Description: Iron Titanium Mineral
Formula: TiO2
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| TiO2 | 90.00% | 1.00 | |
| Fe2O3 | 10.00% | 0.06 | |
| LOI | 0.10% | n/a | |
| Oxide Weight | 88.78 | ||
| Formula Weight | 88.87 | ||
Rutile is the mineral name for natural crystals of titanium dioxide. However in nature rutile is always contaminated by other minerals (especially iron but also things like tantalum, niobium, chromium and tin, the analysis provided here is obviously a simplification). In ceramics, the term 'rutile' is generally understood to refer to the brown powder into which these minerals are ground. Industry accepts up to 15% contaminants (below 85% titanium is called ilmenite). Rutile is considered an impure form of titanium whereas ilmenite is considered as FeTiO3. Grades of rutile are sometimes named after one of the impurities. Rutile is employed in many industries, ceramic uses are minor in comparison. There are large reserves of rutile in the world so supply shortages are related to other factors. Manufacturers often blend ores from different deposits, at times from different parts of the world. And they improve the TiO2 content by furnace-processing. Large users of rutile will often track batch numbers and test when the number changes. A situation can sometimes be dealt with by adjusting the amount of rutile in the recipe, firing differently or milling it. In more serious cases additions of iron or pure titanium might be needed.
Rutile is available in light tan calcined ceramic grade powder (light rutile), darker uncalcined powder (dark rutile), and granular form. Either ceramic grade of powder is normally ground very fine (e.g. 325 mesh). In glazes, it is better to use a calcined grade (since the decomposition of raw rutile during firing could be a source of glaze imperfections like pinholing and bubbles). In our experience the LOI (weight loss on firing) when calcining rutile from our suppliers is less than 1%, so we are getting a calcined material. Milled rutile is normally ground to 200 mesh.
Rutile produces many crystalline, speckling, streaking, and mottling effects in glazes during cooling in the kiln and has been used in all types of colored glazes to enhance the surface character. It is thus highly prized by potters, many attractive variegated glazes are made using it. Many potters would say that their living depends on their rutile supply!
Rutile is very refractory in oxidation, even a mix of 50% borax alumina-free frit like Ferro 3134 will not melt it in a crucible. In reduction, the improvement in melting will depend on the amount of iron present.
In ceramic glazes rutile is more often considered a variegator than a colorant. As little as 2% can impart significant effects in stoneware glazes. It is normally used in combination with a wide range of metal oxide and stain colorants to produce surfaces that are much more visually interesting. In glazes with high melt fluidity (e.g. having high boron), large amounts of rutile (e.g. 6-8%) can be quite stunning. The rutile encourages the development of micro-crystals (it is crystalline itself) and rivulets. Since rutile contains significant iron its use in combination with other colorants will often muddy the color that they would otherwise have or alter it if they are sensitive to the presence of iron. Even though rutile generally makes up less than 5% of stoneware glazes that employ it, they are often called 'rutile glazes' in recognition of its dramatic contribution.
Excessive rutile in a glaze can produce surface imperfections. In addition, when rutile is employed in higher percentages (e.g. 5%+) a given percentage might work well whereas a slightly higher amount can look drastically different. Such situations are vulnerable to chemistry changes in the supply of rutile. Thus people will often do a line blend trying a range of percentages to determine an optimal amount.
In glazes, rutile can be quite sensitive to the presence of opacifiers. While an unopacified glaze might appear quite stunning, the addition of a zircon opacifier will usually drastically alter its appearance and interest because the variegation imparted is dependent on the glaze having depth and transparency or translucency. Strangely rutile and tin, another opacifier, can produce some very interesting reactions and it is quite common to see tin in amounts of up to 4% in rutile glazes. In these cases, the tin appears to react in the crystal formation rather than opacify the glaze.
Pure rutile powder, although its color makes it appear to be a crude ground mineral, normally contains 95%+ titanium dioxide. However, this does not mean that you can use a 95% titanium:5% iron mix and get the same result in a ceramic glaze (obviously line blending would be needed to match the amount of iron). The mineralogy and significant other impurities in rutile are a major factor in the way it acts in glazes (not easily duplicated using a blend of other things). Sometimes the special effects that rutile produces in glazes are also partly a product of a coarser grade (larger particle size). These likewise cannot be easily duplicated by more refined materials. Unfortunately, the trend at some mining operations (at least in Australia) is to fine grind the rutile on-site, making it more difficult for ceramic operations to obtain the coarser grades.
Although rutile will normally stain a glaze brown or yellow, its crystallization effects can significantly lighten the color of iron glazes. Higher amounts of rutile in stoneware glazes will often contribute glaze imperfections.
Granular rutile is sometimes used in bodies and glazes to impart fired speckle.
Rutile is used for special effects in leaded glazes and can form up to 15% of the recipe.
Rutile can be used as a tone modifier to soften the more potent colorants.

This picture has its own page with more detail, click here to see it.
This bag is very small, this material is very dense and heavy. The primary use of this material is obvious: For making welding rods. We can thus assume it will continue to be abundantly available for ceramics. Notice the bag bottom is marked "Ceramic Rutile" (with a batch number). Why would a product intended for making welding rods be used in ceramics? The answer is very interesting.

This picture has its own page with more detail, click here to see it.

This picture has its own page with more detail, click here to see it.
Rutile Crystals

This picture has its own page with more detail, click here to see it.
Rutilite Slices

This picture has its own page with more detail, click here to see it.
Left: GA6-C rutile blue glaze on a brown stoneware. The 4% ceramic rutile powder gives the blue variegated effect. Right: We ball-milled our granular rutile and then screened it down to 325 mesh and put that into the same glaze. The results are the same. So if any of your rutile glazes ever lose this effect with a new supply of the material the cause could be that it has not been milled sufficiently fine. Finer rutile powders are browner in color.

This picture has its own page with more detail, click here to see it.
These metal oxides have been mixed with 50% Ferro frit 3134 and fired to cone 6 oxidation. Chrome and rutile have not melted, copper and cobalt are extremely active melters, frothing and boiling. Cobalt and copper have crystallized during cooling. Manganese has formed an iridescent glass.

This picture has its own page with more detail, click here to see it.
2, 3, 4, 5% rutile added to an 80:20 mix of Alberta Slip:Frit 3134 at cone 6. This variegating mechanism of rutile is well-known among potters. Rutile can be added to many glazes to variegate existing color and opacification. If more rutile is added the surface turns an ugly yellow in a mass of titanium crystals.

This picture has its own page with more detail, click here to see it.
Rutile is a high iron and titanium mineral mined in Sudbury, Ontario. When kilns cool this glaze "parties and dances", creating amazing rivulets and crystals of blue and navy. Both of these glazes are made from materials mined by Plainsman Clays (in Montana, Alberta and Saskatchewan). Both produce a wide range of effects with different thicknesses, bodies and firing schedules. These effects were achieved by firing to cone 6 (2200F) and slow cooling down to 1400F (my C6DHSC schedule).

This picture has its own page with more detail, click here to see it.
Rutile blue glazes are actually titanium blues (because rutile mineral is an impure source of TiO2 and Fe2O3). The iron and titanium in the rutile react to form the floating blue effect. The GA6-C recipe has always relied on a 4% rutile addition. Its GA6-A base recipe contains significant iron (because of the 80% Alberta Slip), so could titanium oxide deliver the same floating blue effect? Yes.
These mugs are M390 clay. The top left one is the standard GA6-C (with rutile) fired using the C6DHSC slow-cool firing schedule (the bottom left normal cool PLC6DS schedule produces little color). But the ones on the right switch the 4% rutile for titanium dioxide (the L4655 recipe). The top right was fired using the slow cool, the bottom right was the normal cool schedule.
Titanium thus seems more consistent and reliable material than rutile. An excellent blue color is produced even without a slow cool (lower right).

This picture has its own page with more detail, click here to see it.
The clay body is Plainsman P700. This was fired in cone 10R using the C10RPL firing schedule. The outside glaze is G2571C. The inside glaze is G1947U.

