0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Formula | Oxide Interaction | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Clays for Ovens and Heaters

Thermal mass heating ovens (such as Rocket Mass ovens or heaters, Cob ovens, pizza or baking ovens) employ heat sinking mechanisms to store energy. Their construction often involves the use of heavy blocks (purchased or made) and raw clay mixed with sand and/or straw or other fibre to cement the whole thing together. Dried clay mix is obviously not as strong as cement, but it is quite practical for this application (e.g. much less expensive, adequate strength coupled with easy construction, disassembly and adjustments).

Some sources recommend using a Fireclay because these can withstand the temperatures in the oven. However, this is not really correct. Red hot coals in a campfire are only about 1000-1200F, even the lowest duty clay (e.g. terra cotta) is capable of easily withstanding temperatures to 1800F+. Fireclays (or clays in general) come in a wide range of plasticities, water permeabilities, drying performances, etc (these properties are an important practical issue to constructing the oven). Plainsman Clays, for example, most often recommends their 98Mix (a very plastic greenish-colored terra cotta raw quarry clay). It dries hard and strong and maintains plasticity even when blended with significant sand.

Some sources advise simply digging clay out of the ground and mixing it in a certain proportion with sand. This might have worked for the author with his clay and sand, but will it work for you? Sands and clays vary widely in grain size and shape (that variation can multiply to orders of magnitude difference in grain surface area). Clays vary widely in plasticity (ability to form a shape), stickiness, drying hardness, permeability, drying speed and drying shrinkage. The most plastic clays (e.g. 98Mix mentioned above) are the stickiest and shrink and crack the most. They can host higher percentages of sand, which cuts the shrinkage, yet still dries hard and strong. While pottery clays might be plastic for building pottery most dry fairly fragile. Most pottery clays dry shrink about 6.5% whereas a superplastic terra cotta or ball clay might shrink 8-10%. And dry like concrete! Of course, you must experiment with varying proportions of sand (plus fiber) to find a compromise between something that will dry with minimal cracking and still be hard and strong enough.

To withstand the rain a roof is often needed to shed water and protect from direct rain (a dried clay might seem hard, but it will slake and turn back into mud when it comes into contact with water). Alternatively, a plaster or stucco finish can be employed. Or apply a sealant layer or add a hardener/sealant to your clay mix (e.g. silicone, corn starch, polymers, gums). If you choose to use an in-mix hardener, do plenty of testing to make sure it will work, hardeners can reduce plasticity significantly.

Related Information

A Thermal Mass Pizza or Baking Oven


This picture has its own page with more detail, click here to see it.

Lower section is metal construction, dome is clay and brick with stucco surfacing. Door is cement and brick. Fire is started inside to heat it up, then ash is removed for baking. By Bruce Fochler, Prince George, B.C.

Inbound Photo Links


Uzume thermal mass oven in operation
Mass-Wood stove project at Wooly Ewe yarn shop in Smithers, BC

Links

URLs https://en.wikipedia.org/wiki/Rocket_mass_heater
Rocket Mass Heater on Wikipedia
A form of slow-release radiant heating system, designed to primarily heat people and secondary to warm areas in line of sight around it.
URLs http://buildnaturally.blogspot.ca/2013/06/build-clay-cob-oven-in-your-yard.html
Build a Clay Oven in Your Backyard
Lots of pictures and text with plenty of viewer comments at the bottom.
URLs https://www.fornobravo.com
US manufacturer of pizza ovens and fireplaces
They make modular and assembled pizza ovens, wood and gas fired brick ovens for homes, outdoor kitchens, restaurants, and mobile businesses. They have an impressive gallery with many pictures of completed ovens. Lots of technical resources and accessories.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy