Alternate Names: Hard wood ash
Description: Washed
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 21.51% | 0.30 | |
| K2O | 33.44% | 0.28 | |
| MgO | 15.85% | 0.31 | |
| Na2O | 2.30% | 0.03 | |
| P2O5 | 16.34% | 0.09 | |
| SiO2 | 0.67% | 0.01 | |
| Fe2O3 | 0.58% | - | |
| MnO | 2.60% | 0.03 | |
| SO3 | 6.71% | n/a | |
| Oxide Weight | 72.66 | ||
| Formula Weight | 77.88 | ||
| Materials |
Cherry Ash
A type of wood ash used as an ingredient in pottery glazes. |
| Materials |
Wood Ash
For centuries, pottery glazes have been made from ash mostly mixed with clay and feldspar. |
| Materials |
Eucalyptus Ash
A type of wood ash used as an ingredient in pottery glazes. |
| Materials |
Soft Wood Ash
A type of wood ash used as an ingredient in pottery glazes. |
| Materials |
Oakwood Ash
A type of wood ash used as an ingredient in pottery glazes. |
| Materials |
Applewood Ash
A type of wood ash used as an ingredient in pottery glazes. |
| Typecodes |
Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies. |
| Glossary |
Wood Ash Glaze
Common washed wood ash can supply important ceramic oxides when melted, so it can comprise significant percentages in a recipe. Plus it can produce unique visual effects. |