0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Interaction | Oxide Molecular Formula | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Molecular Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Plaster table

Essential in a pottery studio for dewatering reclaim clay, stiffening clay that is too soft or making your own clay bodies.

Key phrases linking here: plaster table - Learn more

Details

Every serious potter, studio, school and lab needs a plaster table. The bigger the better. Plaster is porous, it can absorb a lot of water. Thus, when a clay slurry is poured onto a plaster surface the water is pulled out of it. The speed at which the water can be removed is determined by the permeability of the mix, more plastic clays are less permeable. On a dry table if is often possible to dewater a slurry to throwing consistency in a very short time (e.g. 30 minutes). Also, clay does not stick to plaster, that makes it a perfect surface for wedging. And it is great for setting freshly wheel-thrown ware (to pull water out of the thicker, and thus slower-drying base).

If you live in a wet climate, water may not evaporate from a table fast enough. You can solve that by emulating the industry practice of making molds air-releasable (especially important in RAM pressing operations). Molds are made with internal ductwork and a compressed air fitting/coupler. On pressurization air travels outward through the plaster's capillary system, releasing the just-pressed object. A side benefit is that the escaping air also purges the plaster of water that may be blocking the capillaries, it bubbles out with the escaping air. This same principle can be adapted to a plaster table by incorporating molduct tubing (available at Lagunaclay.com) making it possible to quickly purge water.

Some potters are sworn to avoid plaster in their workflow, likely due to a bad experience of getting plaster contamination into a body. But if a table is kept in good condition this will not occur. While there are other proven techniques for dewatering slurries (e.g. hanging it in canvas bags or putting it in bisque containers), without a pugmill a porous plaster slab is still needed for the final stages to fine tune the stiffness.

Related Information

A plaster table: Better than a pugmill, essential for testing


A plaster table

This picture has its own page with more detail, click here to see it.

This is an example of an angle iron utility table being made into a plaster table. The cardboard sides extend upward to make the slab thicker and create a buffer gap to prevent the expanding and setting plaster from pressing outward on the frame. 150 lbs plaster (92 lbs water) was poured into the plastic-lined space (the bottom cardboard sections were supported from below). In a dry enough climate, this table could make enough clay to support slurry-to-plastic production for a potter (a thicker slab and a fan would enable even more capacity). The slurry-up process is better than a pugmill for small operations. It's much cheaper and is an easier way to utilize scrap material and weigh out custom recipes. The clay quality and de-airing is better (without hard chunks and contamination common to pugmilling). The procedure generates much less dust and the tank is easily cleaned. Slurries are easily sieved, especially if you have a sieve shaker.

Resurface your plaster table and make it like new!


A plaster table and a capenter's plane

This picture has its own page with more detail, click here to see it.

This plaster slab is about 5 years old. I have used it to dewater many raw clays that contain significant soluble salts. Over time they sealed the surface with a hard scum. That not only made the table slower to dewater slurries but it also significantly slowed down the time it took for water to evaporate out of it. Using this carpenter's plane I removed about half a millimetre. The blade self-sharpened. It took some experimentation to set it at a depth that would effectively remove the hard layer. I thought it would produce grooves and unevenness in the surface, but it did not. Sanding was not necessary. And the first slurry stiffened quickly, like a freshly-poured slab, and there were no bits of plaster in it.

Sanding the surface of a plaster table to keep it absorbent


This picture has its own page with more detail, click here to see it.

The water that a plaster table absorbs from clay slurries contains soluble salts. They penetrate into the plaster and then come back out to the surface as the water evaporates, forming a hard and less absorbent layer. Variable absorbency in a plaster surface can easily be observed as it is cleaned with a sponge and water. Fortunately, that layer is very thin and can be removed by sanding. Plaster is durable and can serve for decades using this technique. These durable fabric sand paper screens work exceptionally well because they can be used with water and to not blind. They are available in hardware stores and sold as drywall sand screens. We have seen 150, 120 and 80 grit (the latter is the one used here).

Pouring the slurry on a plaster table to dewater it


This picture has its own page with more detail, click here to see it.

Pottery plaster is highly absorbent, it can remove the water from this thick slurry, made from a 5 kg powder mix, in an hour. Slurries of higher water content dewater much quicker, a 1 kg mix can be ready in minutes. This table weighs 400 lbs dry, but smaller ones are equally practical for smaller test batches. Plaster tables are much more practical in arid climates, it is dry here so one this size can supply enough clay for production of a potter. In wetter climates ductwork can be installed within the plaster and air pressure can be used to dewater the table. If you need one of these, photos are linked to our plaster table article.

A plaster table makes a good base as a drying box


Freshly thrown porcelain mugs placed on a plaster table and being covered by a wax-lined box

This picture has its own page with more detail, click here to see it.

These mugs are on a plaster table, freshly thrown on the wheel. I made the box cover from a large sheet of cardboard and painted wax emulsion on the inside. When left overnight under the box the mugs dewater evenly, the plaster pulls water from the air in the box and directly from the thicker bases. If I am worried they will stiffen too much overnight I water down the plaster to keep the humidity. When things are right, in the morning they are stiff enough for handle attachment and to turn over to ready them for trimming. An advantage of this method is that I can throw ware minutes before closing time, come back in the morning, and they are ready. And pieces do not experience the unevenness in drying that happens typically when pieces are left to air dry (after throwing) until they are stiff enough to support a cloth and plastic to cover them.

Why are there so many different kinds of plaster?


Screenshot of Laguna clays plaster products page

This picture has its own page with more detail, click here to see it.

The Laguna catalog is striking for the number of different kinds of plaster they stock (at the time of this writing: fifteen). This catalog is an eye opener to the number of applications in which plaster is used and the number of properties it can offer. Among these are ability to pressure purge, the wet strength or dry strength, setting expansion, setting speed, absorption, density, toolability, suitability for hand layup or carving or layering, ability to surface harden, high density for simulating stone, low water needs, fire resistance and others. Plastic notches and molduct tubing are notable also (these are not generally easy-to-find, the latter is also available at axner.com).

Inbound Photo Links


A plaster bat, or flat disk
Plaster bats are indispensable to the potter

Links

Glossary Propeller Mixer
In ceramic studios, labs and classrooms, a good propeller mixer is essential for mixing glaze and body slurries.
URLs https://www.youtube.com/watch?v=GQLiKLuvatU&authuser=0
Video of water evacuation from plaster by compressed air
These molds have molduct tubing within and a compressed air fitting. The video shows the pressure being applied and the water vapour escaping in clouds.
URLs https://www.lagunaclay.com/
Laguna Clay Co website
URLs https://wiki.glazy.org/t/how-to-make-an-industrial-air-release-mold/812
How to make a forced moisture release plaster mold
URLs https://www.lagunaclay.com/materials
Laguna web page with "Plaster/Mold Making Catalog" link
Projects Making a Plaster Table
Projects Slurry Mixing and Dewatering Your Own Clay Body
Weigh out the ingredients, mix them using your propeller mixer and then dewater and fine-tune the stiffness on your plaster table.
Articles Recylcing Scrap Clay
Guidelines for collecting, reprocessing, testing and adjusting scrap recycle clay in a pottery or ceramics studio or production facility.
Articles Formulating a body using clays native to your area
Being able to mix your own clay body and glaze from native materials might seem ridiculous, yet Covid-19 taught us about the need for independence.
Articles A One-speed Lab or Studio Slurry Mixer
A single-speed lab mixer can be made for much less money than buying a commercial unit. Using it you can slurry up a 100 lb batch of porcelain powder in minutes and it will be smooth as silk.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy