The fired pieces appear to be made from black porcelain. But this is L3954F cone 6 black engobe over a white porcelain. Multiple factors make this work. First, a non-gummed dipping engobe will not work for this (it will not apply by brush evenly or thickly enough). This brushing version mixes 500 grams of L3954F powder (with black stain) into 280g water and 75g of Laguna Gum Solution. Second, the engobe recipe is tuned to have the same degree of vitrification as the body, in this case M370, so pieces don’t stick to the kiln shelf during firing. Of course, this procedure rewetted the bases of the leather hard mugs, extending drying time so extra precautions were needed to avoid cracking. For example, I painted wax emulsion on the handle outers and covered them all in cloth and plastic for a day to slow down drying.

This picture has its own page with more detail, click here to see it.
To prove that using an engobe is the best way to make a black cone 6 stoneware clay surface consider the mug on the left, a version of L4768E. This is not the best way but it is the one most used (and what Plainsman Clays does with Coffee Clay). This is a DIY mix, the darkest that it is practical (I used the hyper-red burning C-Red clay as a base, thus needing much less umber to darken it). While it looks black beside red burning bodies, beside this true black it doesn't, First, it is not a body, it is just a thin veneer of stained porcelain engoben (if the surface is all we see why stain it all the way through?). That being said, some people need a totally black and safe clay, like this one, and can afford to make it themselves (if that is you try using the L4053B recipe as a starter). Get a plaster table and a propeller mixer and you will be unstoppable!
What about using metal oxides to make the engobe? Black stain is expensive but is far superior (and safer) for black. Consider using 10-15% colorant in this 500g mug, which would require 50-75 grams of stain (~$5-8). 10% stain in an engobe applied in this thin layer likely needs only a few grams of stain (for pennies of cost). What about using a commercial black underglaze? There are normally vitreous, would stick to a kiln shelf and not cover evenly like this.
Buy me a coffee and we can talk