1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Epsom Salts

Alternate Names: Magnesium Sulfate, HEPTAHYDRATE, hydrous magnesium sulphate

Description: Flocculant

Formula: MgSO4.7H2O

Oxide Analysis Formula Tolerance
MgO 16.36% 1.00
LOI 51.14%n/a
SO3 32.51%n/a
Oxide Weight 40.30
Formula Weight 246.48

Notes

Colorless transparent crystals. Also known as magnesium sulphate.

Magnesium sulphate is commonly employed in ceramics as a flocculant. Its dissolved ions reduce the electrostatic repulsion between suspended mineral particles, allowing them to associate into a loose three-dimensional structure. The resulting slurry develops yield stress: particles remain suspended, and the applied slurry resists running or dripping. This not only suspends them in the slurry but makes them stay put on non-porous surfaces (by virtue of the gelling mechanism). Epsom salts does not “make a slurry thicker”, it changes how the particles associate. The resulting flocculated structure produces suspension, yield stress and thixotropic behavior, very small additions can produce very large changes.

Some finely divided non-clay mineral suspensions can be flocculated. Epsom salts are generally better for flocculating ceramic glaze suspensions than vinegar (although less easily obtained). Calcium chloride is often more effective than both.

One strategy is to make a stock solution (30g dissolved in 100ml of water). If the crystals are added directly, it takes time for them to dissolve and act, and it is easy to overdo it and thicken the slurry too much (if you do not give the crystals time to dissolve). Notwithstanding this, sprinkling in a pinch of the granules and waiting while the mixer runs for a while is a tactile way of being aware of how much you are using.

The addition of Epsom salts is commonly done with engobes. A suitably flocculated engobe develops enough yield stress (gels) to apply evenly and remain in place while drying. Without the Epsom salt addition, it will run and drip (even with a low water content). It is better to add Epsom salts as a saturated solution (rather than in powdered form) since the system is so sensitive to over-gelling if too much is added.

Epsom salt additions can be invaluable for glazes; it enables creating a thixotropic (gelled) slurry that applies evenly, holds in place and goes on in the right thickness on porous or dense bisque ware. When the slurry has a sympathetic specific gravity, about 2g per gallon of Epsom salts is a good starting point. CMC-gummed glazes often respond differently to electrolyte flocculants and may be much less responsive to Epsom salts, so their rheology is normally managed differently. Some glaze slurries respond only weakly because their particles provide relatively little active surface area. Kaolin, for example, normally has much less rheological influence than ball clay or bentonite. A small bentonite addition can greatly increase both surface area and sensitivity to flocculation. When adding a small amount of bentonite to a glaze recipe, an equal weight of kaolin can often be removed so the recipe continues to total 100%. At additions of only 1–2%, this usually has little effect on fired chemistry while greatly increasing the slurry's rheological response.

Flocculant addition is a process adjustment, not really a recipe ingredient. Water chemistry, soluble salts in the materials, clay type, particle size and specific gravity can all change the amount required from batch to batch.

Some clay body manufacturers add Epsom salts to their body mixes. It can counteract deflocculating soluble alkalies, restoring particle association and thereby improving the apparent plasticity, stiffness and working behavior of a body. It is typical to use .2-.3%.

It is sometimes said that Epsom salts can be a helpful addition to glazes containing Gerstley Borate to help prevent particle agglomeration (e.g. about 4 g per 100g of Gerstley Borate). However, this is not our experience; Gerstley Borate gels slurries on its own (in fact, it is famous for over-gelling them), so deflocculation seems a more logical approach.

Related Information

See the magic of thixotropy as I mix a 20kg batch of G2926B glaze

In this video, I mix 20kg of G2926B glaze powder into 20kg of water using our powerful propeller mixer. The resulting slurry is like water, absolutely unusable. Yet on measuring the specific gravity (using a hydrometer because it floats freely) I find that it is too high, I actually have to add more water! How is that even possible? Instead, I add Epsom salts and mix again and the slurry gels and hangs on in a perfectly even layer when I dip the spatula. This is a thixotropic gel, it will apply evenly to bisque ware yet not go on too thickly. We normally recommend a specific gravity of 1.44 for this glaze, but in this case, it seemed watery enough at 1.46 (on use, it will become clear if 1.46 is OK e.g. if it goes onto the ware too thick). If that happens I'll just add water to 1.44 (and more Epson salts if needed). Based on online pricing at this time, coverage is minimum six times and as much as twenty times less expensive than buying jars of transparent brushing glaze (considering both the total powder weight and the specific gravity difference between this and commercial glazes we use).

How stop dripping and running:

Add water! Then make it thixotropic.


This picture has its own page with more detail, click here to see it.

The white slip on the left, L3685Z2, (applied to a leather hard cup) is dripping downward from the rim (even though it was held upside down for a couple of minutes!). Yet that slurry was very viscous with a 1.48 specific gravity. Why? Because it was not thixotropic. The fix? I watered it down to 1.46 (making it runny) and added pinches of powdered Epsom salts (while mixing vigorously) until it thickened enough to stop motion in about 1-2 seconds on mixer shut-off. But that stop-motion is followed by a bounce-back. That is the thixotropy. It is easy to overdo the Epsom salts (gelling it too much), I add a drop or two of Darvan to rethin it if needed. When the engobe is right, it gels after about 10 seconds of sitting, so I can stir it, dip and extract the mug, shake to drain it and then it gels and holds in place. Keep in mind, this is a pottery project. In industry, they deflocculate engobes to reduce water content and then impose thixotropy, but that is more technical than the average potter would want.

The same engobe. Same water content. What is the difference?


Two samples, the same engobe runs but not the other

This picture has its own page with more detail, click here to see it.

The engobe on the left, even though it has a fairly low water content, is running off the leather hard clay, dripping and drying slowly. The one on the right has been flocculated with epsom salts (powdered), giving it thixotropy (ability to gel when not in motion but flow when in motion). Now there are no drips, there are no thin or thick sections. It gels after a few seconds and can be uprighted and set on the shelf for drying.

The engobe on this stainless steel spoon has not cracked in drying or firing. How?


Engobe applied to a metal spoon

This picture has its own page with more detail, click here to see it.

This spoon was dipped into a ceramic dipping engobe, L3954B. It contains no CMC gum, it was only flocculated using powdered Epsom salts. Without the Epsom salts, the engobe runs off, leaving only a film. But, when turned into a thixotropic slurry, it stays on the spoon in an even layer (as a gel), then hardens as it dewaters (left) and finally dries completely (right). With no cracks! It also fires to cone 03 with no cracks. Of course, if this were fired high enough, it would begin to shrink, crack, crawl, melt and then craze, ceasing to be an engobe. Of course, special low-expansion frits and additives and mixing, preparation and application techniques make enamels, which do melt, possible for metals.

Pure feldspar applied as a glaze:

Because of the magic of thixotropy.


Suspending feldspar in water

This picture has its own page with more detail, click here to see it.

These are pure Custer feldspar and Nepheline Syenite. The coverage is perfectly even on both. No drips. Yet no clay is present in the mix. The secret? Epsom salts. I slurried the two powders in water until the flow was like heavy cream. I added more water to thin and then started adding the Epsom salts (powdered) as it mixed. After only a pinch or two, they both gelled. Then I added more water and more Epsom salts until they thickened again and gelled even better. The result is a thixotropic slurry. They both applied beautifully to these porcelains. The gelled consistency prevents them from settling to a hard layer (which they would otherwise do in seconds).

Could you do this with pure silica? Yes. Of course, this is just a demonstration of the power of Epsom salts (that's why no attempt was made to measure amounts). No potter or manufacturer would attempt to put a clayless slurry method into production as a dipping glaze without any additives.

When to use vinegar and when to use epsom salts to flocculate a slurry


This picture has its own page with more detail, click here to see it.

Slurries with more clay (like engobes, slips) generally respond better to epsom salts. However the extra clay also makes them more likely to go moldy, so you may need to add a few drops of Dettol to kill the bacteria (if they are stored for any length of time). Vinegar works better for glaze surries, but only if they have sufficient specific gravity. Many people like to make an epsom salts solution and add that, but if you have a good mixer you may find it more intuitive to add the crystals (which you should crush to a powder) and wait 30 seconds for the viscosity to respond.

30g of Epsom salts dissolved in 100cc of water:

Is this the best way to use it?


This picture has its own page with more detail, click here to see it.

That produces a solution that can be added to glazes and clay slurries to flocculate them. This being said, it is not necessarily a good idea to add it to slurries as a solution, especially if you have a variable-speed propeller mixer. Creating a thixotropic slurry is a delicate business. The initial challenge is discovering a specific gravity that is not oversensitive or undersensitive to an Epsom salt addition (for many of our dipping glazes, this is 1.43-1.44, a fairly watery consistency). While discovering the right amount of Epsom salts to add can be done by adding this solution we have a propeller mixer and actually prefer adding the crystals by the pinch from a pre-weighed amount. We set the mixer speed to enable visually detecting differences in thixotropy and do a cycle of adding a pinch per gallon, let it mix for a couple of minutes and then stopping to check bounce-back (thus gel). At times the salts get over-supplied (easily undone with a tiny amount of Darvan).

Links

Materials Calcium Chloride
Commonly used as a flocculating agent in ceramic glazes (to suspend and gel them).
Materials Vinegar
Vinegar is often used in ceramic slurries to change the viscosity (thicken them).
Hazards Epsom Salts
Temperatures Epsom salts decompose to lose water (150-)
Typecodes Generic Material
Generic materials are those with no brand name. Normally they are theoretical, the chemistry portrays what a specimen would be if it had no contamination. Generic materials are helpful in educational situations where students need to study material theory (later they graduate to dealing with real world materials). They are also helpful where the chemistry of an actual material is not known. Often the accuracy of calculations is sufficient using generic materials.
Typecodes Additives for Ceramic Glazes
Materials that are added to glazes to impart physical working properties and usually burn away during firing. In industry all glazes, inks and engobes have additives, they are considered essential to control of cohesion, adhesion, suspension, dry hardness, surface leveling, rheology, speed-of-drying, etc. Among potters, it is common for glazes to have zero additives.
Glossary Thixotropy
Thixotropy is a property of ceramic slurries of high water content. Thixotropic suspensions flow when moving but gel after sitting (for a few moments more depending on application). This phenomenon is helpful in getting even, drip-free glaze coverage.
Video
Watch Thixotropy Happen With a 20kg Batch of Dipping Glaze
I mixed 20kg of glaze powder into 20kg of water, turned out super watery. Yet the specific gravity was 1.46, too high. How? But, instead of more water, I added Epsom salts—and boom: A perfect thixotropic gel. It glides on smooth, no drips, no thickness issues.

Data

Density (Specific Gravity) 1.68

Mechanisms

Glaze SuspenderUsed to thicken glaze slurries.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 