| Monthly Tech-Tip | No tracking! No ads! |
This is the standard Plainsman L3954D white engobe recipe with the 10% Zircopax switched for Burnt Umber. The result is a dark, rich, ultra-gloss brown (almost black). The engobe is applied inside and half-way down the outside. The mug on the left is glazed inside and out with the base GA6A Alberta Slip cone 6 recipe (but uses Ferro Frit 3195 instead of 3134). The one on the right has the same glaze on the outside but the G2926B clear transparent on the inside (it is micro-bubbling). This engobe works even better with a black stain.
| Recipes |
L3954B - Cone 6 Engobe (for M340)
Dry and firing shrinkage fitted to Plainsman M390, M340 |
| Materials |
Burnt Umber
|