0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Formula | Oxide Interaction | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Kiln Controller

In ceramic kilns the firing schedule is typically managed automatically by an electronic controller. But that may not mean that ware gets automatically fired to the correct temperature and atmosphere.

Key phrases linking here: electronic controller, kiln controllers, kiln controller - Learn more

Details

An electronic device attached to a kiln (usually an electric kiln). These controllers are usually capable of firing a kiln to a specific schedule and can shut it off at the right time, soak it for a specified period, and cool it down at a controlled rate. All industrial kilns, electric or gas, have controllers to assure repeatable firing conditions. All modern electric hobby kilns are equipped with controllers. Hobby and pottery gas kilns are also increasingly employing devices to control the schedule as well as the atmosphere.

Controllers for electric kilns work on a duty cycle, switching the power to the elements on for a few seconds, then off for a few seconds. The controller adjusts the on/off durations based on how the temperature is following the program. Technically, the controller switches relays (either mechanical or solid-state) on and off, and they turn the power on and off to the elements. During a firing, relays trigger thousands of times, and you guessed it, they are the most failure-prone part of the system.

Controllers have built-in programs and can also be programmed manually by entering the rate, temperature and hold time for each step. Hobbyists are more prone to rely on the built-in pre-programmed schedules, using these to fire off-the-shelf glazes to low and medium temperatures. However, via manual programming, these controllers have revolutionized our ability to create special-purpose glazes (e.g. crystalline, silky mattes). By creating drop-and-soak schedules (e.g. PLC6DS), they can reduce glaze defects and improve surface quality and brilliance. Slow cool schedules (e.g. C6DHSC) are important to enhancing visual effects that depend on crystal growth (e.g. in rutile glazes) and for mattes.

Even hobbyists have a key motivation for learning to program their controller manually: To be able to fine-tune or even correct the final firing temperature. This is because using the built-in cone-firing programs on many kilns fires well above the temperature a cone would confirm correct. For example, suppose a cone 6 bends to four o'clock at around 2200F on your pyrometer. But the cone fire program fires it to 2232! Obviously, this is going well beyond a cone 6 firing. This is difficult to convey to a pottery community inclined to totally trust controllers on their easiest working mode, it has almost gone to the point that "cone 6", for example, is no longer defined as what an Orton cone indicates, it is defined as "a program option in a controller".

Older kilns can often be retrofitted with controllers. Some integrate tightly into the control of individual elements, these can potentially work well if they come with relays that can withstand the thousands of on/off cycles of a typical firing. Another option is for the controller to have one large super relay, the main kiln power cable plugs into it and it plugs into the wall. These obviously cost more but require no modification to the kiln. Even if the device is guaranteed to work in your kiln a further caution is also in order: Some of the replacements may employ older programmable devices. For example, the Bartlett LED/Keypad V6-CF or 3K controllers are now old and have been superseded by their touch-screen Genesis device.

Many DIY controllers have been made, they are based on microcontrollers or Raspberry Pi computer boards. These are not CSA or UL approved of course, so fire insurance coverage will be implicated. A warning found on one site may affect your decision to try one of them: Most kiln manufacturers state "Do Not Fire Unattended". Commercial controllers deal with many fault modes that this controller does not address. Intermittent thermocouple connections, stuck relay, shorted element and weak elements, these faults have all happened to me and the control just keeps saying "kiln thinks kiln can, kiln thinks kiln can". I had to intervene. Stuck relay and bad thermocouple readings are runaway conditions that could become meltdown/fire/death. "DO NOT FIRE UNATTENDED!"

Another option is to use a kiln monitor, these are independent of kiln control, they just watch using their own thermocouple. Monitors record firing data and enable comparing what happened with fired ware compared with was supposed to happen. Or comparing actual firing curves with intended ones, either in past tense or real time.

Related Information

A test kiln with firing controller: A necessity.


Pottery test kiln

This picture has its own page with more detail, click here to see it.

Every potter should have one of these. Every clay body manufacturer should have one. This one has a Bartlett Genesis electronic controller, you will never go back after having one. Start with a kiln like this and then graduate to having a large, second kiln (or more of these if you are doing lab or development work). We have done 950 firings on this one in the past few of years, it is still like new. Ongoing testing is the key to the constant development of your products and their quality.

Two standalone electric wall-mount kiln controllers. But they are very different.


This picture has its own page with more detail, click here to see it.

The red controller on the right is a Skutt Kilnmaster, the blue controller to the left is an Orton Autofire. As of 2022 both of these are now ancient devices, having been replaced with newer touch panel units. The principle of operation for both is the same: They turn the power on and off in a duty cycle to control temperature rise. A 50% duty cycle, for example, sees the power on for 50% of the time. The length of individual bursts increases with kiln temperature. The controllers monitor a thermocouple in the kiln to determine the length and frequency of power bursts needed. Both of these devices are external to the kilns (but there is a big difference). The KilnMaster controller is attached to the 220V power line and the kiln power line attaches to it (there are heavy-duty electrical relays inside). The blue Autofire controller does not have internal heavy-duty relays or switches, they are in the kiln. The KilnMaster is thus more flexible since it can connect to any kiln, but it is also triple the price. In 2022 the AutoFire now has its own relays like the KilnMaster.

Inside a kiln with a Bartlett Genesis controller


A Bartlett Genesis kiln controller circuit board

This picture has its own page with more detail, click here to see it.

The 220V enters lower left to a terminal block. That splits to a transformer (above) and relays (below that). The 4-07-6024 transformer supplies power to the SMT_3140 controller board (converting the 220V down to that needed by the circuit board). The controller is run by an MSP430 Texas Instruments microcontroller (lower left closeup). That controller has inputs from the thermocouple and a current monitor (yellow donut shape around the wires going to the elements). The board has outputs that connect to the relay, that relay in turn controls the flow of current to the elements. This is a simple device, but not something to be replaced lightly. DIY controller boards documented online look tempting but they are not CSA or UL approved (so fire insurance coverage is implicated). Commercial controllers focus on safety and liability over functionality, they handle intermittent thermocouple connections, bad thermocouple readings, stuck relays and shorted and weak elements - these are runaway conditions that could become meltdowns in a kiln controlled by a DIY device. This being said, these commercial products do have a weakness: The relays. They are mechanical devices and are the first thing to need replacement. Kiln controllers thus need To be good at recognizing relay failure.

Manually programming a Bartlett V6-CF hobby kiln controller


This picture has its own page with more detail, click here to see it.

I document programs in my account at insight-live.com, then print them out and enter them into the controller. This controller can hold six, it calls them Users. The one I last edited is the one that runs when I press "Start". When I press the "Enter Program" button it asks which User: I key in "2" (for my cone 6 lab tests). It asks how many segments: I press Enter to accept the 3 (remember, I am editing the program). After that it asks questions about each step (rows 2, 3, 4): the Ramp "rA" (degrees F/hr), the Temperature to go to (°F) to and the Hold time in minutes (HLdx). In this program I am heating at 300F/hr to 240F and holding 60 minutes, then 400/hr to 2095 and holding zero minutes, then at 108/hr to 2195 and holding 10 minutes. The last step is to set a temperature where an alarm should start sounding (I set 9999 so it will never sound). When complete it reads "Idle". Then I press the "Start" button to begin. If I want to change it I press the "Stop" button. Those ten other buttons? Don't use them, automatic firing is not accurate. One more thing: If it is not responding to "Enter Program" press the Stop button first.

Are you using your expensive kiln like a pop-up toaster?


A small controller-equipment kiln and views of programming it

This picture has its own page with more detail, click here to see it.

Put the pots in, select a cone, press start. It is time to rethink that approach! The Bartlett Genesis kiln controller is standard equipment on hobby and production electric kilns now. It is not meant to be run like a toaster! Good glazes are about much more than recipes, they are about firing schedules. None of the built-in "toaster schedules" have hold times on any segments, drop-and-hold sequences or controlled cools. Or even fire-to-cone accuracy. Yet such are a must for defect-free glazes, enhancing the effects of reactive glazes that must develop crystallization or variegation or firing accurately. It is easy to program: Tap the blue edit button to edit a program, tap a column of any segment to edit its value. Tap a segment number to delete or duplicate it. Search "bartlett genesis controller" on YouTube for videos on creating and editing a schedule.

Program your firings manually

Calibrate the final temperature using cones


This picture has its own page with more detail, click here to see it.

Here is an example of our lab firing schedule for cone 10 oxidation (which the cone-fire mode does not do correctly). To actually go to cone 10 we need to manually create a program that fires higher than the built-in cone-fire one. Determining how high to go is a matter of repeated firings verified using a self-supporting cone (regular cones are not accurate). I keep notes in the schedule record in an account at insight-live.com. And we have a chart on the wall showing the latest temperature for each of the cones we fire to. What about cone 6? Controllers fire it to 2235, we put down a cone at 2200!

Why is the clay blistering on this figurine?


This picture has its own page with more detail, click here to see it.

This is an admirable first effort by a budding artist. They used a built-in cone 6 program on an electronic controller equipped electric kiln. But it is overfired. How do we know that? To the right are fired test bars of this clay, they go from cone 4 (top) to cone 8 (bottom). The data sheet of this clay warns not to fire over cone 6. Why? Notice the cone 7 bar has turned to a solid grey and started blistering and the cone 8 one is blistering much more. That cone 8 bar is the same color as the figurine (although the colors do not match on the photo). The solution: Calibrate the kiln sitter by using a self-supporting cone.

Old-style hobby kilns with a sitter are usable if you become "the controller"!


A hobby kiln with kiln sitter shutoff

This picture has its own page with more detail, click here to see it.

Yes. This kiln has a Dawson LT-3 kiln sitter (new ones have electronic controllers). It is a mechanical device with a safety timer and triggered latch on the external housing. A ceramic tube extends into the chamber where a pyrometric cone sits on supports with a rod on the top center. As the cone softens and bends the rod drops with it and eventually releases the shut-off latch. The utility of this depends on careful placement of the cone, sitter adjustment and keeping the rods and supports in good condition. Although not shown, these kilns had a pyrometer and one or more thermocouples (temperature gauge and heat sensing probes). Is a kiln like this useable today? Yes - if you become "the controller"! Learning to use a kiln like this involves monitoring cones on each shelf (self-supporting cones are recommended). By "babysitting" the switch settings (low, medium, high) during firings and creating paper logs (and graphs) to track the kiln's temperature against time over multiple firings you can evolve a schedule of switch-setting, from low-to-medium-to-high. It is possible to get the desired climb, even heat distribution, achieve the final temperature accurately and even implement drop-and-hold and slow cool firings. Vigilance of changes in the firing speed can be balanced by adjustments to the switch-change times.

Inbound Photo Links


Orton cones bending badly
Cones bending badly, cones bending goodly

Links

Glossary Pyrometric Cone
Cones are ceramic and bend through a narrow temperature range. They used to be actively used to determine when firings were completed but now are used to calibrate electronic devices.
URLs https://en.m.wikipedia.org/wiki/Proportional–integral–derivative_controller
Proportional–integral–derivative Controller on Wikipedia - PID is a control loop mechanism widely used in industrial control systems and the basis on which kiln controllers function.
URLs https://github.com/jdeantoni/KilnRegulator3.0
Kiln Regulator 3
The objective is to provide a cheap and up to date kiln regulator based on an Arduino micro controller and a smart phone app. Had not been updated for 2 years in 2022. Mainly French language.
Typecodes Kiln Controller Device List
If you are aware of devices not listed here please contact us. We want to focus on those in active development. Devices supplied on manufactured kilns are usually relabelled, they are not actually made by the kiln manufacturer.
Projects Build a kiln monitoring device
Projects Firing Schedules
Articles Electric Hobby Kilns: What You Need to Know
Electric hobby kilns are certainly not up to the quality and capability of small industrial electric kilns, being aware of the limitations and keeping them in good repair is very important.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy