We want to achieve embossed lettering inside the foot rings of slip-cast ceramic pieces by using a standard consumer 3D printer with PLA filament. There are plenty of obstacles to overcome in doing this. Since plaster does not release well at all from lettering having sharp corners, bevelling has to be done. However, our CAD software has problems rounding the corners of many fonts, I had to search for one having no variations in stroke width. Then it was a matter of discovering how much to extrude and how much bevelling it would tolerate - this one permits a 1 mm extrusion with a 0.6 radius bevel.
Left front: A 1mm extrude without bevelling and cold release produced very poor results.
Centre: 1mm extrude, 0.6 radius bevelling, 0.2mm rise of background to minimize verticals and cold release - better but still problems.
Right: Same as center but released with heat gun - almost perfect.
Bottom: A test casting from the first prototype mold - looking really good (albeit backwards!).
| Projects |
2019 Jiggering-Casting Project of Medalta 66 Mug
My project to reproduce a mug made by Medalta Potteries more than 50 years ago. I cast the body and handle, jigger the rim and then attach the handle. 3D printing made this all possible. |