, then mixing well using a propeller mixer. It is important agitate in such a way that the air bubbles break at the surface during mixing. It is doubly important to use the same water-plaster ratio and procedure when making separate mold pieces that must fit and work together (so they mate properly and have the same absorbency).

Gypsum cements are not the same as pottery plasters. They are designed for optimum density, hardness and dimensional stability. Hydrocal, UltraCal and Hydrostone are examples.

Plaster dust is not harmful. It is calcium sulphate, or Selenite. Many raw clays contain small chunks of natural Selenite, it normally just gets ground up with the rest of the clay or converted to calcium oxide during firing (that subsequently reacts with surrounding particles to form calcium silicates and aluminates). If there is a significant amount of calcium sulphate you may smell sulphur during firing (but with ventilation in modern kilns this is highly unlikely). If any larger particles of plaster get into a clay body they can absorb water from the air or surrounding body (if sufficiently porous) to become calcium hydroxide. This reaction causes expansion that can be enough to pop out a piece of the clay.

A continuous plaster mixing machine as available from: Hoge Warren Zimmermann Co., 40 West Crescentville Rd., Cincinnati, OH 45246 FAX 513-671-3514

Related Information

The demise of USG plasters!

If true, this is seismic for ceramics.


Mini beer bottle mold, bag of plaster

This picture has its own page with more detail, click here to see it.

The ceramic industry depends on some surprisingly specialized materials made by very few companies. When one of those companies exits the market, we need to notice. Consider how much of ceramics depends on plaster: slip casting of pottery and sanitaryware, jiggering, RAM pressing, mold making and countless studio processes. Yet plaster is so inexpensive and familiar that we tend to forget how technologically specialized—and indispensable—it actually is.

July 30, 2026: The Bad News USG is closing its historic Southard, Oklahoma gypsum operation, apparently ending production of a wide range or specialty plasters including #1 Pottery Plaster, Hydro-Stone, Ultracal, Hydrocal, Puritan. This is a potentially seismic event for ceramics.
There is an Alternative Fortunately, there is another major North American producer: Georgia-Pacific. Its K-59 Pottery Plaster is a remarkably close counterpart to USG #1, having essentially the same normal water/plaster ratio and density, with similar strength and expansion. Without products like these from Georgia-Pacific, the USG withdrawal could have been a genuine supply-chain earthquake for ceramics. Instead, it should be a wake-up call.
Cautious Optimism Georgia-Pacific has a long-established Industrial Plasters division with dedicated sales managers covering both the U.S. and Canada. GP already manufacture pottery and tooling plasters, ceramics is one of the industries they explicitly target. If they embrace the opportunity, they would become the primary North American supplier of specialty ceramic plasters. The biggest uncertainty is whether they can produce enough to replace what USG has historically supplied. And whether ceramic suppliers will begin stocking larger inventories.

Links

Oxide Analysis Formula Tolerance
Materials Sodium Selenite
URLs https://en.wikipedia.org/wiki/Plaster
Plaster at Wikipedia
Information on the chemical reactions that occur when gymsum is heated.
URLs https://plaster.glazy.org/
Glazy Plaster Calculator
Choose the shape, enter the measurements in cm or inches, choose type of plaster and consistency.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy