Description: Washed
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 54.14% | 0.80 | |
| K2O | 9.01% | 0.08 | |
| MgO | 4.20% | 0.09 | |
| Na2O | 1.45% | 0.02 | |
| P2O5 | 3.43% | 0.02 | |
| SiO2 | 2.06% | 0.03 | |
| LOI | 25.70% | n/a | |
| Oxide Weight | 61.27 | ||
| Formula Weight | 82.46 | ||
| Materials |
Cherry Ash
A type of wood ash used as an ingredient in pottery glazes. |
| Materials |
Wood Ash
For centuries, pottery glazes have been made from ash mostly mixed with clay and feldspar. |
| Materials |
Soft Wood Ash
A type of wood ash used as an ingredient in pottery glazes. |
| Materials |
Pine Wood Ash
A type of wood ash used as an ingredient in pottery glazes. |
| Materials |
Eucalyptus Ash
A type of wood ash used as an ingredient in pottery glazes. |
| Materials |
Hardwood Ash
A type of wood ash used as an ingredient in pottery glazes. |
| Materials |
Rice Husk Ash
A type of plant ash used as an ingredient in pottery glazes. |
| Materials |
Rice Straw Ash
A type of plant ash sometimes used as an ingredient in pottery glazes. |
| Materials |
Oakwood Ash
A type of wood ash used as an ingredient in pottery glazes. |
| Typecodes |
Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies. |
| Hazards |
Plant Ash Toxicity
The hazards of using plant and wood ash in ceramic glazes |
| Glossary |
Wood Ash Glaze
Common washed wood ash can supply important ceramic oxides when melted, so it can comprise significant percentages in a recipe. Plus it can produce unique visual effects. |