These are pure Custer feldspar and Nepheline Syenite. The coverage is perfectly even on both. No drips. Yet no clay is present in the mix. The secret? Epsom salts. I slurried the two powders in water until the flow was like heavy cream. I added more water to thin and then started adding the Epsom salts (powdered) as it mixed. After only a pinch or two, they both gelled. Then I added more water and more Epsom salts until they thickened again and gelled even better. The result is a thixotropic slurry. They both applied beautifully to these porcelains. The gelled consistency prevents them from settling to a hard layer (which they would otherwise do in seconds).
Could you do this with pure silica? Yes. Of course, this is just a demonstration of the power of Epsom salts (that's why no attempt was made to measure amounts). No potter or manufacturer would attempt to put a clayless slurry method into production as a dipping glaze without any additives.

This picture has its own page with more detail, click here to see it.
This is a slurry of pure feldspar. A tiny addition of powdered Epsom salts flocculates it enough that it can remain suspended for days; without that, the watery slurry settles very quickly. Remarkably, it can even be applied to absorbent bisque despite containing no clay. But suspension is only one requirement of a usable glaze slurry. The deposited feldspar layer is extremely permeable, so the bisque sucks water through it almost unhindered. The coating therefore builds at remarkable speed—the piece must essentially be dipped in and out with no dwell time. Then a second problem appears. While the coating is damp, it can be handled, but after drying it has almost no strength: The feldspar particles form a fragile, easily disturbed powder layer. The Epsom salts have solved suspension, but not binding.
Some industrial dipping glazes likewise contain little or no clay. They compensate using organic binders and rheology modifiers such as CMC gum. These retain water, control application behavior and, especially important here, bind the particles together after drying so the glazed ware can survive handling before firing.

This picture has its own page with more detail, click here to see it.
This stoneware mug was glazed inside and halfway down the outside with pure silica. At some point during heatup the outside layer, not shrinking like the piece, simply fell down. And was sintered enough to hang together and remain intact through the rest of the firing (on the inside, the shrinking forced the silica to flake off into a pile at the bottom). Cone 10 has sintered the silica enough that it will not slake in water but it is fragile and soft and must be handled carefully.

This picture has its own page with more detail, click here to see it.
Crackle glazes are often thought of simply as recipes that somehow produce a crack pattern. However, crackle is a glaze/body fit phenomenon, not simply an intrinsic visual property of the glaze. They have very high levels of Na2O and/or K2O (collectively, KNaO). These two have the highest coefficients of thermal expansion, by far, of oxides commonly found in pottery glazes. Feldspars, and particularly nepheline syenite, can supply them in abundance.
Shown here is the 77E10A recipe, originally from Luke Lindoe. It is simply Nepheline Syenite and water (shown on three types of clay bodies). Of course, this won't suspend in water so special measures are needed to make it suitable as a dipping glaze or brushing glaze. Think of it as an on-ramp to understanding more about this type of glaze. 77E10A1 and 77E10A2 are improvements on this; both provide a path to develop and adapt it for your needs.
![]() |
Watch Thixotropy Happen With a 20kg Batch of Dipping Glaze
I mixed 20kg of glaze powder into 20kg of water, turned out super watery. Yet the specific gravity was 1.46, too high. How? But, instead of more water, I added Epsom salts—and boom: A perfect thixotropic gel. It glides on smooth, no drips, no thickness issues. |
| Troubles |
Powdering, Cracking and Settling Glazes
Powdering and dusting glazes are difficult and a dust hazard. Shrinking and cracking glazes fall off and crawl. The cause is the wrong amount or type of clay. |
| Glossary |
Thixotropy
Thixotropy is a property of ceramic slurries of high water content. Thixotropic suspensions flow when moving but gel after sitting (for a few moments more depending on application). This phenomenon is helpful in getting even, drip-free glaze coverage. |
| Materials |
Epsom Salts
Employed in ceramics as a flocculant to thicken and gel suspensions by electrostatically charging particles so that they attract each other. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
Buy me a coffee and we can talk