| Monthly Tech-Tip | No tracking! No ads! |
How would you like to be able to create a parametric CAD model of a teapot lid? Then 3D print a case mold and pour a multi-piece plaster working mold? Imagine easily making multiple-size one-off molds to accommodate any teapot you throw!
This is perfect for M370 or Polar Ice (both have throwing and casting versions). Or, how would you like to be able to formulate a casting slip having the same appearance and degree of maturity as the throwing body you use? More information coming soon (based on the L4807 casting body).
Next, imagine casting the handles, rims and spouts also. Information on how to draw and print them also coming soon.
Available on the Downloads page

This picture has its own page with more detail, click here to see it.
Once you try these you will never go back to the use of registration keys in traditional mold making. Unfortunately, these natches are not easy to get in North America. Or even online. But you can 3D print them yourself (we use PLA filament, but TPM would be a good option). This design interlocks with standard 3/8" natches used in industry. There are more aspects to printing and using these than meets the eye. Here are some things we noted (and changed):
-The base can be widened for sticking on the build plate better.
-Glue the build plate, on your 3D printer, to make sure these stick well.
-The inner edge is chamfered to ensure better insertion of the nipple.
-Print without infill for better strength.
-These are hollow, no print support is needed.
-The bottom can be widened to stick better to the build plate.
-The ribs can be moved.
-A 9.8 mm hole is needed in the mold.
Once we moved to the use of CAD and 3D printing of block and case molds, these were abandoned in fovor of a four-part system.

This picture has its own page with more detail, click here to see it.
Rather than L4807 being just another cone 6 porcelain casting slip recipe it is a pattern of the flexibility potters/hobbyists could have in making their own bodies. We’ve never seen another body that can match how easily this deflocculates and its incredible casting speed. Don’t let anyone tell you that porcelains have to be difficult to cast.
Typical slips made from ball clay and talc (or mixes of common feldspars, clays and quartz) take 20-30 minutes to get the needed thickness (in our circumstances and assuming a new dry mold). But this one poured out in 12 minutes. We are used to extracting pieces in 30-60 minutes, with this clay I can demold in 10 minutes. The secret is not the recipe, it is similar to a typical 25-porcelain. The secret is choice of kaolin and ball clay. It employs OptiKast Kaolin and KT#1-4 ball clay, both are large particled clays targeted at slip casting.
Buy me a coffee and we can talk