These plates are made at the HomeVSS factory in China. The plate is placed on a soft rubber-surfaced spinning wheelhead that is rotating fast enough that a ladle full of glaze poured into the center is expelled within a second and dries within four seconds. At the two-second mark, a sponge is used to catch drips and even coverage on the lip. The thixotropic character of the glaze enables the quick drying (since no CMC is needed). The plate is finished by a follow-up bottom-dip, using a suction cup holder. Finally, the lip is finished using a brush with the same glaze slurry. Watch this on Instagram using the link below.
| URLs |
https://www.instagram.com/reel/Db6gU0fCuMZ
Factory worker glazing bisque-fired plates by spinning and dipping Their process involves using a thixotropic glaze slurry that dries incredibly fast. |
| URLs |
https://homevss.com/collections/plates
HomeVSS tableware factory in China Crafting high quality table ware since 1990. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
Buy me a coffee and we can talk