0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Formula | Oxide Interaction | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Permeability

In ceramics, the permeability of clay slurries and plastics determines the rate as which water can move through the matrix

Key phrases linking here: permeability - Learn more

Details

The term permeability is used in several ceramic contexts. Most often, it describes how readily water can move through a clay—either through a compacted powder, a dried clay body, or a layer deposited from a slurry.

Particle size and surface area have a major influence. Bentonites consist of extremely fine particles having enormous surface area and are among the least water-permeable clays. They also dry very slowly. When bentonite powder is wetted, the outermost particles can swell and form a gel layer only a few millimetres thick. That layer may become nearly impermeable, preventing additional water from penetrating into the dry powder beneath it.

Kaolins generally have much larger particles and lower surface areas. Some are relatively non-plastic and highly permeable to water, enabling them to wet and dry much more quickly. Certain non-clay minerals can also resist water penetration, so permeability is not determined by plasticity alone.

Interestingly, a clay that has already been thoroughly mixed into a plastic mass is normally quite impermeable. The plate-like particles are packed closely together, and the remaining pore channels are very small. After that same clay has been completely dried, however, shrinkage cracks and interconnected pores permit water to enter. The piece can then slake rapidly as water penetrates between particles and breaks it apart.

Permeability is especially important in slip casting. Water must pass from the slurry through the growing clay layer and into the porous plaster mould. A highly permeable casting slip builds thickness quickly, whereas a slip containing more extremely fine clay particles generally casts more slowly. Those fine particles may be desirable because they increase plasticity and dry strength, but they can also reduce casting rate and make dewatering more difficult.

Manufacturers therefore need a repeatable way to measure permeability. One method is the Baroid permeability test, performed in a small pressure vessel fitted with filter paper or a membrane and a liquid outlet. The slurry is placed under a specified pressure for a set time. The amount of liquid expelled is measured, and the deposited filter cake can be removed, weighed and measured for thickness. The test provides useful information about both filtration rate and cake-forming behaviour.

The very low permeability of bentonite is also valuable outside ceramics. In agriculture, pond construction, landfill liners and geotechnical applications, compacted bentonite can swell to seal pores and greatly restrict the movement of water.

Related Information

Permeability of Texas and Montana talcs:

Larger round particles vs tiny platelet particles


This picture has its own page with more detail, click here to see it.

Texas talc (left) quickly absorbs all the water poured on it. Montana talc (right) resists whetting of the particles much more, the water is just sitting on top and has not penetrated at all.

The Montana material is more pure, and it is a platy talc. Talc platelets expose broad basal water repellent surfaces that are difficult for water to wet. When these fine plates settle parallel to the surface, they can form a tightly packed, water-repellent layer with very small pore entrances. Surface tension and trapped air then prevent water from entering, so it remains pooled on top.

The Texas is chemically and physically different. It contains appreciably more calcium-bearing material and other non-talc components. It also has rounder, fluffier and substantially coarser particles. These characteristics provide larger, better-connected pore passages and more readily wetted mineral surfaces. Once water enters those pores, capillary suction quickly pulls it through the powder.

A stock pile of raw, unground ball clay


This picture has its own page with more detail, click here to see it.

Plainsman A2 ball clay. In spite of three times the normal rainfall this summer, its natural high impermeability made it shed almost all of the water. But there is a back story. When mined, this clay was quite wet, about 10% moisture - some of the lumps are microwave-oven-sized! The outer ones dried over a period of weeks and, in the process, fractured down to what you see here. But the inner section of the pile takes years to dry out. By now it has broken down so fine that a completely dry sample put into water will slake in minutes to produce a smooth slurry. We can thus say that the pile has been "weathered".

A few drops of water on top of a tiny pile of bentonite powder.


This picture has its own page with more detail, click here to see it.

Notice the water just sits there in a little lake. It does not soak in because the bentonite gels in contact with the water and that gel acts as a non-permeable barrier. This water-barrier property of bentonite is a key to its use in many products. When ceramic bodies and glazes contain bentonite, they dry more slowly. In industrial settings, this can slow down production. But in studio settings, slower drying can enable more time to work with the material and more opportunities to intervene to make sure drying is happening evenly throughout.

Links

Materials Ball Clay
A fine particled highly plastic secondary clay used mainly to impart plasticity to clay and porcelain bodies and to suspend glaze, slips and engobe slurries.
Materials Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries.
Materials Bentonite
Bentonite can make a clay body instantly plastic, only 2-3% can have a big effect. It also suspends slurries so they don't settle out and slows down drying.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy