0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Formula | Oxide Interaction | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Mold Natches

At digitalfire we are big fans of slip casting and want to help people and companies (even hobbyists) to integrate it into their production.

Key phrases linking here: mold natches, natches, natch - Learn more

Details

3D design and 3D printing are enabling a rethink of almost every detail of how molds are made. The way in which natches are incorporated into working molds, what natches need to be and even if they need to be there at all, are all on the table. The precision of 3D-printing can really be leveraged to imagine and create new ways of interlocking multipiece molds.

At its simplest, incorporating natches in mold parts is simply incorporating holes in 3D printed shells to accommodate clips or retainers (and what they connect to, either a natch or an embed). Natches and spacers can then be inserted (and glued) into the embeds after the plaster has set. The biggest benefit of this is being able to sand flat mating surfaces (before gluing in the natches).

More advanced options involve fitting natches to already created working mold parts. This is done by the incorporation of smooth recessed 3D printed platforms to which natch hardware can be positioned and epoxied.

While natches can be purchased, the other hardware needed to embed them necessitates 3D printing anyway. So you might as well print the natches also. Making them all yourself enables not only flexibility in shape and size but also assures that you will never be caught out of stock.

Related Information

Standard 3/8 inch Self-Interlocking Mold Natch

We can 3D print these and improve them

Available on the Downloads page


Standard 3/8 inch mold natch

This picture has its own page with more detail, click here to see it.

Once you try these you will never go back to the use of registration keys in traditional mold making. Unfortunately, these natches are not easy to get in North America. Or even online. But you can 3D print them yourself (I use PLA filament, but TPM would be a good option). This design interlocks with standard 3/8" natches used in industry. There are more aspects to printing and using these than meets the eye. Here are some things we noted (and changed):

-The base can be widened for better sticking on the build plate.
-Glue the build plate on your 3D printer to make sure these stick well.
-The inner edge is chamfered to ensure better insertion of the nipple.
-Print without infill for better strength.
-These are hollow; no print support is needed.
-The bottom can be widened to stick better to the build plate.
-The ribs can be moved.
-A 9.8 mm hole is needed in the mold.

Once we moved to the use of CAD and 3D printing of block and case molds, these were abandoned in fovor of a four-part system.

v1 DIY Four-Part Mold Natch System

Essential for 3D mold-making in ceramics

Available on the Downloads page


3D printed mold natches

This picture has its own page with more detail, click here to see it.

Plastic natches are used in traditional mold making for slip-cast ceramics (instead of registration keys). They are cast into plaster molds to provide durable and good-fitting interlocks between pieces. They are self-interlocking, a popular size is the 3/8" or 9.5 mm (nipple diameter) natch. However, these have not proven suitable for the mold making process described on this site. The Digitalfire four-part system accommodates 3D printing (usually using PLA filament) case molds for pouring plaster, block molds for pouring rubber case molds and even hybrid solutions. Here are some features of our system:
-13.5mm holes in 3D printed case molds are all that is needed to adapt to these.
-3D printing case and block molds necessitate pouring plaster and rubber into shells with planar mating surfaces downward that must sit flat on the work table (traditional natches don’t work in this setting).
-Casting an embed into a mold enables gluing (or friction fitting) a natch or a spacer inside.
-The use of embeds permits flat mating surfaces, these can be sanded (for better flatness and fit). They also allow replacing natches if they get broken.
-A set of four interlocks (4 embeds, 4 clips, 2 spacers, 2 natches) weighs 8.7g.
Consider starting with a 0.1mm allowance (e.g. 4.8mm nipple inside a 4.9mm space). Print all four to check for fit. Then do cycles of adjusting the allowances and printing again until they fit.

DIY natches, spacers and embeds in a plaster handle mold


Natches, spacers, embeds in a plaster handle mold

This picture has its own page with more detail, click here to see it.

This is our third-generation alternative to the use of traditional mold natches (like the red ones in the photo). Here is what you are seeing:

Right: A 3D-printed case mold for a mug handle. Clips (retainers) have been inserted from the bottom side. An embed has been pushed down over the one in the rear.

Center: The plaster mold created from it. The embed at the rear is ready for inserting a spacer (the nipple of the other half will it into that). A natch has also been inserted into the embed in the front. These fit tight enough in the hole that glue was not needed here.

Left: Spacers have been inserted into both embeds. A standard natch fits into the one in the rear and one of our natches fits into the one in the front.

Soon the CAD drawing for these (natches, spacers, embeds, clips) will be available on digitalfire.com.

Slotted natches make this bottle mold possible


Slotted natches in a slip casting mold

This picture has its own page with more detail, click here to see it.

These enable pulling apart the top halves of our ceramic beer bottle molds while the leather hard bottle is still embedded into the base. Starting upper left and clock wise:
#1 The 3D design for making a rubber case mold.
#2 It has been 3D printed in three parts (which are then glued together).
#3 PMC-746 rubber was poured in and the 3D printed parts were peeled off.
#4 Natch parts have been 3D printed.
#5 The embeds have been rubber cemented onto the rubber mold (to hold them in place during casting).
#6 Plaster was poured in.
#7 The plaster working mold has been extracted from the rubber, the embeds firmly rooted in place.
#8 The slots have been epoxied in place (lined up and positioned accurately so the natches hit the end of the slots just as the halves contact).
Centre: The mold partly assembled.

Why 3D design and printing is a better way to make slip casting molds


3D printed plaster mold master

This picture has its own page with more detail, click here to see it.

I dread the traditional mold making process, the mess, all the supplies and tools involved. I am a potter, I make functional ceramics. I am not a mold-maker, but 3D design and printing have put it within my reach. This way more fun! There is no stopping this, it’s the future.
-I spend most time on design, pouring the plaster or rubber takes minutes.
-Many fewer tools and supplies are needed, the process is less messy, as easy as downloading a file, printing it and pouring in plaster - this is doable in my kitchen! I don't even need mold soap!
-Sanding of flat mating faces is possible (for better seams than I've ever had). This is because natches can be added later (using embeds).
-I can make my own natches and interlock schemes.
-No spare is needed, the 3D-printed pour spouts work better.
-The range of shapes seems limitless. Especially because designs can be split up into pieces, each printed in optimal orientation (and glued together).
-I make molds through multiple design-print iterations. 3D makes do-overs or changes in design as easy as a reprint and plaster-pour. So, I can make a mold just to test an idea!


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 