0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Interaction | Oxide Molecular Formula | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Molecular Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Ceramic Oxide

In glaze chemistry, the oxide is the basic unit of formulas and analyses. Knowledge of what materials supply an oxide and of how it affects the fired glass or glaze is a key to control.

Key phrases linking here: ceramic oxide, oxides - Learn more

Details

An oxide is a combination of oxygen and another element. There are only about ten common oxides that we need to learn about (most glazes have half that number). CaO (a flux), SiO2 (a glass former) and Al2O3 (an intermediate) are examples of oxides. CaO (calcium oxide or calcia), for example, is contributed by calcium carbonate, wollastonite and dolomite.

The heat in the kiln "decomposes" materials into their oxides. This decomposition breaks the bonds that held the oxides together in their materials, creating a liquid "melt" (or mixture) of unbonded oxide molecules (ready to form a new compound, normally a glass, when the kiln cools). This phenomenon occurs because the molecular bonds that hold oxides together are stronger than those that hold oxides to one another.

There are direct links between the oxide chemistry of a glaze and its fired presence; each oxide imposes specific properties (according to its concentration) on the fired glass. Its effects can be modified by interactions. Glaze chemistry is about looking at mixtures of raw material powders as if they were already the fired glaze. It does an inventory of all the oxides being contributed by all the materials, discards the ones that will gas off during firing (e.g. CO2, SO4, H2O) and tries to visualize what the glass will be like.

A glaze "oxide molecular formula" expresses relative oxide molecule numbers in the fired glass (a "chemical analysis" expresses the concentration of each oxide, by weight of molecules, in a material). Oxides are divided into three categories that recognize their functions. There is a correlation between the amount of oxygen in each class and the contribution that class of oxide makes. Fluxes are designated RO, intermediates R2O3 and glass formers RO2. When the links between how a glaze fires and its oxide formula are well understood, the glaze formula can be manipulated to produce the desired changes in the fired properties.

"Target Formulas" (or limit formulas) characterize the balances of oxides in a type of glaze (e.g. low temperature, crystalline, matte). However, limit formulas are general guides only, they express what is likely to melt into a usable glaze.

Glazes for lower temperatures have more flux. We see that in unity formulas as lower SiO2 and Al2O3. Some of the properties that oxides contribute can be quantified. Thermal expansion is an example. Na2O, for example, has a very high expansion. SiO2 is low. We know the thermal expansion of each oxide; thus, it is fairly simple to tabulate their expansions, according to percentage, to predict the thermal expansion of the glaze (high-expansion glazes craze). When the SiO2:Al2O3 ratio is high (e.g. 12:1), the glaze will likely be glossy (matte when low). If MgO is 0.3 or higher (in a unity formula) the glaze will likely be matte. If Al2O3 is low, the glaze melt will be runny. If SiO2 is also low, it will melt at a low temperature.

Related Information

A limit or target glaze formula. What does this mean?


A glaze formula compared to a target formula

This picture has its own page with more detail, click here to see it.

Recipes show us the materials in a the glaze powder (or slurry). Formulas enumerate the oxide molecules and their comparative quantities in the fired glass. Oxides construct the fired glass. The kiln de-constructs ceramic materials to get their oxides, discards the carbon, sulfur, etc. and builds the glass from the rest. There is a direct relationship between fired glaze properties (e.g. melting range, gloss, thermal expansion, hardness, durability, color response, etc) and its oxide formula. There are 8-10 oxides to know about (vs. hundreds of materials). From the formula-viewpoint materials are thus "sources-of-oxides". While there are other factors besides pure chemistry that determine how a glaze fires, none is as important. Insight-live can calculate and show the formula of a recipe, this enables comparing it side-by-side and with a target formula (or another recipe known to work as needed). Target formulas are opened using the advanced recipe search, choosing the limits batch and clicking/tapping the search button (search 'target recipe' in Insight-live help for more info).

Oxide effects on frit physical properties


This picture has its own page with more detail, click here to see it.

When both mineralogy and chemistry are shown on a data sheet


This picture has its own page with more detail, click here to see it.

Some material data sheets show both the oxide and mineralogical analyses. Dolomite, for example, is composed of calcium carbonate and magnesium carbonate minerals, these can be separated mechanically. Although this material participates in the glaze melt to source the MgO and CaO (which are oxides), it's mineralogy (the calcium and magnesium carbonates) specifically accounts for the unique way it decomposes and melts.

Ionic Forces Chart


This picture has its own page with more detail, click here to see it.

Cations having high charges and small radiuses (and thus high field forces like boron and silicon), are network formers. Network modifiers have small charges, large radiuses and a big coordination number for oxygen ions. While considering ions as rigid spheres is an over-simplified way to describe reality, it has still proven useful to describe characteristics of each. For instance lithium has a ionic radius smaller than sodium and so it can locate into smaller cavities. The ionic field force of lithium is also stronger than sodium and it is essentially non-directional, thus it more easily produces crystals of a separate phase. Alkaline earth elements locate into cavities of the network as well, but they have double charges and thus act like a bridges between two oxygen ions (preventing the three-dimensional network from being fully destroyed). Moreover bonds between alkaline earth ions and oxygen are stronger than alkaline so we observe neither a rapid decrease in viscosity or a significant increase of the thermal expansion coefficient. It is notable that for similar molar percentages, frits containing magnesium crystallize more easily than frits containing calcium.

Aluminum, titanium and zirconium are classified as intermediate glass formers because they have a strong four-way coordination for oxygen ions, like silicon. Thus, for these oxides, we do not observe any interruption of the three-dimensional silicate-based network. For a better understanding consider more details about aluminum, boron, zirconium and titanium.

Aluminum: Usually aluminum shows a four-way coordination when it acts as a glass former, tetrahedrons are linked to four oxygen atoms while the local excess of negative charge is counterbalanced by an alkaline cation placed close to the aluminum ion. Thus additions of aluminum to a glass help to stop alkaline ions from breaking the three dimensional network of the glass. This produces the characteristic lower melt fluidity and tendency to crystallize and also reduces the thermal expansion and thermal stability. One downside to alumina is that it contributes to a higher viscosity of frit batches during melting (in the furnace tank) making homogenization more difficult. Usually the percentage of aluminum oxide is in the range 4 – 12%.

Boron: Boron is a basic component of frits yet its characteristics are so peculiar that it cannot easilly be compared to other elements. Boron, like aluminum, exhibits a four-way coordination when forming a glass network (being in the center of a tetrahedron of oxygen ions). This is possible only when the molar alkaline percentage is less than 30-40% because above this limit boron has three-way coordination, forming triangles.

Another peculiar characteristic is that boron is not just dispersed as tetrahedrons or triangles in the network of silica tetrahedrons. Rather it forms boric groups, containing from 3 to 5 boron atoms and the groups are randomly dispersed in the glassy matrix. However single BO3 triangles and BO4 tetrahedrons are always present. For quenched frits the presence of these groups is likely minimal but we can presume they form again when glazes containing the frit are fired (there are experimental evidences demonstrating this).

Boron oxide is an important component of low melting frits because it increases fusibility without a proportional increase in thermal expansion. Moreover boron oxide and sodium borate, due to their low melting point, are useful during smelting of frits because they form a glassy matrix early and act as catalysts in the melting and dissolving of other materials.

Zirconium - Titanium: Their influence on surrounding oxygen ions is very strong and scarcely directional so their solubility in frits is poor. Their solubility in glass and actions as glass formers are proportional to temperature. In quenched frits they remain in the dissolved in the glassy matrix but when we fire them again (within a glaze), these oxides easily precipitate crystal compounds.

Inbound Photo Links

Periodic table of ceramic oxides
Ceramic Oxide Periodic Table

Links

Projects Oxides
Oxides MgO - Magnesium Oxide, Magnesia
Oxides Na2O - Sodium Oxide, Soda
Oxides K2O - Potassium Oxide
Oxides B2O3 - Boric Oxide
Oxides SiO2 - Silicon Dioxide, Silica
Oxides KNaO - Potassium/Sodium Oxides
Oxides Al2O3 - Aluminum Oxide, Alumina
Oxides CaO - Calcium Oxide, Calcia
Glossary Limit Formula
A way of establishing guideline for each oxide in the chemistry for different ceramic glaze types. Understanding the roles of each oxide and the limits of this approach are a key to effectively using these guidelines.
Glossary Chemical Analysis
In ceramics, raw material chemistry is expressed a chemical analyses. This is in contrast to fired glaze chemistries which are expressed as oxide formulas.
Glossary Decomposition
In ceramic manufacture, knowing about the how and when materials decompose during firing is important in production troubleshooting and optimization
Glossary Glaze Chemistry
Glaze chemistry is the study of how the oxide chemistry of glazes relate to the way they fire. It accounts for color, surface, hardness, texture, melting temperature, thermal expansion, etc.
Glossary Alkaline Earths
Refers to a group of ceramic fluxing oxides that contribute similar properties to fired glazes. They contrast with the alkalis which are stronger fluxes.
Glossary Oxide Molecular Formula
In ceramics, the chemistry of fired glazes is expressed as an oxide formula. It expresses the relative molar proportions of the oxides contributed by a glaze recipe. There are direct links between the oxide chemistry and the fired physical properties.
Glossary Mineralogy
Raw ceramic materials are minerals or mixtures of minerals. By taking the characteristics of these into account technicians can rationalize the application of glaze chemistry.
Articles Where do I start in understanding glazes?
Break your addiction to online recipes that don't work or bottled expensive glazes that you could DIY. Learn why glazes fire as they do. Why each material is used. How to create perfect dipping and brushing properties. Even some chemistry.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy