L3724F fluxed terra cotta slip applied over a white burning stoneware (L3685R) fired at cone 03. Most slips in use are not adequately fluxed and do not adhere well to the body below. The frit in this one attaches much better and even enables it to develop a sheen. Also, because of its volatility of color in the cone 03 range, variations in the shade and degree of sheen will impart an appearance like flashing.
| Recipes |
L3724F - Cone 03 Terra Cotta Stoneware
An experimental Zero3 using Plainsman 3D clay |
| Recipes |
L3685U - Cone 03 White Engobe Recipe
A white burning body with enough added frit to produce a cone 03 stoneware or white slip for use on the matching red Zero3 stoneware. |