0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Formula | Oxide Interaction | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Water Content

Water content is one of the most important and most misunderstood variables in ceramics. Almost every ceramic process depends on controlling it. Water affects plasticity, drying behavior, shrinkage, density, rheology, strength, casting rate, pressing behavior, glaze application and even dust generation. In many situations, the amount of water present is not just a convenience variable; it is the property that determines whether a process works or fails.

Plastic clay bodies exhibit ideal working properties only inside a surprisingly narrow water-content window. Small changes can dramatically alter stiffness, plasticity and drying behavior. For example, a porcelain body that throws well on the potter's wheel at 21–22% water may become short and difficult at 19%, while a RAM-pressed version of the same body may intentionally target that lower value. Highly plastic ball-clay bodies can often tolerate wider water ranges than porcelains because they retain workability at lower moisture levels.

The amount of water also strongly affects drying shrinkage and drying performance. More water generally means greater particle separation and therefore greater shrinkage during drying. Bodies formulated for low shrinkage often target the minimum water content needed for forming. Coarse particles, grog and non-plastics reduce the amount of water needed and therefore reduce drying shrinkage and cracking risk.

Casting bodies are defined largely by their water content and specific gravity. Deflocculants enable slips to remain fluid at lower water percentages. A casting slip at a specific gravity of 1.75-1.8 contains far less water than an equivalent slurry mixed without deflocculation. This lower water content is critical because it speeds casting rates, increases plastic strength and reduces drying shrinkage. Excess water in a casting slip slows production because more water must migrate into the plaster mold before a layer can form.

Glazes are equally dependent on water content. Dipping glazes are normally adjusted to a target specific gravity and then fine-tuned rheologically using gums, flocculants or deflocculants. A glaze with too much water applies too thinly and dries slowly; too little water causes excessive thickness, cracking during drying. Brushing glazes generally contain much more water and gum to improve brushability and prevent rapid drying. Industrial glaze application on sanitaryware or electrical porcelain often employs very dense glaze slurries with much lower water percentages than hobby glazes.

Spray drying depends entirely on controlled water content. Clay slurries are atomized into heated air to produce granules containing carefully controlled residual moisture, often around 5–7%. These granules must contain enough water to compact properly during pressing but not so much that they stick or deform.

Water content also determines whether raw materials can be ground efficiently. Clays containing too much moisture cannot usually be dry-ground because they agglomerate and coat grinding surfaces. Powders intended for pneumatic conveying, hopper feeding or silo storage require low enough moisture to flow freely. Even small increases in moisture can convert a free-flowing powder into one that bridges, cakes or plugs equipment.

The relationship between water and clay exists at several levels. Some water is simply free water between particles. Some is mechanically held on particle surfaces. Some exists as interlayer water within clay crystal structures. And some is chemically combined water that is part of the mineral itself. This last category contributes to LOI (loss on ignition). For example, kaolinite contains chemically combined water that is driven off as the mineral converts to metakaolin.

Water content is commonly measured by weighing a wet sample, drying it completely, and weighing it again. The percentage is then calculated as:

(wet weight - dry weight) / wet weight * 100
​
Some technicians instead calculate water percentage based on dry weight:

(wet weight - dry weight) / dry weight * 100

This method produces larger numbers and is common in soil science and industrial processing, so it is important to know which convention is being used.

In production environments, water content is monitored constantly because consistency depends on it. Pugged clay, pressing powder, casting slip and glaze slurries are often tested daily. Even a 1% change in water content can alter forming behavior enough to affect productivity and defect rates. For this reason, water percentage is not merely a laboratory measurement in ceramics, it is one of the primary process-control variables.

Related Information

How much powder is in this jar of ceramic glaze?

Here is how to derive that.


Weighing a glaze sample

This picture has its own page with more detail, click here to see it.

In order to add 0.5% CMC gum to this already-mixed glaze I need to know how much powder is present. Here’s how:

Put a teaspoon of the slurry (well stirred) on the tared-tray of an accurate gram scale. In this case it weighed 5.04g. The tray was just dried under a heat lamp, the scale now reports 2.46g. The water content of the slurry is thus (5.04 - 2.46) / 5.04 * 100 = 51.2% (making the solids content 48.8%). The glaze slurry weighs 645g. 48.8% of that = 315g of powder. 0.5% of 315 = 1.6g of CMC gum to blender mix into this.

Links

Tests LOI/Density/Water Content
LDW LOI, density and water content test procedure for plastic clay bodies and porcelains
Glossary Clay Stiffness
In ceramics, clays exhibit plasticity in accordance with their recipe but also the water content. Each types of forming method has an ideal combination of stiffness and plasticity.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy