0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | | Drying Shrinkage | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Formula | Oxide Interaction | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Drying Performance

In ceramics, drying performance is very important to optimizing production. More plastic clays shrink more and crack more, but they are also better to work with.

Key phrases linking here: drying performance - Learn more

Details

Refers to the ability of a clay to dry without cracking (excluding process factors). Lab results for drying factor (DFAC test) and drying shrinkage (SHAB test) along with observations of the material's performance in actual use can give a well-rounded picture of its drying performance. Of course, the expected performance is always related to the type of ware being made and the economic and convenience costs associated with drying it the necessary way to avoid drying cracks.

Clay having a lower drying shrinkage normally dries better (without cracking). However, it can also dry poorly if lacking excessively in dry strength. Likewise, clays with higher drying shrinkage normally dry more poorly. But good dry strength can help them dry better than you might expect (also because stronger clays have higher plasticity and thus dry slower). Adding an aggregate or fiber to a plastic body can greatly improve its drying performance (because of shrinkage reduction, greater permeability to water passage and micro-crack termination by the larger particles). In fact, bodies that would be very difficult to dry on their own can be superior driers if they contain lots of grog.

Drying performance tests can be done in simple ways. Typical ones normally accelerate the drying of one section of a sample while slowing down water release in another section. This sets up a situation where the rigid section resists the shrinkage of the undried section. Differences in the type of failure provide opportunities to rate one clay against another.

Drying performance is best viewed as the coupling of a clay body of known capability with a process tailored to it. When cracking occurs there are generally many measures that can be taken to improve the drying process. As an interesting example, a large studio reported a "handle failure rate" of less than 1% - by workers and students despite greatly increasing the speed of their process. This was possible because the focus was put on evenness of drying.

Related Information

It is not the speed of drying, but how even it is


This picture has its own page with more detail, click here to see it.

Half of these Plainsman Polar Ice mugs cracked. But I know exactly why it happened! After throwing them I put them on a slowly rotating wheelhead in front of a fan to stiffen them enough so I could attach the handles quickly. Of course, I forgot them and they got quite stiff on the lip (while the bottom was still wet). I quickly attached the handles and then covered them with cloth and plastic and let them sit for two days to let them even out. Notwithstanding that, that early gradient sealed their destiny. The lesson: At no time in the drying process should any part of a piece be significantly ahead of another part.

Can you dry a mug with handle in two hours? Yes.


This picture has its own page with more detail, click here to see it.

The lid of my firing kiln seems to be just the right environment for even drying, even of freshly thrown pieces. By the time this mug really got under way here the kiln was at 1000F and the lid was getting pretty hot. The bottom was the warmest and the top coolest, the exact opposite of how drying normally becomes uneven (the top drying first). This principle could be employed to make a heated drying chamber. The interior space could be kept at high humidity and a draft of air through it could remove humid air and the needed rate.

It is impossible to dry this clay. Yet we did it. How?


Two dried pottery mugs

This picture has its own page with more detail, click here to see it.

These are made from a 50:50 mix of bentonite and ball clay! The drying shrinkage is 14%, more than double that of normal pottery clay. These should have cracked into many small pieces. Yet notice that the handle joins with the walls are flawless, not even a hairline crack (admittedly the base has cracked a little). Remember that the better the mixing and wedging, the smaller the piece, the thinner the walls, the more even wall thickness, the better the joins, the fewer the sharp contour changes, the more even the water content is throughout the piece (during the entire drying cycle) and the damper the climate the more successful drying will be. What did it take to dry these in our arid climate? One month under cloth and plastic, changing the cloth every couple of days. Implementing these same principles on a normal clay body will assure drying success.

Worst case scenario for handle joins and successful drying


Leather hard mugs with waxed handles

This picture has its own page with more detail, click here to see it.

These M390 mugs had progressed to stiff leather hard (after handles were applied, using just slip, and bases trimmed). A white engobe was then applied to the inside. It significantly softened the bodies of the mugs (to re-dry them to the point of being able to turn them over takes 4-6 more hours). This process sets up a big moisture differential between the mug and handle. "Even drying" is the key to success, so slowing down the handles is obviously needed. How? I apply wax emulsion (actually, I like Reed Wax), leaving just the inside handle-curves bare. That slows down drying enough to keep them even with the body of the mug. This method works so well that these do not even need covering during drying (even in our desert climate). Even drying is the goal - fast and even drying is much better than slow and uneven.

Wanna throw porcelain plates with thick bottoms and thin rims?


A large freshly thrown plate

This picture has its own page with more detail, click here to see it.

They need ten days to dry in our climate! This 14" plate has been thrown with a 1" thick base. The rim is a quarter of that. During the first few hours, the rim would dry quickly, leaving the base far behind. So as soon as it will support the weight of a cover-cloth I put it under that and plastic for several days. After that has to be cut off with a wire (there is a lot of clay here, it waterlogs the bat). The rim is stiff enough to support it for trimming but the base will still be quite soft. Thus, it is doubly important to trim it deep enough to create a cross-section of even thickness. Then, to try to even out the water content between base and rim I place it under layers of cloth and under plastic for several more days. Finally, out of the bag, it dries, with cloth still covering it. Even then, the base may bow upwards or crack. These are difficult, there is no getting around it!

Designing your own humidity controlled tunnel drier


This picture has its own page with more detail, click here to see it.

The ideal drying chamber is a tunnel. Typical tunnels pass wheeled-ware-carts single file. Hot dry air enters where the ware exits. The moving air touches all surfaces and picks up humidity as it moves toward the entrance. The tunnel must be calibrated so that air reaching the entrance, is still very warm and laden with water it got from ware down the tunnel. When an equal volume of ware is passing constantly, manual calibration of cart movement, air volume and temperature is possible. But if flow is not constant multi-location monitoring and intervention is needed. ESP8266/ESP32 controllers are revolutionizing industrial control. As cheap as $5, these tiny battery-powered WIFI servers can display a web page, email or text you and communicate with an online dashboard to relay measurements. And they can respond to commands and actuate relays to control blowers, heaters and vents. Hiring a technician on Upwork.com to design a system is only a matter of a few thousand (even hundreds) of dollars. Shown here is an Amazon listing for a development kit of an 8266, sensor and cables (the humidity/temperature sensors are the key element, search for them specifically on Amazon). Shown also is a listing for a ready-made one, dozens of these will be found for the search "esp32 humidity temperature sensor controller". Greenhouse automation uses this same technology.

Do grog additions always produce better drying performance?


This picture has its own page with more detail, click here to see it.

This DFAC test for drying performance compares a typical white stoneware body (left) and the same body with 10% added 50-80 mesh molochite grog. The character of the crack changes somewhat, but otherwise, there is no improvement. While the grog addition reduces drying shrinkage here by 0.5-0.75% it also cuts dry strength (as a result, the crack is jagged, not a clean line). The grog vents water to the surface better, notice the soluble salts do not concentrate as much. Notice another issue: The jagged edges of the disk, it is more difficult to cut a clean line in the plastic clay.

DFAC disk under a heatlamp


This picture has its own page with more detail, click here to see it.

The heat lamp dries the out edge in minutes (this photo makes it appear hotter than it really is). The center section of the disk is protected by the glazed bowl and takes an hour or more to dry. This sets up stresses that cause the disk to crack. The nature and size of the cracks enable establishing a drying factor value for the clay.

A typical DFAC drying disk of an iron stoneware clay


This picture has its own page with more detail, click here to see it.

The center portion was of this DFAC test disk was covered and so it lagged behind during drying, setting up stresses that caused the disk to crack. This test is such that most pottery clays will exhibit a crack. The severity of the crack becomes a way to compare drying performances. Notice the test also shows soluble salts concentrating around the outer perimeter, they migrated there from the center section because it was not exposed to the air.

How to interpret the crack in a DFAC drying disk


This picture has its own page with more detail, click here to see it.

Drying disks used for the DFAC test are 12cm in diameter and 5mm thick (wet). A crack pattern develops in almost all common pottery clays as they shrink during drying. This happens because the center portion is covered and stays soft while the perimeter dries hard. This sets up a tug-of-war with the later-drying inner section pulling at the outer rigid perimeter and forcing a crack (starting from the center). If the clay has high plasticity and dry strength it can pull so hard from the center that cracks appear at the outer dried edge to relieve the tension. Or, it can create cracks that run parallel to the outer edge but at the boundary between the inner and outer sections. The nature, number and width of the cracks are interpreted to produce a drying factor that can be recorded.

Inbound Photo Links



Fibers visible along a broken edge of a dried paper clay slab

A dry cracked pottery mug
It dry shrinks much more yet cracks less. How is that possible?


Various grogs available in North America


Large particle grogs are difficult to produce


Grog does not always have the intended effect

Links

Tests Drying Factor
The DFAC Drying Factor test visually displays a plastic clay's response to very uneven drying. It is beneficial to show the relative drying performance of different clays.
Glossary Firing Shrinkage
During drying, clay particles draw together and shrinkage occurs. During firing the matrix densifies and shrinkage continues. More vitreous bodies shrink more.
Articles Drying Ceramics Without Cracks
Anything ceramic ware can be dried if it is done slowly and evenly enough. To dry faster optimize the body recipe, ware cross section, drying process and develop a good test to rate drying performance.
Troubles Cracking of Clays During Drying
The best way to avoid drying cracks when making ceramics or pottery is to avoid doing the things that cause it. Do not just blame the clay, anything can technically be dried.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy