Original development of the G2896 recipe was done to match the chemistry of Randy's Red (a popular recipe). At the time we did not do any special firing schedule to encourage the growth of the red crystals.

This picture has its own page with more detail, click here to see it.
| Recipes |
G2826X - Randy's Red Cone 5
A popular Gerstley Borate based iron-red glaze. |
| Recipes |
G2896 - Ravenscrag Plum Red Cone 6
Plainsman Cone 6 Ravenscrag Slip based iron-red glaze. It can be found among others at http://ravenscrag.com. |
| Glossary |
Iron Red Glaze
A type of ceramic glaze, typically fired around 2200F, where iron oxide in the cooling glass precipitates out to form a striking red crystalline mesh on the surface. |