Desertalc

Description: Originally from Johns-Manville

Oxide Analysis Formula Tolerance
SiO2 59.20% 1.37
MgO 23.50% 0.81
Al2O3 0.81% 0.01
Fe2O3 0.25% -
CaO 5.80% 0.14
Na2O 1.23% 0.03
K2O 1.21% 0.02
TiO2 0.04% -
LOI 7.96%n/a
Oxide Weight 127.98
Formula Weight 139.04

Notes

From our information, this is the forerunner of Pioneer talc.
The chemistry is a little different, but that could be attributed to variation in the material, different blending, mining location, etc.

Related Information

Links

Materials Talc
A source of MgO for ceramic glazes, a flux or thermal expansion additive in clay bodies, also used in the manufacture of cordierite.
Materials Pioneer 2661 Talc
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.
Hazards Talc Hazards Overview
Talc is invaluable in the ceramics industry, it is used as a glaze and body ingredient and as a parting a release agent in various processes. Is it safe?

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy