| Monthly Tech-Tip | No tracking! No ads! |
Management now thinks they can outsource his technical work. Danny was good, but he didn’t build a centralized, searchable record of material testing, shipment histories, specs, production problems, and solutions. Instead, his knowledge is buried in thousands of Excel and Word docs and PDFs. He should have used Insight-Live.com to organize, interlink, and preserve this critical data. Sadly, the company does not even realize what they face without Danny:
Had Danny been not just a watchdog but a technical innovator, suppliers and consultants would have been secured to support—not replace—his in-house expertise.

This picture has its own page with more detail, click here to see it.
A kaolin shipment just came in. "UnReady Freddie" is panicking. He thinks he remembers that products made with the last shipment were lacking plasticity and the fired color was off. He is going to have to come up with different lame excuses for complaining customers this time.
"Ready Freddie" has Insight-Live and has collected years of data on incoming shipments in one searchable place. He knows what to check on each and has fired bars, in-mix tests, particle size checks, data sheets, lots of pictures, notes, etc. He also has traceability - he knows what material batch went into what product. He works with production to do material lot tracking and with purchasing to keep suppliers aware he is testing. Because Ready Freddie knows how materials vary he can compensate recipes and processes so customers see a consistent product.
UnReady Freddie has a few spreadsheets somewhere. But he is busy with other things. Who do you want in charge of product consistency (and company reputation)? Here is what to do next: Have your technician study the page "Testing a New Load of EP Kaolin" (link below). You will be hearing from him/her soon.

This picture has its own page with more detail, click here to see it.
He is the lone quality technician, part time. Incoming materials properties keep changing, but management pretends they aren't. Freddie is tired of dealing with what could be lurking in these pallets—grit and fired specks, drying cracks, warping, blistering - he's flying blind. It’s just a matter of time before something fails… and his name is on it! But there is a way to start "owning the problem" by starting QC small (using Insight-live):
-Number the pallets with a big marker.
-Add a new record in Insight-live, assign a new code number and date and link it to a specification.
-In the notes, log lot numbers from the bags and any pertinent details (e.g. supplier invoice, PO#).
-Upload supplier certificate photos.
-Grab samples through the bag spouts— one per lot or pallet.
-Do testing for oversize particles (especially in clays).
-Make SHAB test bars (for clays). Dry them in a dehydrator and fire them overnight (because production wants to start using this tomorrow!).
-Snap close-up photos of the fired bars and upload and annotate them for future comparison.
This is survivable QC. It won’t fix everything. Now he is Ready-Freddie, with a solid plan to stand on when the blame starts flying. Maybe he will even be able to establish coordination between sales, production, and QC (using a group account) and even refine the specifications and procedures for each material type.
Made using a simple prompt at ChatGPT.This picture has its own page with more detail, click here to see it.
Management says AI can do most of the technical work now. Tommy had no automation, no models, no data pipelines. Just “the way we’ve always done it,” trapped in spreadsheets and sticky notes. When the new AI system went live, his expertise didn’t plug in. It got left behind!
Technicians aren’t just there to keep things running—they should teach the future how to work. Refusing to adapt doesn’t protect your job. It writes your own pink slip.
Buy me a coffee and we can talk