0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Interaction | Oxide Molecular Formula | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Molecular Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Raku

Gas fired rustic ceramic ware is cooled from red-hot in a closed container with organic material. The zero-oxygen atmosphere produced reduces carbonate metal decoration to its metallic form.

Key phrases linking here: raku - Learn more

Details

The raku process is an economical way of firing ware in reduction to achieve metallic and carbon effects. Normally ware is heated in a kiln until the glaze is melted to the desired degree then it is removed with tongs and put into a container of organic material (i.e. sawdust) where it is cooled. The organic material burns and uses the available oxygen in the container and the metallic effects develop. Because of the thermal shock during heat-up most people bisque fire ware before rakuing.

Raku ware is very porous and lacking in strength (because of the low temperatures employed in the process). Most raku clays are not fluxed to develop any kind of strength and low temperatures. Their weak, coarse fired character is actually needed to enable pieces to survive the heat shock of the cooling process. Raku glazes are almost always crazed. This is because high percentages of sodium are needed to melt them (sodium has the highest thermal expansion of all common oxides). The thermal shock of cooling also adds to crazing. Crazing further weakens ware to the point that it must be handled with great car, thinner pieces can easily be torn apart with ones bare hards. Thus raku ware is only suitable for decorative uses.

Metallic effects that look great out of the firing can tarnish and disappear with time and people have developed ways to preserve these with various fixatives and surface treatments. Do not buy raku ware unless this has been done.

Raku firings often generate a lot of smoke, and people have developed different ways to try to contain this smoke. Unfortunately some have developed and even promoted quite casual methods that pose significant dangers. Raku kilns can emit harmful (even dangerous) metal fumes (depending on how pots are decorated) and vapors of chlorine and sulfur (from salts, chlorides, and sulphates). Inhalation of chlorine can cause chemical pneumonia, immune reactions, rashes, irritated mucous membranes, diarrhea, nausea, vomiting, cancer, brain damage, etc. Smoke from raku is hazardous simply because ALL smoke is hazardous and possibly carcinogenic. Incomplete combustion ("yellow" smoke) produces the most hazardous substances (i.e. wood tar and thousands of other compounds). While some people claim to wear respirators with "smoke blocking filters" there is no such thing. This is why firefighters wear tanks of compressed air.

We do not deal with this process since it falls outside the realm of functionality, predictability and control that we normally advocate. However, one principle does apply: Rather than have different glaze recipes for every effect, find one clear base recipe that has nice slurry properties, melts well and crazes to the degree you want (which could be as simple as 85% frit and 15% kaolin). Then add colorants to get different effects (where possible, employ stains rather than metal oxides and carbonates, they are much less troublesome and don’t produce gases or metal fumes). Avoid a base recipe that calls for Gerstley Borate because it turns slurries into jelly, frits are much better melters (yes, they are more expensive but will save you from so many problems). Be sure to read up on thixotropy, that will enable you to create slurries that work so much better.

Related Information

Texture of a typical raku body after throwing


This picture has its own page with more detail, click here to see it.

This is Plainsman Raku. It has 18% 35-65 mesh grog, 65% Plainsman A3 buff stoneware clay, 14% Pyrax and 3% bentonite. Throwing it on a pottery wheel affords a better sense of the texture than any other method. Apparent texture is a product of a combination of particulate percentage, the distribution of particle sizes, particle shape and distribution of shapes, particle surface topology and the nature of the clay matrix they exist in.

Temporary Raku Kiln


This picture has its own page with more detail, click here to see it.

Used for firing raku test specimens at Plainsman Clays.

What is the simplest, most practical raku base crackle recipe?


A glazed tile showing the raku crackle effect

This picture has its own page with more detail, click here to see it.

Many people suffer high-percentage Gerstley Borate "bucket-of-jelly" raku recipes they find online. Most of these are just transparent base recipes to which colorants are added. After years they found ways to tolerate this strange bedfellow. Now, a more normal material, Gillespie Borate, seems odd and is causing issues in the alternate reality "Ghastly Borate ecosystem". There is a better way. A frit is perfect for this application, Ferro Frit 3110 (or Fusion frit F-75). All it needs is 15% kaolin (e.g. EPK) to produce and easy-to-use recipe that is guaranteed to craze. The degree to which it crazes can be adjusted by trading off some of it for Ferro Frit 3249. We have assigned it a code number of L4264, a raku base transparent recipe. We have also catalogued some common recipes that people use and outlined the issues they have: L4264A, L4264B, L4264C, L4264D. Do you need a white? It is a simple matter of adding 10% Zircopax to this.

Links

Glossary Thixotropy
Thixotropy is a property of ceramic slurries of high water content. Thixotropic suspensions flow when moving but gel after sitting (for a few moments more depending on application). This phenomenon is helpful in getting even, drip-free glaze coverage.
Glossary Primitive Firing
The use of some traditional firing techniques is still popular among modern potters and sculptors (who are accustomed electric and gas kilns, often with computer controllers).
Materials Kyanite
A refractory aluminum silicate mineral notable for low thermal expansion and one-way volume expansion as it converts to mullite at high temperatures.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy