0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Formula | Oxide Interaction | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Ball milling

A method of grinding particles in ceramic powders and slurries. A porcelain, metal or rubber vessel filled with pebbles tumbles and particles are ground between colliding pebbles.

Key phrases linking here: ball milling, ball milled, ball-milled, ball mill - Learn more

Details

A device used to reduce the particle size of materials, bodies or glazes. In traditional ceramics, a ball mill is simply a container that is filled with pebbles (either of porcelain or stones e.g. Flint) into which a charge (powder or slurry) is put and that is then mechanically rotated to cause the tumbling pebbles to crush particles that happen between them. Ball mills can be continuous or periodic, they can be small or gigantic, low-speed or high-speed, rotated or vibrated. For maximum efficiency, a ball mill should be made of, or lined with, a porcelain or other very hard surface (so grinding also occurs between the wall and the balls), and the balls should be of a range of sizes (to maximize points of contact), the mill should have the correct quantity of balls, the slurry should be the right viscosity and the charge should be an optimal amount (overcharging reduces efficiency). Various compromises are often made (for example, rubber-lined mills to reduce wear and noise).

Large manufacturers hire ball mill supervisors, operators and mechanics. Commercial mills can be large enough to need 30 tons of balls! Technicians occupy themselves with getting a consistent and predictable processed product (surface area and particle size distribution), they employ mathematical formulas to determine the volume and weight of balls needed, the distribution of ball sizes and other operating parameters like duration and speed. They are wary of grinding products as mixes; it is often better to mill hard and soft powders separately and combine them later. Engineers typically use surface area measurement instrumentation to evaluate mill efficiency. The rheology of wet slurries being processed is also controlled. Milling time and efficiency can be greatly improved by additives to increase cohesion.

Some ball mills can reduce particles to nano sizes (e.g. powders used in hi-tech industries). So, it takes time. To grind a ceramic glaze in a periodic mill might take hours. Industrial mills seeking nano-sizes might run 24 hours or more! Ball milling is normally done in conjunction with wet screening and/or roller-milling/air floating, for example, so that large particles have already been removed by the time the material reaches the ball mill. Air floating can also be done in conjunction with dust ball milling. The milling process can also reduce particle sizes by too much for an application, so a means of measuring the distribution of ultimate particles is important.

A clay body that has been ball-milled will be more plastic, potentially much more plastic. Ball milling of the body, or selected body materials, will reduce or eliminate many types of fired glaze imperfections (especially specking, blistering and pin-holing). That being said, iron particulates are best removed before milling.

As noted, milling a glaze will produce a cleaner-fired result with fewer imperfections. Materials deliver their chemistry to the glaze melt only if their particles fully dissolve in the melt. Consider materials that are refractory and resistant to dissolving (e.g. silica, alumina). When silica does not completely dissolve in a transparent glaze, for example, it will fire cloudy and the actual glaze thermal expansion will not be as low as it could be. However, by ball milling the silica to very small particle sizes, all the particles will dissolve.

Milling of slurries presents fewer technical challenges than dust milling. We have found that thicker creamy slurries mill better than watery ones. A simple ball mill can be constructed by almost anyone, but obtaining the hard pebbles with the correct range of sizes for inside the mill can be a challenge (they are expensive).

In some places, the difficulty of finding specialists who still know how to reline ball mills used for the production of glazes, underglazes and engobes is motivating investment in alternative, more modern grinding equipment.

Ultrafine grinding to nano-scale particle sizes lies largely outside the scope of traditional ceramics. Conventional ball mills used in pottery and ceramic plants are designed to reduce particles into the fine micrometer range, sufficient for glaze suspension, melt homogeneity, and body plasticity, but not for true nano-scale production. Achieving nano-scale particles requires dramatically higher energy input and much more precise control of grinding conditions. For this reason, advanced mills such as attrition mills, stirred-media mills, planetary mills, jet mills, and vibration mills are employed in technical ceramics and high-performance materials industries.

These systems use much smaller grinding media, much higher rotational or vibrational energy, and often carefully controlled atmospheres or liquid chemistries to prevent agglomeration of the ultrafine particles being produced. At nano scale, particles develop enormous surface area and strong surface attraction, so newly created particles tend to re-cluster unless dispersants are used and rheology is carefully controlled. Grinding times can be long, wear contamination from media becomes a critical issue, and even laboratory-scale equipment is expensive compared with traditional ceramic milling systems. For most traditional ceramic applications, the benefits of nano-scale grinding seldom justify the cost because glaze melting, body maturation, and fired appearance are usually fully achieved with much coarser particle sizes.

Related Information

How long do you need to ball mill a glaze?


This picture has its own page with more detail, click here to see it.

You can measure to see. How? Wash a measured amount through a 200 mesh screen and note the amount of residue. These two show the oversize on a 200 mesh screen of 100 grams of glaze slurry. On the left: Unmilled. On the right: Milled 1 hour. Clearly, it needs more than 1 hour in this mill. A factor here is the high percentage of silica in this recipe. And the fact that the coarser grade of US Silica #95 was used (rather than #45).

