0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Formula | Oxide Interaction | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silica:Alumina Ratio | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Bone China

A ceramic whose priorities are translucency, whiteness, fired strength and resistance to thermal shock failure.

Key phrases linking here: anorthite porcelains, anorthite porcelain, bone china - Learn more

Details

Photo not found
or not published

True bone china is a special type of translucent porcelain. Actually, it is a calcium aluminosilicate glass-ceramic. Traditional porcelain microstructure is mullite + glass, while white bone china is anorthite + glass. Traditional porcelain relies on feldspar as a flux, while bone china relies on calcium from bone ash reacting with SiO2 and Al2O3 (from the kaolin and feldspar) to form the anorthite crystals. The reward is strength and translucency (without brittleness), which is why pieces can be so thin-walled. The amount of feldspar in the recipe and firing temperatures are carefully controlled to enable enough glass formation to bind the crystalline network, promote translucency and enable full densification, but not so much that the crystal structure is adversely affected. Firing must also be carefully tuned to avoid warping because the porcelain becomes pyroplastic near maturity.

Bone ash is used (today available in synthetic form as tri-calcium phosphate). A typical recipe is 50% bone ash, 25% Cornwall Stone (or feldspar) and 25% kaolin. As noted, tuning a firing curve and executing it consistently is a key to ware quality. Quality also hinges on the materials, especially the kaolin, it needs to be low in iron (for whiteness) and low in titanium (for translucency). With only 25% kaolin, the bodies have extremely low plasticity, which limits manufacturing methods (casting is most suitable). As a plastic material, it can only be formed in controlled industrial contexts (e.g. jiggering, jollying).

The glazing process is completely different than what a potter would do: Bisque fire to maximum density, glaze, high fire. Bone china is bisque-fired to high fire and then glazed at a lower temperature. Since the porcelain has zero porosity, typical potters would balk at the process needed to get a glaze to stick and dry on the bisque ware. And they would be surprised at how thin a layer is needed.

Why don't they use calcium carbonate to source the CaO? Because of its high LOI. Calcined bone ash produces no gas and it introduces CaO into the system at the right time and over time so that it reacts more gradually and distributes Ca more uniformly. Bone ash also introduces P₂O₅, which enters the glass phase, modifying viscosity, enhancing crystallization, aiding translucency and altering thermal expansion subtly.

How do they fit glazes on a body that has no silica? Bone china is a phosphate glass ceramic; its thermal expansion is well within the reach of borosilicate glazes.

How do they keep the thin pieces from warping during bisque firing? Custom-made setters for each piece.

Why don't pieces warp in the glaze firing, which may only be 100C lower? The ceramic created in the bisquit firing has surprising rigidity upon refire because the glass phase was already developed and remains stable.

Why did they use lead glazes? First, lead silicate was used (up to 60% PbO), but industry switched to lead borosilicate. Compared to simple borosilicates used in traditional ceramics, they melt lower, flow better, and produce superior optical qualities. They gave a "wet surface" appearance, with brighter gloss, greater depth, and enhanced brilliance. They also increased surface tension control and levelling, and reduced pinholing and minor surface defects. Modern alkali-borosilicate and zinc-borosilicate systems are much less forgiving and less appealing visually. They rely on B2O3 for low melt, KNaO adjustments for fit, ZnO for gloss and melt behavior, and careful silica/alumina balance.

Why is bone china so translucent? The best ceramic achieved has very fine and evenly dispersed crystals and outstanding density (no pores to scatter light). The refractive indices between the glass and crystal phases are also very similar, further preventing light scattering. These factors also combine to achieve high strength and thermal shock resistance.

So-called "fine china" is a marketing term that can refer to bone china, but most often to mullite porcelain (which can be fired much hotter).

The strength, translucency and the process needed to make bone china, are likely well beyond your capability as a potter or hobbyist. Consider other ways to achieve white-porcelain-translucency using more humble materials and firing. Modern controller-equipped kilns enable precise firing, so all manner of mullite porcelains and even fritware are at your disposal. It is even possible to make porcelain-like ceramic down to cone 06 using frit additions (e.g. Zero4 porcelain). This being said, bone china is still within the reach of determined people with studio kilns and a willingness to do a testing program to optimize the body, glaze and process. It will be about data, consider collecting and analyzing it in an account at insight-live.com.

Related Information

Mullite and anorthite porcelains:

The microstructure was only understood recently


Produced by Gemini, combining a picture of a mug I made with a generated bone china one.

This picture has its own page with more detail, click here to see it.

The porcelains that potters and traditional industry (sanitaryware, electrical insulators, common tableware) know and love are actually "mullite porcelains", named such because the fundamental source of strength (both fired and pyroplastic) is the needle-shaped mullite crystals that grow during the final stages of firing. The mug on the left is fired at 2200F and is made of high-feldspar Polar Ice. The kaolin crystals converted to mullite rather than dissolving in the feldspar glass.

Bone china, by contrast, is a calcium aluminosilicate glass-ceramic. It is "anorthite porcelain", relying on calcium from bone ash reacting with SiO2 and Al2O3 (from the kaolin and feldspar) to form anorthite crystals. The reward is strength and translucency (without brittleness), having fine and evenly dispersed crystals and outstanding density (no pores to scatter light). The refractive indices between the glass and crystal phases are also very similar, further preventing light scattering.

Both of these crystal types can be found in nature. But here, they are grown spontaneously during firing. Gradual recognition of these mechanisms was two centuries in the making, but not clear until the 1960s-1980s! Anorthite system mapping being the latter. Understanding and relationships with thermal expansion and translucency and kinetic control in fast-fire kilns has happened since then.

Zero3 casting porcelain at cone 04, 03


This picture has its own page with more detail, click here to see it.

Compared to a typical cone 6 porcelain, left, which has zero translucency, these are fired 10 cones lower. I am using the G3879 clear glaze and it is working very well.

A Lithophane exploits porcelain translucency to reveal its design


This picture has its own page with more detail, click here to see it.

Top: A thin porcelain tile with etched design. Bottom: The same tile with a back light. By Stephanie Osser. L3778G is an example of a translucent mullite porcelain that will work for this.

Now that is a translucent porcelain! But much more.


Polar Ice porcelain mug with a light inside to demonstrate its translucency

This picture has its own page with more detail, click here to see it.

These are two cone 6 transparent-glazed porcelain mugs. On the left is the porcelainous Plainsman M370 (Laguna B-Mix 6 would have similar opacity - none). Right is the highly vitreous, New Zealand kaolin-based porcelain, Polar Ice. The secret to making this porcelain super-white is the NZ kaolin. The secret of its impossibly high plasticity is the very expensive plasticizer, VeeGum T. What about the translucency? That is a little more complicated. Nepheline syenite is used as the feldspar, but it alone, in a practical recipe, cannot deliver this kind of translucency at cone 6. Amazingly, the 4% Veegum acts as a translucency catalyst; it is the real secret. Commercial manufacturers could never use a sticky and difficult-to-dry porcelain like this, but a potter can do incredible things with it (e.g. throw thinner, lighter, bigger than any other clay he/she has ever used!). Can you make this? Yes. Try the L3778D or L3778G recipes.

Inbound Photo Links


Bona china 3D printed mold pieces
Bone China Anti-Warp Setter test molds

Links

URLs http://home.howstuffworks.com/lenox.htm#
What is bone china and how is it made at howstuffworks.com
URLs https://www.instagram.com/reel/DZXXBa_iIdG
Studio slipcasting bone china mugs at https://www.repeatrepeat.co.uk in Stoke-On-Trent
Very interesting way to quickly cut handles to fit and the use of one-piece molds.
Glossary Fritware
A porcelain with significant added frit. The frit matures it at a far lower temperature than typical. The strength mechanism is one of particle glass bonding rather than mullite development.
Glossary Translucency
A highly sought-after property in porcelain, fired close enough to melting to take on the glass-like property of passing light. Translucency implies tendency to warp during firing.
Glossary Vitrification
A process that happens in a kiln, the heat and atmosphere mature and develop the clay body until it reaches a density sufficient to impart the level of strength and durability required for the intended purpose. Most often this state is reached near zero p
Glossary Stoneware
To potters, stonewares are simply high temperature, non-white bodies fired to sufficient density to make functional ware that is strong and durable.
Glossary Terra Cotta
A type of red firing pottery. Terra cotta clay is available almost everywhere, it is fired at low temperatures. But quality is deceptively difficult to achieve.
Glossary Plasticity
Plasticity (in ceramics) is a property exhibited by soft clay. Force exerted effects a change in shape and the clay exhibits no tendency to return to the old shape. Elasticity is the opposite.
Materials Bone Ash

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy