The body is Plainsman M390. The firing schedule is Plainsman PLC6DS. The tin is on the right.

This picture has its own page with more detail, click here to see it.
This melt fluidity tester demonstrates that the cone 6 G1214Z recipe fires highly melt fluid, much more than one might expect from a matte glaze. When applied as a thin layer on pottery it does behave as a matte glaze. A quick look at its chemistry reveals the reason: High CaO and a low Si:Al ratio. Unfortunately, many matte glaze are such simply because they are not melted enough.
| Glossary |
Opacifier
Glaze opacity refers to the degree to which it is opaque. Opacifiers are powders added to transparent ceramic glazes to make them opaque. |
| Materials |
Zircon
|
| Materials |
Tin Oxide
Its principle use in ceramics is as an opacifier in glazes. It is very expensive. |
| Recipes |
G1214Z1 - Cone 6 Silky CaO matte base glaze
This glaze was born as a demonstration of how to use chemistry to convert a glossy cone 6 glaze into a matte. |