| Monthly Tech-Tip | No tracking! No ads! |

This picture has its own page with more detail, click here to see it.
Original development of the G2896 recipe was done to match the chemistry of Randy's Red (a popular recipe). At the time we did not do any special firing schedule to encourage the growth of the red crystals.
| Recipes |
G2826X - Randy's Red Cone 5
A popular Gerstley Borate based iron-red glaze. |
Buy me a coffee and we can talk