3D printed spout for ball mill prevents hernias!

Available on the Downloads page


Ball mill jar with spout

This picture has its own page with more detail, click here to see it.

When full of balls and glaze, this Royal Doulton ball mill weighs about 80 lbs. If efforts to pour it out don't cause a hernia, the slurry ends up spilling everywhere as the balls come out with it! Trying to stop the balls with my hand ends up spilling more. The answer was to 3D print two pieces: A spout and a ball retainer (upper right). The bar and screw that normally hold the lid on work well to keep the spout in place. For multiple batches of the same glaze, the jar can now be poured right from our table-mounted rack.

This was drawn in Fusion 360, but it would be doable in any other CAD program capable of revolving, extruding and lofting. I first printed the green ring and flange (without the spout) to achieve a good fit into the neck the jar. This took several prints. It became evident that a better seal is possible by scaling it back enough to make room for a wide rubber band stretched around it. Your jar will, of course, be different than this, so you'll have to custom-design for it. On cation: If printed using PLA filament, don't wash it in hot water or it could deform.

Ball mill jar and rack made by @andygravesstructures


This picture has its own page with more detail, click here to see it.

DIY wheel mount ball mill rack


This picture has its own page with more detail, click here to see it.

Courtesy of Lawrence Weathers

Make your own ball mill rack - Front side


This picture has its own page with more detail, click here to see it.

Possible to grind your own ceramic grade rutile?


Rutile color changes as it is milled

This picture has its own page with more detail, click here to see it.

Yes, the granular and powdered grades of pure rutile are the same material. But, for producers, the milling process it is very difficult because the raw mineral is so hard. Commercial ceramic grade powder is minus 325 mesh, the companies doing this obviously have very good grinding equipment. They also have patience because even in this efficient porcelain ball mill, 90 minutes was only enough to get 50% to minus 325 mesh! The color of the powder is a good indication of its quality, the finer the grind the lighter tan it will be. That means you can use the color to gauge the mesh size. And, if you have a ball mill you can milled it more if needed.

Particle size drastically affects drying performance


This picture has its own page with more detail, click here to see it.

These DFAC testers compare the drying performance of Plainsman A2 ball clay at 10 mesh (left) and ball milled (right). This test dries a flat disk that has the center section covered to delay its progress in comparison to the outer section (thus setting up stresses). Finer particle sizes greatly increase shrinkage and this increases the number of cracks and the cracking pattern of this specimen. Notice it has also increased the amount of soluble salts that have concentrated between the two zones, more is dissolving because of the increased particle surface area.

Can we ball mill a clay and make it more colloidal? Yes.


This picture has its own page with more detail, click here to see it.

This 1000 ml 24 hour sedimentation test compares Plainsman A2 ball clay ground to 10 mesh (left) with that same material ball milled for an hour (right). The 10 mesh designation is a little misleading, those are agglomerates. When it is put into water many of those particles break down releasing the ultimates and it does suspend fairly well. But after 24 hours, not only has it settled completely from the upper section but there is a heavy sediment on the bottom. But with the milled material it has only settled slightly and there is no sediment on the bottom. Clearly, using an industrial attrition ball mill this material could be made completely colloidal.

An hour in a ball mill does less than I thought for this clay


+200 mesh clay particles

This picture has its own page with more detail, click here to see it.

This is all of the oversize on a 35-200# PSD test of a clay body slurry of a 50-gram sample (thus the +200 mesh material). The oversize on the right was measured after 1 hour in our ball mill (porcelain jar). That hour only reduced the total +200 oversize from 7g to 3g. This underscores the amount of energy it can take to reduce the particle size of a ceramic material.

Links

URLs https://colloid-mills.com/colloid-mill-type-o
Colloid Mills - Since 1926 building colloid mills, multi-stage grinding gear and perforated disk mills.
URLs https://www.sbm-mill.com
SBM Shibang Machinery
They manufacture Raymond mills, crushers, vertical roller mills, trapezium mills, ball mills, hammer mills, and vibrating screens for the mineral processing.
URLs http://www.thecementgrindingoffice.com/typesofballmills.html
Types of Ball Mills
URLs https://alpapowder.com
Biggest ultrafine powderizing equipment manufacturer in China 2024
Air Jet Mill, Air Classifying Mill, Classifier, Ball Mill and Classifying, powder surface modification.
URLs https://morehousecowles.com/products/mills/stone-mills/
MorehouseCowles Stone Grinding equipment for continuous particle reduction
URLs https://www.tilemachinery.com
Xiangtan Weida Electrical and Machinery Co., Ltd
They make feeders, crushers and grinders, Raymond mills, ball mills and filter presses, mixers, pug mills, cutting machines, forming presses, setting machines, kilns and dryers. Also production lines for cordierite catalysts, clay roofing, terra cotta facades, tile and ceramic rollers.
Articles Ball Milling Glazes, Bodies, Engobes
Industries ball mill their glazes, engobes and even bodies as standard practice. Yet few potters even have a ball mill or know what one is.
Articles Make Your Own Ball Mill Stand
Pictures of a ball mill rack that you can make yourself

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy