Alumina Toxicology | Ammonia and Latex Toxicity | Antimony Oxide | Are colored porcelains hazardous? | Arsenic Oxide | Asbestos Toxicity | Ball Clay | BARIUM and COMPOUNDS Toxicology | Barium Carbonate in Clay Bodies | Barium Carbonate in Glazes | Bentonite Toxicity | Beryllium Monoxide Toxicology | Bismuth Trioxide Toxicology | Boron Compounds and Their Toxicity | Brown Stain | Cadmium Toxicity | Calcium Carbonate Toxicology | Carbon Monoxide Toxicity | Cesium Toxicology | Chromium Compounds Toxicology | Clay Toxicity | Cobalt Oxide and Carbonate | Cobalt Toxicology | Copper Compounds Toxicology | Copper Oxide and Carbonate | Cristobalite Toxicity | Cryolite and Ceramics | Dealing With Dust in Ceramics | Diatomaceous Earth Toxicology | Dioxins in Clays | Epsom Salts | Eye Injuries Due to Radiation | Feldspar | Fighting Micro-Organisms in Ceramics | Fluorine Gas | Fumes from gas kilns | Gallium Oxide Toxicology | Hafnium Oxide Toxicty | Hydrofluoric Acid Toxicity | Iron oxide and Hematite | Lead Chromate | Lead in Ceramic Glazes | Lead Toxicology | Lithium Carbonate Toxicity | Lithium Toxicology | Man-Made Vitreous Fibers (MMVF) Toxicology | Man-Made Vitreous Fibers Safety Update | Manganese and Parkinsons by Jane Watkins | Manganese in Clay Bodies | Manganese Inorganic Compounds Toxicology | Manganese Toxicity by Elke Blodgett | Manganese: Creativity and Illness by Dierdre O'Reilly | Molybdenum Compounds Toxicology | Nickel Compounds Toxicity | Niobium Oxide Toxicity | Occupational Dermatoses | Overview of Material Safety by Gavin Stairs | Paraffin Toxicology | Perlite Toxicity | Plant Ash Toxicity | Potassium Carbonate Toxicity | Pregnancy and Ceramics | Propane Toxicology | Quartz Toxicity | Quartz Toxicity on Clayart | Rare Earth Compounds Toxicity | Rubidium and Cesium Toxicology | Rutile Toxicology | Silicosis and Screening | Silver Compounds Toxicology | Sodium Azide Toxicology | Sodium Carbonate Toxicology | Sodium Silicate Powder Toxicology | Stannous Chloride Toxicity | Strontium Carbonate Toxicity Note | Sulfur Dioxide Toxicity | Talc Hazards Overview | Talc Toxicology | Thallium Oxide Toxicology | Thorium Dioxide Toxicity | Tin Inorganic Compounds | Titanium Dioxide Toxicology | Toxicological Assessment of Zeolites | Tungsten Compounds Toxicology | Understanding Acronyms on MSDS's | Uranium and Ceramics | Vanadium and Compounds Toxicology | Vermiculite | Zinc Compounds Toxicology | | Zirconium Encapsulated Stains Toxicity

Zirconium Compounds Toxicity

Introduction

Zirconium (Zr) constitutes about 0.2% of the earth039;s crust, common minerals bind zircon, zirconium dioxide and zirconates.

Uses

Typical Compounds

Occupational exposures

Potential occupational exposures to zirconium may be encountered during:

Toxicology

Zirconium compounds are generally considered to be of low toxicity.

Skin

Granulomata have been produced by repeated topical applications of zirconium salts to human skin.

Zirconium compounds are commonly used in antiperspirants and thus sometimes cause granulomata of the axillary skin. Aluminium zirconium compounds, which are mainly used today, are considered to be safer in this regard.

Lungs

Studies among workers exposed to zirconium compounds fumes have failed to demonstrate adverse pulmonary effects.

However, a recent report shows that severe pulmonary fibrosis containing high concentrations of several zirconium compounds occurred in a worker polishing and blocking lenses in an optical company.

Eyes

In my personal experience I have encountered a corneal burn with a subsequent scar in a titanium dioxide plant caused by the ocular projection of a small drop of liquid zirconium sulfate at the place where it was introduced into the process.

Quebec039;s exposure limit

VEMP (Valeur d039;Exposition Moyenne Pondérée) = 5mg/m³

References

  1. Occupational Medicine,Carl Zenz, last edition.
  2. Clinical Environmental Health and Toxic Exposures, Sullivan & Krieger; last edition.
  3. Sax039;s Dangerous Properties of Industrial Materials, Lewis C., last edition.
  4. Toxicologie Industrielle et Intoxications Professionnelles, Lauwerys R.R. last edition.
  5. Chemical Hazards of the Workplace, Proctor & Hughes, 4th edition

By Edouard Bastarache

Related Information

Links

Hazards Zirconium Encapsulated Stains Toxicity
Materials Magnesium Zirconium Silicate
Materials Zircon
Materials Zircopax
Zirconium silicate, its principle use in ceramics is as an opacifier in glazes. It is an expensive material, but less so than tin oxide.
Materials Superpax
Typecodes Article by Edouard Bastarache
Edouard Bastarache is a well known doctor that has written many articles on the subject of toxicity of ceramic materials and books on technical aspects of ceramics. He writes in both English and French.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy