These mugs are Plainsman H450 fired at cone 10R. Both have a black engobe (L3954N) applied to the insides and half way down the outside during leather hard stage (the insides are glazed with Ravenscrag silky matte and G1947U over the black engobe). The bamboo glazes can thus be seen over the black (upper half) and the raw buff body (lower). The bamboo glaze on the left has 1% iron added to the base G2571A recipe. The one on the right has 3.5% powdered rutile and 10% zircopax added.
| Recipes |
L3954N - Cone 10R Base White Engobe Recipe for stonewares
Cone 10 reduction black engobe for stonewares (not porcelains). |
| Recipes |
GR10-J1 - Ravenscrag Cone 10R Bamboo Matte
Plainsman Cone 10R Ravenscrag Slip based glaze. It can be found among others at http://ravenscrag.com. |
| Recipes |
G2571A - Cone 10 Silky Dolomite Matte glaze
A cone 10R dolomite matte having a pleasant silky surface, it does not cutlery mark, stain or craze on common bodies |
| Glossary |
Bamboo Glaze
A high temperature reduction glaze made by adding a small amount of iron oxide to a magnesia matte base glaze |
| Materials |
Ceramic Rutile
Rutile mineral ground to a very fine particle size (e.g. 325 mesh) contributes titanium and iron that colors and variegates ceramic glazes. |