Alumina Toxicology | Ammonia and Latex Toxicity | Antimony Oxide | Are colored porcelains hazardous? | Arsenic Oxide | Asbestos Toxicity | Ball Clay | BARIUM and COMPOUNDS Toxicology | Barium Carbonate in Clay Bodies | Barium Carbonate in Glazes | Bentonite Toxicity | Beryllium Monoxide Toxicology | Bismuth Trioxide Toxicology | Boron Compounds and Their Toxicity | Brown Stain | Cadmium Toxicity | Calcium Carbonate Toxicology | Carbon Monoxide Toxicity | Cesium Toxicology | Chromium Compounds Toxicology | Clay Toxicity | Cobalt Oxide and Carbonate | Cobalt Toxicology | Copper Compounds Toxicology | | Cristobalite Toxicity | Cryolite and Ceramics | Dealing With Dust in Ceramics | Diatomaceous Earth Toxicology | Dioxins in Clays | Epsom Salts | Eye Injuries Due to Radiation | Feldspar | Fighting Micro-Organisms in Ceramics | Fluorine Gas | Fumes from gas kilns | Gallium Oxide Toxicology | Hafnium Oxide Toxicty | Hydrofluoric Acid Toxicity | Iron oxide and Hematite | Lead Chromate | Lead in Ceramic Glazes | Lead Toxicology | Lithium Carbonate Toxicity | Lithium Toxicology | Man-Made Vitreous Fibers (MMVF) Toxicology | Man-Made Vitreous Fibers Safety Update | Manganese and Parkinsons by Jane Watkins | Manganese in Clay Bodies | Manganese Inorganic Compounds Toxicology | Manganese Toxicity by Elke Blodgett | Manganese: Creativity and Illness by Dierdre O'Reilly | Molybdenum Compounds Toxicology | Nickel Compounds Toxicity | Niobium Oxide Toxicity | Occupational Dermatoses | Overview of Material Safety by Gavin Stairs | Paraffin Toxicology | Perlite Toxicity | Plant Ash Toxicity | Potassium Carbonate Toxicity | Pregnancy and Ceramics | Propane Toxicology | Quartz Toxicity | Quartz Toxicity on Clayart | Rare Earth Compounds Toxicity | Rubidium and Cesium Toxicology | Rutile Toxicology | Silicosis and Screening | Silver Compounds Toxicology | Sodium Azide Toxicology | Sodium Carbonate Toxicology | Sodium Silicate Powder Toxicology | Stannous Chloride Toxicity | Strontium Carbonate Toxicity Note | Sulfur Dioxide Toxicity | Talc Hazards Overview | Talc Toxicology | Thallium Oxide Toxicology | Thorium Dioxide Toxicity | Tin Inorganic Compounds | Titanium Dioxide Toxicology | Toxicological Assessment of Zeolites | Tungsten Compounds Toxicology | Understanding Acronyms on MSDS's | Uranium and Ceramics | Vanadium and Compounds Toxicology | Vermiculite | Zinc Compounds Toxicology | Zirconium Compounds Toxicity | Zirconium Encapsulated Stains Toxicity

Copper Oxide and Carbonate

With limited exposure, copper is considered relatively safe to use. However, when added to low lead solubility glazes, copper causes the solubility of the lead to be greatly increased. The solubility of glazes of other types can also be increased by the presence of copper.

OSHA does not consider copper exposure in the workplace to be a significant problem. At worst, they state that copper is an irritant, especially airborne.

Copper has a TLV (threshold limit value) of 1.0 milligrams per cubic meter of air breathed. By comparison, iron oxide is considered a safe-to-use material at 5.0, kaolin is 2.0, barium carbonate is 0.5, quartz is 0.1-0.05.

Copper is not as toxic by ingestion as many of the other metals (it is not a heavy metal). The standard for water is 1.3 mg/L based more on its effects on taste than toxicity (cadmium is 0.005 mg/L).

Volatile copper given off during certain firing techniques can cause copper metal fume fever. If the exposure is limited, this is a temporary condition that goes away by itself.

People suffering from Wilson's Disease must be very careful of copper intake because their bodies cannot excrete it, thus it can build up to dangerous levels. Zinc and vitamin C cause the body to excrete copper and taking megadoses of these products could result in copper deficiency.

Copper has several roles in the body, one of which is to keep the connective tissues intact. Copper plays an essential role in the production of elastin, which is what keeps our skin soft and supple and wrinkle-free. Estrogen increases the amount of copper your body can absorb. The US RDA for copper is 3mg (although figures vary quite a bit). For someone with depleted copper, a daily dosage of 10 mg for a period of one month is not considered unsafe. Copper deficiency can increase LDL cholesterol and decrease HDL. It also has an effect on glucose levels. It is believed that some 90 percent of Americans are copper-deficient.


By Tony Hansen
Follow me on

Related Information

Lemon leaching test on a copper-containing glaze


This picture has its own page with more detail, click here to see it.

This was left for 24 hours. Wrapped in stretch wrap. Then the surface of the glaze was inspected under a lamp to detect any differences between the lemoned and non-lemoned surfaces. Lemons are highly acidic. This glaze passed because the base recipe, G3806N, was methodically developed so that it has plenty of Al2O3 and SiO2 (in the fired chemistry) to build a stable glass.

Copper does not necessarily cause glazes to leach ...

If used in moderate amounts


This picture has its own page with more detail, click here to see it.

These are four cone 6 glazes of diverse chemistry. They have varying melt fluidities. They are soaked (halfway up) in lemon juice overnight. None show any evidence of surface changes. All contain 2% copper carbonate. If the copper were increased, especially to the point of going metallic or crystallizing, the leaching test would produce different results (especially on the ones that are running; they lack SiO2 and Al2O3). So, if you use copper sensibly (in moderate amounts), there is a good chance of making a glaze that resists leaching.

Black ash glaze for 20% raw metal pigments: Suitable for functional ware?


Saturated metal ash glaze

This picture has its own page with more detail, click here to see it.

This glaze is 49% Wood Ash, 24% Soda Feldspar and 27% Ball Clay. 10 copper carbonate and 10 manganese dioxide are added to that. This beautiful sculpture was made by Dan Ingersoll, aesthetically this glaze is perfect for it. But there are two red flags here. Significant manganese and copper metal fumes are certain to be generated at cone 10 (they are seriously not healthy) so anyone using this must be very careful. But there is something much more serious - this glaze is being used on functional ware. Copper is well known to destabilize other metals in the fired glass. This 10:10 combination is a perfect storm for leaching heavy metal into food and drink. This is not an argument for the use of commercial glazes, it is one for common sense application of the concept of limit recipes.

Links

Materials Copper Oxide Red
Materials Copper Oxide Black
The purest source of CuO copper oxide pigment used in ceramic glazes.
Materials Copper Carbonate
A source of CuO copper oxide used in ceramic glazes to produce a variety of colors (used only or with other colorants).
Materials Copper Carbonate Basic
This form of copper carbonate is the article of commerce, a mixture of theoretical copper carbonate and copper hydroxide.
Glossary Leaching
Ceramic glazes can leach heavy metals into food and drink. This subject is not complex, there are many things anyone can do to deal with this issue
Articles Are Your Glazes Food Safe or are They Leachable?
Many potters do not think about leaching, but times are changing. What is the chemistry of stability? There are simple ways to check for leaching, and fix crazing.
Hazards Copper Compounds Toxicology

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy