Robert has done really valuable work in this research, what an amazing range of color! Surfaces are unpolished and unglazed. All are fired to cone 6. Browns are missing, they can be made using iron oxide. For blacks, Mason 6600 is also effective. The blues can be intense using lower percentages than shown here, as low as 2% can be effective. There is an optimal amount for each stain, beyond that, increases in percentage bring little increase in color intensity. There is another reason to keep stain percentages to a minimum: To reduce the impact on body maturity (and firing shrinkage). Blues, for example, can significantly heighten the degree of vitrification, even melting the porcelain. If you plan to marble different colors, keeping stain percentage as low as possible is even more important, unless you can do fired shrinkage compatibility testing, for example, the EBCT test. Need to develop your own white porcelain? See the link below.
Stains in bodies will usually bleed color into glazes used over them, especially if the body is vitreous. This can be leveraged to create or amplify variegation. Strangely, stains can increase micro bubbles in transparent glazes.

This picture has its own page with more detail, click here to see it.
Fired to cone 6. These are not glazed. Polar Ice is very vitreous and very white, an ideal host for stains. You can make a very similar porcelain yourself using the L3778D recipe (you just need a propeller mixer and plaster table). However, there is a caution: If a stain is refractory, it can reduce the firing shrinkage of the porcelain considerably. On the other hand, some stains will flux bodies and do the opposite. That means if high and low shrinkage stained versions of Polar Ice are laminated or marbled, the firing can create a tension-time-bomb that either exits the kiln cracked or cracks down the road. Of course, a polished surface would not be suitable for food or drink surfaces if the porcelain is being stained by an inclusion pigment containing cadmium or other known hazardous metal. This work is courtesy of Robert Barritz.

This picture has its own page with more detail, click here to see it.
This is L4588 red burning porcelain. I got the idea after coffee break and was rolling and pressing specimens right after lunch.
10.30 am: I got the idea to make this, created a record in my Insight-live account, code-numbered it and printed the recipe.
10.35 am: I started weighing it out.
10.40 am: I blender mixed it really well to remove all agglomerates.
10.45 am: I poured it onto my plaster bat.
12.30 pm: It had stiffened to the perfect consistency to roll a couple of SHAB test bars and press and stamp some porcelain theme rocks.
Next day: In the kiln. Next day: Incredible red porcelain at cone 6.
Much of the reason not to be intimidated by mixing tests like this is having all the tools and materials close at hand and a good record-keeping system. And making sure to enter results, notes and pictures as tests are completed. And linking this to related tests (I am also working on a pink and a blue).
| Materials |
Spectrum 2276 Yellow Stain
|
| Materials |
Mason 6464 Yellow Stain
|
| Materials |
Mason 6485 Yellow Stain
|
| Materials |
Mason 6537 Grey Stain
|
| Materials |
Mason 6386 Blue Stain
|
| Materials |
Mason 6600 Black Stain
A cobalt-containing stain useful in bodies, engobes and glazes at a wide range of temperatures. |
| Materials |
Stain 6121
|
| Materials |
Stain 6201
|
| Materials |
Stain 6219
|
| Materials |
Stain 6234
|
| Materials |
Stain 6200
|
| Materials |
Mason 6255 Stain
|
| Materials |
Mason 6266 Stain
|
| Materials |
Frit VO 6200
|
| Materials |
Frit VO 6255
|
| Materials |
Mason 6363 Stain
|
| Materials |
Mason 6304 Violet Chrome Tin
An encapsulated purple stain. Purple is very difficult in ceramic glazes and this stain delivers incredible color in glossy glazes. |
| Materials |
Mason 6308 Stain
|
| Materials |
Mason 6306 Stain
|
| Materials |
Mason 6368 Copen Blue Stain
|
| Materials |
Stain 6388
|
| Materials |
Mason 6027 Stain
|
| Materials |
Mason 6021 Red Stain
An encapsulated red stain, it has proven better than any other red we have ever tried for glazes. And it works in bodies. |
| Glossary |
Ceramic Stain
Ceramic stains are manufactured powders. They are used as an alternative to employing metal oxide powders and have many advantages. |
Buy me a coffee and we can talk