0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Formula | Oxide Interaction | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Glaze Mixing

In ceramics, glazes are developed and mixed as recipes of made-made and natural powdered materials. Many potters mix their own, you can to. There are many advantages.

Key phrases linking here: glaze mixing - Learn more

Details

Potters in affluent places in the world have increasingly adopted commercial brushing glazes as their glazing method of choice. These have some clear advantages but also some important disadvantages (especially related to whether they fit the body, the fact that their recipe is unknown so they are not adjustable and the problem that they take so long to apply and dry slowly). In industry likewise, companies in more affluent countries have changed from mixing their own glazes (and understanding them) to buying them premixed from suppliers (and knowing nothing about their makeup).

Glaze mixing is "swimming upstream" in this river! However, potters and companies in developing countries still make their own glazes. And everywhere there is still a strong movement among potters to adjust and mix their own glazes. It is practical if you can learn about why glazes do what they do, what they need to do to work in your application and you are willing to do plenty of testing to develop your own. Surprisingly, with a little effort, you will find yourself being quite critical of commercial products that you used to use or that competitors still use, finding that many of these are actually quite poorly designed. Armed with an account at Insight-live.com to plan and record your testing work, all all the reference material it provides (like this page), you will be surprised at the results you can obtain.

The way glazes fire is primarily a product of their chemistry. Most glazes are a base transparent with additions to opacify, color, variegate and modify surface texture. The base needs to have the right thermal expansion to fit the body, stay in suspension in the slurry, apply evenly and dry quickly, not be prone to surface defects like pinholes and blisters, not leach or cutlery mark and work with a variety of additives. Other factors include optimization to cut material costs, lower firing costs and be adapted to idiosynchaeies of the body. Additions to that base (depending on percentage) usually affect some of the above properties so extra work is often needed to compensate.

The chemistry of glazes is sourced by ceramic materials. The chemistry is called a "formula". The mix of materials to produce the chemistry is called "the recipe". Recipes are akin to those used in a kitchen. They specify amounts-by-weight (that may or may not sum to 100). You simply recalculate the total and weigh out the needed amount of each powder. Typically around 2500 grams of dry material mix with 2500 grams of water produce a gallon of about 1.45 specific gravity.

Glaze mixing makes the most sense for cover and liner glazes, especially if you want to do production. Glazes for food surfaces carry responsibility and there is no substitute for knowing the recipe and being in control of the properties and fit with your clay body. Liner glazes should typically be uncolored, have low colorant content or employ non-toxic colorants. Of course for decorative, non food surfaces, exotic premixed brushing glazes and layering can make sense in low-production situations.

Glaze mixing is also about rheology, that is, producing a slurry that has good working properties. This is an area where mixing your own glazes can really pay off. It is possible to produce a glaze that goes on silky smooth and evenly and dries within seconds on bisque ware (compared to laborious multi-coat painting and long drying sessions between each coat).

Potters often fall victim to the "illicit online trafficking" of recipes that do not work. Typically these recipes produce some special effect while punishing the potter in many other ways (thus the 'illicit' designation). Not sure what I mean? You will find out! Based on the above-mentioned base-with-additions approach to glazing, it is far better to employ base transparent recipes proven to work with your body and add the colorants, opacifiers and variegators to them to get the effects you want. For reactive glazes, ones that run and crystallize, you can do the same, using a melt-fluid base that you understand and can maintain some control over. Of course, you have all of your testing and trial work recorded in your account at Insight-live.com so you learn from both your successes and failures.

Related Information

Think the idea of mixing your own glazes is dead? Nope!


This picture has its own page with more detail, click here to see it.

These are two pallets (of three) that went on a semi-trailer load to a Plainsman Clays store in Edmonton this week. They are packed with hundreds of bags of powders used to mix glazes. More and more orders for raw ceramic materials are coming in all the time. Maybe you are using lots of bottled glazes but for a cover or a liner glaze it is better to mix your own. And cheaper! And there are lots of recipes and premixed powders here to do it. One of the big advantages is that when you dip ware into a properly mixed slurry it goes on perfectly even, does not run and dries on the bisque in seconds. No bottled glaze can do that.

Better to mix your own cover glazes for production?


This picture has its own page with more detail, click here to see it.

Yes. In this case, the entire outside and inside of the mug need an evenly applied coat of glaze. For hobby, this makes sense. But in production, cover brushing makes less sense. The right pail has 2 gallons of G2934Y base (the most expensive one we use) with 10% Cerdec yellow stain: $135 (in 2023). Cost of brushing jars with the same amount: $600+! And each jar logs 10-15 minutes of painting time plus waiting between coats. The one in the pail is a true dipping glaze (unlike many commercial dipping versions that dry slowly and drip-drip-drip). This one dries immediately after dipping in a perfectly even layer (if mixed as a thixotropic slurry).

Veteran potters never thought they would see the time when people would have never learned or even seen how to weigh out and slurry up a glaze. But it has happened!

The powder blender for making porcelain bodies at Plainsman Clays


This picture has its own page with more detail, click here to see it.

All of the equipment has been washed in preparation for a porcelain run. Original container bags are broken in the dust-hood unit on the right and augered and elevated into the rotating blender/mixer. It feeds a vibrating screen (not visible) that removes paper and other contaminants. For wet clay bodies the screen feeds hoppers on the other side of the wall, they in turn feed the pugmill. For dry bodies and glazes the powder goes to one of the hoppers and that feeds a bagging unit. This type of equipment can handle 1200 lb batches (doing one every five minutes for some products, longer for others).

Links

Glossary Brushing Glaze
Hobbyists and increasing numbers of potters use commercial paint-on glazes. It's convenient, there are lots of visual effects. There are also issues compared to dipping glazes. You can also make your own.
Glossary Digitalfire Insight-Live
A cloud-hosted ceramics-targeted LIMS (lab info management system). It does glaze chemistry and physical testing the “Digitalfire way”. For technicians, educators, potters and hobbyists.
Glossary Glaze Chemistry
Glaze chemistry is the study of how the oxide chemistry of glazes relate to the way they fire. It accounts for color, surface, hardness, texture, melting temperature, thermal expansion, etc.
Articles Where do I start in understanding glazes?
Break your addiction to online recipes that don't work or bottled expensive glazes that you could DIY. Learn why glazes fire as they do. Why each material is used. How to create perfect dipping and brushing properties. Even some chemistry.
Articles Concentrate on One Good Glaze
It is better to understand and have control of one good base glaze than be at the mercy of dozens of imported recipes that do not work. There is a lot more to being a good glaze than fired appearance.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy