| Monthly Tech-Tip | No tracking! No ads! |
Notice the inside of this large transparent glazed cone 6 stoneware bowl. There is a concentration of specks on one part because that area was sponged at the leather hard and dry stages to smooth surface problems that happened during the jiggering process. These specks are normally driven below the surface during forming.
| Troubles |
Specking on Ceramic Ware
Specking, or speckling, can be both a fault or feature in fired ceramic ware - caused or produced by metal-bearing contaminants to metallic additives |
| Glossary |
Stoneware
To potters, stonewares are simply high temperature, non-white bodies fired to sufficient density to make functional ware that is strong and durable. |
| Glossary |
Jiggering
Jiggering is a process of forming pottery that employs a spinning plaster mold and a tapered template to press soft clay or porcelain against it. |