This picture has its own page with more detail, click here to see it.
The glaze is G191T (a variation of G1916Q). Firing was cone 04 drop-and-hold with slow cool. Sometimes a raw colorant is advisable over a ceramic stain. At low temperatures stains are almost universal. But in this case, the orangey-yellow color that rutile produces merits further testing. On the red body (Plainsman L215) the color is barely perceptible, but on the light Buffstone body it is working well. The variations in thickness highlight contours better than what a stain would do.
| Minerals |
Rutile
Rutile is the mineral name for natural crystals of titanium dioxide. It is a very hard (6-6.5 Moh) a |
| Minerals |
Brookite
A mineral form on titanium dioxide. |
| Minerals |
Anatase
A mineral form of titanium dioxide. |
| Glossary |
Variegation
Ceramic glaze variegation refers to its visual character. This is an overview of the various mechanisms to make glazes dance with color, crystals, highlights, speckles, rivulets, etc. |
| Glossary |
Reactive Glazes
In ceramics, reactive glazes have variegated surfaces that are a product of more melt fluidity and the presence of opacifiers, crystallizers and phase changers. |
| URLs |
http://www.sciencedirect.com/science/article/pii/S0168583X03018214
Report on the composition of Nigerian Rutile |
| URLs |
http://en.wikipedia.org/wiki/Rutile
Rutile on Wikipedia |
| URLs |
http://www.consrutile.com.au/ABOUTCRL/dwnstream.htm
Consolidated Rutile Ltd in Australia |
| URLs |
http://www.theimage.com/mineral/rutile/
Rutile information website |
| URLs |
http://webmineral.com/data/Rutile.shtml
Rutile at WebMineral.com |
| URLs |
http://www.mindat.org/min-3486.html
MinDat.org Information |
| URLs |
http://mineral.galleries.com/minerals/oxides/rutile/rutile.htm
MineralGalleries.com Information |
| Oxides | TiO2 - Titanium Dioxide, Titania |
| Materials |
Ruflux 61
|
| Materials |
Ceramic Rutile
Rutile mineral ground to a very fine particle size (e.g. 325 mesh) contributes titanium and iron that colors and variegates ceramic glazes. |
| Materials |
Ilmenite
|
| Materials |
Granular Rutile
The same material as milled rutile, but ground only to granular size. |
| Materials |
Titanium Dioxide
A super white powder used in ceramic glazes to variegate, opacify and moderate color. |
| Typecodes |
Colorant
Metallic based materials that impart fired color to glazes and bodies. |
| Typecodes |
Generic Material
Generic materials are those with no brand name. Normally they are theoretical, the chemistry portrays what a specimen would be if it had no contamination. Generic materials are helpful in educational situations where students need to study material theory (later they graduate to dealing with real world materials). They are also helpful where the chemistry of an actual material is not known. Often the accuracy of calculations is sufficient using generic materials. |
| Hazards |
Rutile Toxicology
|
| Hazards |
Titanium Dioxide Toxicology
|
| Hardness (Moh) | 6.0-6.5 |
|---|---|
| Frit Softening Point | 1600C M |
| Density (Specific Gravity) | 4.20 |
| Body Color | Rutile sand (granular) can be used to add speck to bodies. |
|---|---|
| Body Color | Rutile can be added to low fire bodies to make them burn golden yellow. |
| Glaze Color | Rutile produces many shades from pale straw to tan to cinammon brown to orange brown. Alkaline glazes experience less of the classic rutile crystalline effect. Color intensifies with increased amounts and tends to be darker in reduction. |
| Glaze Color | 5-8% added rutile can give powder to deep blue colors in reduction. These colors can be brilliant and mottled with shades of browns and tans. Rutile effects can be hard to Like copper reds, rutile blue reduction effects depend on adequate silica being available (7 times or more that of alumina). Classic rutile blue glazes are best made by using rutile in fluid glossy bases. The amount of iron in the rutile (or from the body) determines the degree of blue since its reduction to FeO is a key to the effect. Since rutile is variable in makeup, changes in the iron content will change the blue color. The fact that titanium dioxide additions do not make good blues suggests that the iron-titanium mix is the key to good color. Silky matte variegated blue glazes can also be made with rutile additions. If you employ this type of glaze be sure that you have a large supply of rutile on hand and test new supplies throughly. |
| Glaze Color | In zinc glazes powdered rutile develops an orange-tan color. |
| Glaze Color | Rutile can produce soft tan colors due to its iron content, especially in matte glazes. |
| Glaze Color | Rutile and cobalt can crystallize to form green glazes. |
| Glaze Matteness | Even in small amounts, rutile tends to matte the surface of leaded glazes. |
| Glaze Opacifier | As an opacifier rutile is economical compared with pure titanium and it is employed where white shades are not required. It is also used to stain pottery bodies and glazes (yellowish, orange and tan colors are most common because of its iron content). |
| Glaze Variegation | Rutile has the unique property of breaking up and variegating the color and texture of glazes, it is quite popular in tile and art pottery for this reason. However this effect depends on the rutile powder being coarse enough to act as an adjunct (the finer grades disperse more readily into the glass matrix). The addition of 4-8% rutile to many stoneware glazes can make an otherwise drab or flat glaze become much more interesting. When used in combination with colorants, it can be very effective at improving the character, however it will affect the color. When used with added tin streaking and mottling effects can be enhanced, especially in lead glazes. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk