Alumina Toxicology | Ammonia and Latex Toxicity | Antimony Oxide | Are colored porcelains hazardous? | Arsenic Oxide | Asbestos Toxicity | Ball Clay | BARIUM and COMPOUNDS Toxicology | Barium Carbonate in Clay Bodies | Barium Carbonate in Glazes | Bentonite Toxicity | Beryllium Monoxide Toxicology | Bismuth Trioxide Toxicology | Boron Compounds and Their Toxicity | Brown Stain | Cadmium Toxicity | Calcium Carbonate Toxicology | Carbon Monoxide Toxicity | Cesium Toxicology | Chromium Compounds Toxicology | Clay Toxicity | Cobalt Oxide and Carbonate | Cobalt Toxicology | Copper Compounds Toxicology | Copper Oxide and Carbonate | Cristobalite Toxicity | Cryolite and Ceramics | Dealing With Dust in Ceramics | Diatomaceous Earth Toxicology | Dioxins in Clays | Epsom Salts | Eye Injuries Due to Radiation | Feldspar | Fighting Micro-Organisms in Ceramics | Fluorine Gas | Fumes from gas kilns | Gallium Oxide Toxicology | Hafnium Oxide Toxicty | Hydrofluoric Acid Toxicity | Iron oxide and Hematite | Lead Chromate | Lead in Ceramic Glazes | Lead Toxicology | Lithium Carbonate Toxicity | Lithium Toxicology | Man-Made Vitreous Fibers (MMVF) Toxicology | Man-Made Vitreous Fibers Safety Update | Manganese and Parkinsons by Jane Watkins | Manganese in Clay Bodies | Manganese Inorganic Compounds Toxicology | Manganese Toxicity by Elke Blodgett | Manganese: Creativity and Illness by Dierdre O'Reilly | Molybdenum Compounds Toxicology | Nickel Compounds Toxicity | Niobium Oxide Toxicity | Occupational Dermatoses | Overview of Material Safety by Gavin Stairs | Paraffin Toxicology | Perlite Toxicity | Plant Ash Toxicity | Potassium Carbonate Toxicity | Pregnancy and Ceramics | Propane Toxicology | Quartz Toxicity | Quartz Toxicity on Clayart | Rare Earth Compounds Toxicity | Rubidium and Cesium Toxicology | Rutile Toxicology | Silicosis and Screening | Silver Compounds Toxicology | Sodium Azide Toxicology | Sodium Carbonate Toxicology | Sodium Silicate Powder Toxicology | Stannous Chloride Toxicity | Strontium Carbonate Toxicity Note | Sulfur Dioxide Toxicity | Talc Hazards Overview | Talc Toxicology | Thallium Oxide Toxicology | Thorium Dioxide Toxicity | Tin Inorganic Compounds | | Toxicological Assessment of Zeolites | Tungsten Compounds Toxicology | Understanding Acronyms on MSDS's | Uranium and Ceramics | Vanadium and Compounds Toxicology | Vermiculite | Zinc Compounds Toxicology | Zirconium Compounds Toxicity | Zirconium Encapsulated Stains Toxicity

Titanium Dioxide Toxicology

Titanium is one of the most common components of the earth039;s crust, ninth in abundance. It occurs naturally as ilmenite (iron titanate) and rutile (titanium dioxide).

Titanium forms four distinct oxides: titanium monoxide (TiO), dititanium trioxide (Ti2O3), titanium dioxide (TiO2) and titanium trioxide (TiO3).

Occupational and Environmental Exposure Sources

Titanium is frequently used as a white pigment for a wide range of paints, paper, inks, plastics, and the like.

Exposure results from breathing titanium dioxide dust. Possible exposure to intermediate products in titanium dioxide production may also occur.

Exposure may then occur at any stage in the mining of ores, in the preparation of titanium dioxide, and in any of the industries in which the powder is stored and used.

Clinical Toxicology

Titanium dioxide inhalation is the most common route of exposure. Ingestion is certainly possible when some dust accumulates on mucosal surfaces of the oropharynx and nasopharynx.

Titanium dioxide is found in the lymphatics and regional nodes that drain the lungs, indicating a slow removal by this process.

No data are available regarding oral absorption of titanium.

Titanium is excreted by the kidneys.

Titanium dioxide is an irritant to the upper airway, as are other nuisance dusts. No evidence indicates that it induces an acute inflammatory reaction at commonly seen exposure concentrations.

In workers with preexisting chronic obstructive airway disease, titanium dioxide may exacerbate symptoms.

Titanium dioxide is retained in the lungs. Particles of this dust are found also in the regional nodes draining the lungs, suggesting that these particles are slowly cleared by the lymphatics.

Little evidence indicates that titanium dioxide promotes a chronic inflammatory reaction in the lungs.

Titanium dioxide dust currently is considered to be merely a nuisance dust that results only in upper airway irritation.

No data are available regarding human genetic effects.

Evaluation by the IARC : The agent (the mixture) is possibly carcinogenic to humans Evaluation by the NIOSH and OSHA : Potential human carcinogen.

Note it is not classified as a confirmed carcinogen to man by these organisms.

Evaluation by the ACGIH: Substance not classifiable as a carcinogen to man (A4 group).

Limits of exposure

The limits of exposure proposed in the USA and Quebec do not mention this carcinogenic potential, and the limit is in relation with its irritating power.

Titanium dioxide is an irritant dust, therefore, management of exposure is supportive. Exposed workers should be removed from the environment, and supportive pulmonary care should be provided.

Most laboratory tests are not helpful. Assessement of serum and urinary titanium levels help to identify recent exposure.

Acute upper airway irritation may be reduced by keeping exposure to titanium at low limits.

Quebec039;s exposure limit

VEMP (Valeur d039;Exposition Moyenne Pondéré) = 10 mg/m3 as total dust.

Good industrial hygiene and monitoring of the environment should limit employee exposure to titanium dust. If employees must work in an environment with high titanium dioxide dust levels and poor ventilation,respirators should be used.

References

  1. Occupational Medicine,Carl Zenz, last edition.
  2. Clinical Environmental Health and Toxic Exposures, Sullivan & Krieger; last edition.
  3. Sax039;s Dangerous Properties of Industrial Materials, Lewis C., last edition.
  4. Toxicologie Industrielle et Intoxications Professionnelles, Lauwerys R.R. last edition.
  5. Chemical Hazards of the Workplace, Proctor & Hughes, 4th edition

By Edouard Bastarache

Related Information

Links

Typecodes Article by Edouard Bastarache
Edouard Bastarache is a well known doctor that has written many articles on the subject of toxicity of ceramic materials and books on technical aspects of ceramics. He writes in both English and French.
Materials Titanium Dioxide
A super white powder used in ceramic glazes to variegate, opacify and moderate color.
Materials Ilmenite
Materials Rutile
A raw TiO2-containing mineral used in ceramics to color and variegate glaze surfaces.
Hazards Rutile Toxicology

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy