These bars have been fired at cones 4, 2, 02, 04 (top to bottom) using the SHAB testing procedure. We can measure fired shrinkage and porosity in each to get an indication of their fired maturity. The Redart (left) is much more vitreous and reaches almost zero porosity by cone 4 whereas the Lizella still has 11% porosity at cone 4. Lizella also has a much higher drying shrinkage (because it is way more plastic).
| Materials |
Lizella Clay
|
| Materials |
Redart
The most common commercially 200 mesh available raw terra cotta clay in North America. It fires red, has low plasticity and matures a low kiln temperatures. |