This sanitary ware tank lid was made in China. Notice how thick the white glaze is being applied to cover the iron containing body below. This is a testament to how opaque a zircon opacified glaze can be. Zircon often causes crawling (likely due to a combination of the effects of its fine particle size on drying properties and its tendency to stiffen the melt). Extra measures and constant attention to detail (e.g. glaze thickness, slurry rheology, avoidance of sharp contours on ware) are needed with such glazes.
| Materials | Zircon | 
| Glossary | Opacifier Glaze opacity refers to the degree to which it is opaque. Opacifiers are powders added to transparent ceramic glazes to make them opaque. | 
| Glossary | Sanitary ware A type of porcelain zircon-glazed ceramic that includes bathtubs, sinks, toilets, etc. | 
| Troubles | Crawling Ask yourself the right questions to figure out the real cause of a glaze crawling issue. Deal with the problem, not the symptoms. | 