Ag2O | AlF3 | As2O3 | As4O6 | Au2O3 | BaF2 | BeO | Bi2O3 | CaF2 | CdO | CeO2 | Cl | CO | CrO3 | Cs2O | CuCO3 | Dy2O3 | Er2O3 | Eu2O3 | F | Fr2O | Free SiO2 | Ga2O3 | GdO3 | GeO2 | HfO2 | HgO | Ho2O3 | In2O3 | IrO2 | KF | KNaO | La2O3 | Lu2O3 | Mn2O3 | MoO3 | N2O5 | NaF | Nb2O5 | Nd2O3 | Ni2O3 | OsO2 | Pa2O5 | PbF2 | PdO | PmO3 | PO4 | Pr2O3 | PrO2 | PtO2 | RaO | Rb2O | Re2O7 | RhO3 | RuO2 | Sb2O3 | Sb2O5 | Sc2O3 | Se | SeO2 | Sm2O3 | Ta2O5 | Tb2O3 | Tc2O7 | ThO2 | Tl2O | Tm2O3 | Trace | U3O8 | UO2 | WO3 | Y2O3 | Yb2O3

K2O (Potassium Oxide)

Data

Co-efficient of Linear Expansion 0.331
Frit Softening Point 707C (From The Oxide Handbook)

Notes

-Together with sodium and lithium oxides, it is classified as one of the Alkaline group. Colored glazes whose flux portion is alkaline-dominated tend to be visually intense, especially if the alumina is low.

-K2O is considered together with sodium, since the two almost always occur together and have very similar properties. When taken together the two are often labeled KNaO. K2O generally promotes higher melt viscosity than Na2O.

-It is an important auxiliary flux in high temperature glazes.

-It is a heavy oxide and in general hosts the brightest colors of all fluxes except for lead. It is usually preferred even to soda for a more brilliant glossy glaze and longer firing range. Very good colored glazes can be made in K2O-PbO-SiO2 dominant formulas.

-Considered a very stable and predictable oxide.

-Like sodium, it has a very high expansion, this tends to contribute to crazing in higher amounts, but not quite as bad as sodium. Thus high alkali glazes almost always craze. If the color depends on this (i.e. copper blue), then it may be necessary to adjust the body to eliminate crazing (since a reduction of the alkalis to reduce crazing will mean a loss of color).

-The alkalis can increase lead solubility.

Links

Materials Cornwall Stone
Materials Sylvite
Materials Pearl Ash
Materials Pearl Ash Calcined
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Nepheline Syenite
Materials Potash Feldspar
A feldspar having a KNaO content that predominates in potassium.
Glossary Flux
Fluxes are the reason we can fire clay bodies and glazes in common kilns, they make glazes melt and bodies vitrify at lower temperatures.
Glossary Ceramic Oxide
In glaze chemistry, the oxide is the basic unit of formulas and analyses. Knowledge of what materials supply an oxide and of how it affects the fired glass or glaze is a key to control.
Glossary Alkali
Minerals K-Feldspar
Most common feldspars contain both sodium and potassium. The term K-Feldspar designates one where th
Minerals Feldspar
An indispensable material in the ceramic industry. Most ceramic bodies employ feldspar as a flux to
Oxides Na2O - Sodium Oxide, Soda
Oxides KNaO - Potassium/Sodium Oxides

Mechanisms

Glaze ColorAlkaline glazes with barium and small amounts of Mn can produce pink.
Glaze ColorReduction tenmoku black-rust glazes with 8-10% iron work well in high potash glazes.
Glaze Color0.5-1.0% iron in potassium reduction glazes may give delicate blue to blue green.
Glaze ColorCopper red reduction glazes are best in formulations with high alkali. The presence of boron can give a more pleasant red.
Glaze ColorOxidation copper blues work best in high alkaline, low alumina glazes. Increasing copper to 4-6% will move color toward turquoise.
Glaze ColorCobalt blues can be very intense in alkali glazes (up to 2% cobalt).
Glaze ColorAlkaline dominant glazes will produce violet, purple, burgundy, red blue using manganese dioxide to 2%.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy