It is now practical to make true-round, perfect-fitting, all-in-one case molds for jiggering using a consumer 3D printer and PLA filament. This was a one-off test mold to demonstrate the method but these print so fast this is suitable to make dozens of molds. The process: Create the drawing in 3D CAD (e.g. Fusion 360), print the three sections, glue them, turn the assembly upside down, fill with plaster, let it set and peel out the inside two pieces using a heat gun.
Things to note:
-The outside diameter can be adjusted to fit the ring on any jigger machine or cuphead.
-This is very light and prints quickly, the walls are only 0.8mm thick.
-The shoulder (C) is printed solid and the PLA printed surface from A to D is left in place permanently, this enables precise and durable fit into the cuphead. I print the outside shell upside down, so no printed support is needed.
-The down-pointing flange (A) embeds it into the plaster providing a durable edge against which to fit the pour spout (F). The glue joint connecting A & B breaks when B & E are removed.
-B and E are printed upside down, no support is needed for B, since the top is open, it thus prints quickly.
-The base E has a flange that enables gluing it precisely into B. Debossed logos are practical. It prints upside down for maximum quality (print support is generated but because it is short it prints quickly).
You can get this on the downloads page.
Available as a Product on the Downloads page
Available on the Downloads page

This picture has its own page with more detail, click here to see it.
Once you try these you will never go back to the use of registration keys in traditional mold making. Unfortunately, these natches are not easy to get in North America. Or even online. But you can 3D print them yourself (we use PLA filament, but TPM would be a good option). This design interlocks with standard 3/8" natches used in industry. There are more aspects to printing and using these than meets the eye. Here are some things we noted (and changed):
-The base can be widened for sticking on the build plate better.
-Glue the build plate, on your 3D printer, to make sure these stick well.
-The inner edge is chamfered to ensure better insertion of the nipple.
-Print without infill for better strength.
-These are hollow, no print support is needed.
-The bottom can be widened to stick better to the build plate.
-The ribs can be moved.
-A 9.8 mm hole is needed in the mold.
Once we moved to the use of CAD and 3D printing of block and case molds, these were abandoned in fovor of a four-part system.

This picture has its own page with more detail, click here to see it.
I print these using PLA filament, they are strong enough for hobby or studio use (even if not printed solid). The knife-edge prints precise and smooth, there is no need for sanding. Notice that the drawing (far left) includes the contours of the inside and outside of the mug. Making the jigger template only requires adding three straight lines. Then I extrude it forward 1cm and add a 30-degree draft. The top edge can, of course, be extended upward to mount in the jigger arm. The working template has to be narrower than this at the bottom to clear the edge when the jigger arm is lowered. For use in hand-finishing the slip cast mugs (without a jigger arm) it is suitable like this.
Available on the Downloads page

This picture has its own page with more detail, click here to see it.
I have long wanted an easy way to make molds for slipcasting handles that mate perfectly to specifically shaped and sized mugs (or pitchers, teapots, etc). These are the answer. These shells print quickly to only 11 grams of PLA filament. They peel away from the set plaster with a heat gun to give fine detail and a perfect fit. These use 3D-printed pour spouts instead of a mold spare (printed separately) and enable cutting the joint surface cleanly and accurately before the handle is removed from the mold (a version of this is also available with spares). This is the product of a long development process. This drawing is available on the downloads page.
Worried about mixing or tuning your own casting slip recipe? We have lots of help on doing that. As motivation, consider the benefits of mass producing handles and store them in a wet box with the attachment slip.
| Glossary |
0.8mm thickness
This is an ideal wall thickness to print on consumer 3D printer since to normally creates sufficient strength and prints in one two passes |
| Glossary |
All-in-one case mold
A method of 3D printing the case mold shell of an entire assembled plaster mold for using in ceramic production. |
| Glossary |
3D-Printing
Standard 3D printing technology (not printing with clay itself) is very useful to potters and ceramic industry in making objects that assist and enable production. |