The top bars went to cone 10R, the others are cone 11 and 10 oxidation (downward from top). They are Gleason, Spinks Blend, OM#4 and NP Blend. It is amazing now similar different ball clays fire in the kiln. Clearly, soluble salts are an issue with all of them (the brownish scum). These bars are much cleaner on the backsides (since the solubles were left on the surface on the fronts during drying). The drying shrinkages, plasticities and fired maturities are also all remarkably similar.
| Minerals |
Ball Clay
Ball clay is the most common type of secondary clay. They are much more plastic than kaolin because |
| Glossary |
Porcelaineous Stoneware
In ceramics, porcelains lack plasticity and fire to high density with white, glassy surface. Stonewares are plastic and fire cream to brown and lower density, Porcelaineous stoneware are between these two. |
| Materials |
Ball Clay
A fine particled highly plastic secondary clay used mainly to impart plasticity to clay and porcelain bodies and to suspend glaze, slips and engobe slurries. |
Buy me a coffee and we can talk