0.8mm thickness | 200 mesh | 325 mesh | 3D Design | 3D Modeling | 3D Printer | 3D Printing Clay | 3D Slicer | 3D-Printing | 42 mesh | A.I. in Ceramics | Abrasion Ceramics | Acidic Oxides | Agglomeration | AI at Digitalfire | Alkali | Alkaline Earths | All-in-one case mold | Amorphous | Apparent porosity | Artware | Ball milling | Bamboo Glaze | Base Glaze | Base-Coat Dipping Glaze | Basic Oxides | Batch Recipe | Bisque | Bit Image | Black Core | Bleeding of colors | Blender Mixing | Blunging | Body Bloating | Body glaze Interface | Body Warping | Bone China | Borate | Boron Blue | Boron Frit | Borosilicate | Breaking Glaze | Brick Making | Brushing Glaze | Calcia Matte | Calcination | Calculated Thermal Expansion | Candling | Carbon Burnout | Carbon trap glazes | CAS Numbers | Casting Slip | Casting-Jiggering | Catch Glaze | Celadon Glaze | Ceramic | Ceramic Binder | Ceramic Decals | Ceramic Glaze | Ceramic Glaze Defects | Ceramic Ink | Ceramic Material | Ceramic Oxide | Ceramic Slip | Ceramic Stain | Ceramic Tile | Ceramic Transfer | Ceramics | Characterization | Chemical Analysis | Chromaticity | Clay | Clay body | Clay Body Porosity | Clay Stiffness | Clays for Construction | Clays for Ovens and Heaters | Code Numbering | Coil pottery | Colloid | Colorant | Commercial hobby brushing glazes | Cone 1 | Cone 5 | Cone 6 | Cone plaque | Content Management System | Copper Red | Cordierite Ceramics | Crackle glaze | Creative Commons Attribution | Cristobalite | Cristobalite Inversion | CRM | Crucible | Crystalline glazes | Crystallization | Cuerda Seca | Cutlery Marking | Decomposition | Deflocculation | Dehydration | Differential thermal analysis | Digitalfire API | Digitalfire Foresight | Digitalfire Insight | Digitalfire Insight-Live | Digitalfire Reference Library | Digitalfire Taxonomy | Dimpled glaze | Dinnerware Safe | Dip Glazing | Dipping Glaze | Dishwasher Safe | Displacer | Do-It-Yourself | Drop-and-Soak Firing | Drying Crack | Drying Performance | Drying Shrinkage | Dunting | Dust Pressing | Earthenware | Efflorescence | Encapsulated Stain | Engobe | Eutectic | Fast Fire Glazes | Fat Glaze | FDM, SLA, SLS, MEX 3D printing technologies | Feldspar Glazes | Filter Press | Fining Agent | Firebrick | Fireclay | Fired Strength | Firing Schedule | Firing Shrinkage | Flameware | Flashing | Flocculation | Fluid Melt Glazes | Flux | Food Safe | Foot Ring | Forming Method | Formula Ratios | Formula Weight | Frit | Fritware | Functional | GHS Safety Data Sheets | GitHub | Glass vs. Crystalline | Glass-Ceramic Glazes | Glaze Blisters | Glaze Bubbles | Glaze Chemistry | Glaze Compression | Glaze Crawling | Glaze Crazing | Glaze Durability | Glaze fit | Glaze Gelling | Glaze laydown | Glaze Layering | Glaze Mixing | Glaze Recipes | Glaze shivering | Glaze Shrinkage | Glaze thickness | Globally Harmonized Data Sheets | Glossy Glaze | Green Strength | Grog | Gunmetal glaze | Hand Building Techniques | High Temperature Glaze | Hot Pressing | Incised decoration | Industrial clay body | Infill and Support | Ink Jet Printing | Inside-only Glazing | Iron Red Glaze | Jasper Ware | Jiggering | JSON | Kaki | Kiln Controller | Kiln Firing | Kiln fumes | Kiln venting system | Kiln Wash | Kneading clay | Kovar Metal | Laminations | Leaching | Lead in Ceramic Glazes | Leather hard | Limit Formula | Limit Recipe | Liner Glaze | Liner Glazing | Liquid Bright Colors | LOI | Low Temperature Glaze | Magnesia Matte | Majolica | Managed Service Provider | Marbling | Material Sense | Matte Glaze | Maturity | Maximum Density | MDT | Mechanism | Medium Temperature | Melt Fluidity | Melting Temperature | Metal Oxides | Metallic Glazes | Micro Organisms | Microwave Safe | Mineral phase | Mineralogy | Mocha glazes | Mohs Hardness | Mold Natches | Mold Shell Flange | Mole% | Monocottura | Mosaic Tile | Mottled | Native Clay | Non Oxide Ceramics | Oil-spot glaze | Once-Fire | Opacifier | Opacity | Ovenware | Overglaze | Oxidation Firing | Oxide Interaction | Oxide Molecular Formula | Oxide System | Particle classification | Particle orientation | Particle Size Distribution | Particle size reduction | Particle Sizes | PCE | Permeability | Phase Diagram | Phase Separation | Physical Testing | Pinholing | Plainsman Clays | Plaster Bat | Plaster table | Plasticine | Plasticity | Plucking | Porcelain | Porcelain Insulators | Porcelaineous Stoneware | Portable Document Format | Pour Glazing | Pour Spout | Powder Carrier | Powder Processing | Precipitation | Primary Clay | Primitive Firing | Propane | Propeller Mixer | Pugmill | Pyroceramics | Pyrometric Cone | Quartz Inversion | R2O:RO Ratio | Raku | Reactive Glazes | Reduction Firing | Reduction Speckle | Refiring Ceramics | Refractory | Refractory Ceramic Coatings | Representative Sample | Residual Quartz | Restaurant Ware | Rheology | Rutile Blue Glazes | Salt and Soda firing | Sanitary ware | Sculpture | Search Engine Optimization | Secondary Clay | Shino Glazes | Side Rails | Sieve | Sieve Shaker | Silk screen printing | Sintering | Slaking | Slip Casting | Slip Trailing | Slipware | Slurry | Slurry Processing | Slurry Up | Soaking | Soluble colors | Soluble Salts | Specific gravity | Splitting | Spray Glazing | Stain Medium | Stoneware | Stull Chart | Sulfate Scum | Sulfates | Surface Area | Surface Tension | Suspension | Tapper Clay | Tenmoku | Terra Cotta | Terra Sigilatta | Test Kiln | Theoretical Material | Thermal Conductivity | Thermal Expansion in Ceramic Bodies and Glazes | Thermal shock | Thermocouple | Thixotropy | Throwing | Tipping point | Tony Hansen | Toxicity | Trafficking | Translucency | Transparent Glazes | Triaxial Glaze Blending | Ultimate Particles | Underglaze | Unity Molecular Formula | Upwork | Variegation | Viscosity | Vitreous | Vitrification | Volatiles | Water Content | Water in Ceramics | Water Smoking | Water Solubility | Weathering of Clays | Wedging | Whiteware | WooCommerce | Wood Ash Glaze | Wood Firing | WordPress | Zero3 | Zero4 | Zeta Potential

Functional

A term used in ceramic to express the degree to which an item is safe and stands up to everyday use. Functionality embodies strength, hardness, resistance to acid attack and thermal shock, etc.

Key phrases linking here: functional - Learn more

Details

A functional clay body is one that produces a ceramic that is durable. However there are a number of caveats with this. First, the item must maintain that strength and durability in service (degradation is common e.g. because of water logging). Of course, the body has to be fired sufficiently high to vitrify enough to have strength considered to be suitable for the application. Second, if glazed, it needs to fit the glaze (and/or engobe). If the glaze is under compression or tension this can greatly weaken the body both immediately after firing and progressively over time as micro-crack networks grow and water penetrates into available porosity.

Absorption of a fired clay is a key factor in functionality of ware made using it. There is no specific absorption rate that indicates functionality, however obviously more dense ware will be more durable. Absorption is a product of porosity in the body. Obviously a body having micro-cracks as porosity is not going to be as strong as one having normal inter-particle pore space. Porosity is typically a product of the nature of the pore space which in turn is a product of the nature of the matrix that hosts it. Pore shape and inter-connections and the micro-porosity of the ceramic matrix determine the degree to which water can penetrate to fill it. Thus a body may have a much higher porosity than a standard porosity test indicates if the pore-interconnects are lacking. Many potters, for example, assume that higher temperatures produce more functional ware. But this is not necessarily true. The body must fire vitreous for strength and durability and the degree to which it vitrifies is determined by the recipe, not the temperature. High temperature red burning iron ware bodies are an example of bodies producing ware of questionable functionality, they fire porous by necessity to achieve the desired variegated red/brown coloration.

One body having a higher porosity can also be stronger than another having a lower porosity, this can be the case for several reasons. First, the nature of the matrix that hosts the pore network can be a greater determiner of overall strength than the simple existence of pores. A matrix having large silica particles with cracks radiating outward (because of quartz inversion during firing) will obviously not be strong. Also, a well fitted, impermeable glaze can greatly strengthen a body. Many glazed ceramic tiles, for example, are remarkably strong, yet they can have a high porosity. Also, one body of higher porosity may have a matrix that better terminates the growth of micro-cracks than another, and thus maintain its strength over time better.

Functional glazes on food surfaces hold up over time, they do not scratch or stain or mark or fade or craze. This is because they are hard, smooth and resistant to leaching. Glazes on all surfaces are defect free and have a thermal expansion compatible with the body. This does not happen by accident. These glazes are balanced chemically, having enough SiO2 and Al2O3 to build a strong glass, they are not saturated with colorants (like metal oxides), crystallizers or variegators (like rutile, titanium). This site is dedicated to giving technicians the tools and knowledge they need to make functional ware.

An excellent test of functionality is to simply begin using a mug in your kitchen. Pour hot coffee in it every day, bang it around and put it in the dishwasher with the rest of the dishes. Look for crazing over time and changes in the ring it makes when tapped with a spoon (indicating water logging or micro-crack propagation) and changes in the glaze surface (glossy or marking or staining or crazing).

Related Information

Looking for a non-crazed non-cutlery marking cone 10R dolomite matte?


This picture has its own page with more detail, click here to see it.

This is G2571A cone 10R dolomite matte on an ironware body made from native North Carolina clays. Few glazes have the pleasant silky feel that this has yet are still functional. The feldspar content in the body has been tuned to establish a compromise between the warmer color that low percentages have with the higher strength that higher percentages enable. Careful porosity tests were done and recorded in an account at insight-live.com. The objective was to bring the body close to 3% absorption.

What is the secret to cool and functional clay bodies and glazes?


This picture has its own page with more detail, click here to see it.

The secret to cool and functional bodies and glazes is a lot of testing.
The secret to know what to test is material and chemistry knowledge.
The secret to learning from testing is documentation.
The place to document is an account at insight-live.com.

Commercial supposedly-safe glazes leaching. A liner glaze is needed.


Leaching commercial pottery glaze

This picture has its own page with more detail, click here to see it.

Three cone 6 commercial bottled glazes were layered inside this mug, which was then filled with lemon juice overnight. The whitened, altered areas show that the glaze surface has been attacked by the acid. Even if glaze A, B and C have each passed a fired-surface release test individually, A-over-B-over-C is a new fired glass composition and microstructure. The individual certifications do not logically constitute a test of that combination. The color change suggests attack on cobalt-bearing glass, but exactly what is leaching cannot be known without testing because the recipes are proprietary. For functional ware, it is better to use a stable transparent or white liner glaze whose recipe and limits are known.

When manufacturers say their products conform to standards such as ASTM D-4236, they are referring to the safety labeling of the liquid art material for the user of the product, not guaranteeing that layered fired surfaces on finished ware will be leach-resistant

The best firing temperature for this middle range body?


This picture has its own page with more detail, click here to see it.

This cone 6 brown functional stoneware has been fired across a range of temperatures. Cone 4 is too porous. From cone 7 it is expanding and density is not improving, it will likely warp or bloat. Cone 7 is losing the red color, there is no room for over-firing (by accident). The porosity at cone 6 is so much better than cone 5 and color is still stable. Therefore, cone 6 is the one we want.

Bamboo glaze that is actually functional


This picture has its own page with more detail, click here to see it.

The stunning cone 10R Ravenscrag bamboo glaze (it is GR10-J plus 0.5% iron oxide) on a Grolleg porcelain. Up close it can feel and look like a fine wood surface (when used on a porcelain).

Can a glaze act as a sealant?

Yes. But only if it fits.


This picture has its own page with more detail, click here to see it.

Left: Plainsman M340 fired to cone 6 where it achieves good density (about 2% porosity) and excellent strength. Fire it to 1% porosity and it will bloat and warp. So cone 6 is its practical optimal temperature. Being able to measure the 2% porosity demonstrates water penetration, albeit slow penetration. So glazes must fit to seal the surface.

Right: H550, a Plainsman body intended to mature at cone 10, but fired to cone 6 using the same glaze. The clay is much more porous. The piece was dropped and cracked (the crack runs diagonally down from the rim). It was then dipped into water for a few moments. Immediately the water penetrated and began to soak into the body (spreading out from the crack). If this glaze were to craze, the entire thing would be waterlogged in minutes. But it doesn’t craze. So, the piece would be usable (with a sealed foot ring of course).

Water-logging happens when a clay is underfired


This picture has its own page with more detail, click here to see it.

The cone 6 glaze is well developed; it is not crazed. But the clay underneath is not vitreous. This crack happened when the mug was bumped. It is barely visible. But when the mug was filled with water, this happened. How fast? This picture was taken about 5 seconds later. If this were crazing, and this piece was in actual use, the clay would become completely waterlogged. Then one day, someone would put it in the microwave. Boom!

This being said, if the glaze never crazes, the foot ring is sealed and the piece never cracks, this mug could service for years.

We fight the dragon that others do not see


This picture has its own page with more detail, click here to see it.

There are thousands of ceramic glaze recipes floating around the internet. People dream of finding that perfect one, but they often only think about the visual appearance, not of the usability, function, safety, cost or materials. That resistance to understanding your materials and glazes and learning to take control is what we personify as the dragon. Using the resources on this site you could be fixing, adjusting, testing, formulating your own glaze recipes. Start with your own account at insight-live.com.

Links

Glossary Vitrification
A process that happens in a kiln, the heat and atmosphere mature and develop the clay body until it reaches a density sufficient to impart the level of strength and durability required for the intended purpose. Most often this state is reached near zero p
Glossary Microwave Safe
Microwave safety is a concern in the production of function ceramic ware.
Glossary Food Safe
Be skeptical of claims of food safety from potters who cannot explain or demonstrate why. Investigate the basis of manufacturer claims and labelling and the actual use to which their products are put.
Glossary Maturity
A term used in ceramics to signify the degree of vitrification in a fired clay. Mature clays are dense and strong; immature ones are porous and weak.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy