0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Interaction | Oxide Molecular Formula | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Molecular Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Ceramic Material

Ceramic materials are employed in the ceramic industry to make glazes, bodies, engobes and refractories. We study them at the mineral, chemical and physical levels.

Key phrases linking here: ceramic material - Learn more

Details

Ceramic materials are employed in the ceramic industry to make glazes, stonewares, earthenwares, porcelains, engobes, refractories, structural products, etc. We study ceramic materials at the mineral, chemical and physical levels.

At first it might seem strange to define this, but it is not as obvious as it seems. In ceramics the concept of a material is different for different people. To a purchasing agent it is a commodity. To a geologist it is a mineral or mix of minerals. To someone most concerned with the physical presence, ceramic materials are an inorganic, non-metallic solid. To a mining crew materials present various challenges in extraction, transport, initial crushing and stockpiling. To a processing department they present sets of issues to grind, separate, purify, size and package. To a production department they are powders that make up part of the recipe of a glaze or body and have associated issues and benefits in process equipment. To a lab technician materials have a physical presence that can be tested and the results of these tests can be expressed on a data sheet. Labs can also deduce the chemistry of a material. To a glaze chemist, materials are "warehouses" of oxides for use in formulations (manufacturers publish their chemistries), each having physical and process side-effects that must be taken into account (recipes theoretically become 'material independent', oxides being supplied from whatever materials are at hand). To a body formulator, ceramic materials offer properties that influence forming and fired properties (e.g. plasticity, fluxing power, thermal expansion.

Related Information

A material storage rack


This picture has its own page with more detail, click here to see it.

This material storage area employs a rack to keep pails off the floor so the area can be hosed down easily. The materials in each pail are sealed in plastic bags or the pail is covered with a lid.

Refined 200 mesh materials are not guaranteed to be such


This picture has its own page with more detail, click here to see it.

Each of these eight pallets of kaolin are being sampled to screen them for oversize particles. The 50 gram samples needed can be taken without having to open the bags, they are filled through a valve at the top and it can be opened easily. Kaolins and ball clays especially are suspect and body manufacturers must be vigilant about this (each can tell you disaster stories about making product with faulty raw materials containing grit, carbon and iron particles). The samples will be washed through 70, 100 and 150 mesh screens to spot any particles that could introduce grit or fired speckle into the bodies.

Raw red burning clay stockpile


This picture has its own page with more detail, click here to see it.

The raw Plainsman M2 clay stockpile before it is ground. This is mined in Montana and imparts red color to various middle and low temperature clay bodies. It is a remarkably consistent material.

When both mineralogy and chemistry are shown on a data sheet


This picture has its own page with more detail, click here to see it.

Some material data sheets show both the oxide and mineralogical analyses. Dolomite, for example, is composed of calcium carbonate and magnesium carbonate minerals, these can be separated mechanically. Although this material participates in the glaze melt to source the MgO and CaO (which are oxides), it's mineralogy (the calcium and magnesium carbonates) specifically accounts for the unique way it decomposes and melts.

Do not rely on material data sheets, do the testing


This picture has its own page with more detail, click here to see it.

The cone 6 porcelain on the left uses Grolleg kaolin, the right uses Tile #6 kaolin. The Grolleg body needs 5-10% less feldspar to vitrify it to zero porosity. It thus contains more kaolin, yet it fires significantly whiter. Theoretically this seems simple. Tile #6 contains alot more iron than Grolleg. Wrong! According to the data sheets, Grolleg has the more iron of the two. Why does it always fire whiter? I actually do not know. But the point is, do not rely totally on numbers on data sheets, do the testing yourself.

What can you do using glaze chemistry? More than you think!


And Insight-Live screenshot

This picture has its own page with more detail, click here to see it.

There is a direct relationship between the way ceramic glazes fire and their chemistry. These green panels in my Insight-live account compare two glaze recipes: A glossy and matte. Grasping their simple chemistry mechanisms is a first step to getting control of your glazes. To fixing problems like crazing, blistering, pinholing, settling, gelling, clouding, leaching, crawling, marking, scratching, powdering. To substituting frits or incorporating available, better or cheaper materials while maintaining the same chemistry. To adjusting melting temperature, gloss, surface character, color. And identifying weaknesses in glazes to avoid problems. And to creating and optimizing base glazes to work with difficult colors or stains and for special effects dependent on opacification, crystallization or variegation. And even to creating glazes from scratch and using your own native materials in the highest possible percentage.

Bulk 2500 lb bulk bags of Pioneer Kaolin


This picture has its own page with more detail, click here to see it.

The material is much less dense than most other ceramic materials (that is why these bags are so tall). When moved the powder within becomes unstable and they are prone to falling over.

Do ceramic material powders go bad?


This picture has its own page with more detail, click here to see it.

Many minerals are just ground up rocks, they were in the ground for millions of years (e.g. kaolin, feldspars, ball clays, bentonite, calcium carbonate, dolomite, talc, kyanite, wollastonite, etc), so the powders should last millions of years as well. Some are powderized man-made glasses and sintered solids, these are very stable (e.g. frits, stains). Other man-made materials are less stable and can hydrate or oxidize (e.g. carbonate colors, plaster), keep them sealed containers. Some materials are organic (e.g. Gum Arabic) and they can go bad in damp conditions, so keep them in a sealed container also.

The recipe mixing area in the Plainsman Clays lab


This picture has its own page with more detail, click here to see it.

This is my lab work area of mineral, frit, chemical, stain and metal oxide powders for mixing test glazes and clay bodies. Not shown is my propeller mixer, perhaps the most important piece of equipment we have. And my plaster table for dewatering clay body slurries. Building up something like this, over time, is practical for any serious potter, most of these powders are inexpensive. Within minutes I can plan and enter a recipe into my Insight-live.com account, give it a code number, print it and weight it out.

This is what a semi-trailer load (40,000 lbs) of talc looks like


This picture has its own page with more detail, click here to see it.

Talc is not nearly as dense as many other materials. If this was silica these pallets would be half this height.

Ceramic materials can vary widely in density


This picture has its own page with more detail, click here to see it.

A bag of magnesium carbonate beside a bag of feldspar. Although the former weighs 25 kg (vs. 22.7 kg for the feldspar), clearly it is a dramatically lighter (per volume unit) material. Lifting that bag of Mag Carb feels like lifting a pillow!

New Zealand Kaolin original container


This picture has its own page with more detail, click here to see it.

The original bag of this product in 2014.

50 lb bag of soda ash (or sodium carbonate).


This picture has its own page with more detail, click here to see it.

Soda Ash is soluble and is thus not useful in most ceramic glazes. However that very solubility makes it very useful to control the electrolytics of ceramic slurries. This is the dense variety, non-hydrous.

An original container of manganese dioxide


This picture has its own page with more detail, click here to see it.

This bag will give you a clue as to what manganese dioxide, MnO2, is mainly used for. Staining bricks.

Original container of Rockwood Lithium Carbonate


This picture has its own page with more detail, click here to see it.

An original container bag of Tricalcium Phosphate


This picture has its own page with more detail, click here to see it.

Links

Projects Materials
Glossary Ceramics
This term generally refers to the industry that produces the non-metallic objects we use every day (like porcelain, tile, glass, stoneware).
Glossary Theoretical Material
In glaze chemistry, theoretical materials are used to represent what a material would be if it was uncontaminated and perfectly crystallized
Glossary Material Sense
Ceramic glaze and body recipes often need material substitution or just scrutiny. Knowing the chemistry, mineralogy and physical properties of the materials is invaluable.
URLs http://www.ilo.org/public/english/protection/safework/cis/products/icsc/dtasht/index.htm
International Labour Organization Chemical Safety Database
URLs http://www.matweb.com/
MatWeb Materials Properties Database

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy