These are SHAB test bars prepared from two different shipments of the same commercial kaolin (used in porcelain body production). The darker one is markedly more plastic also. This underscores the need to characterize the materials you use in production and maintain an ongoing testing program. This difference was actually easy to deal with: Reduction of the percentage of bentonite in the body.

This picture has its own page with more detail, click here to see it.
A shipment EP Kaolin has arrived for use in some of our production porcelain and stoneware bodies. Of course, this needs to be tested before being put into product. But how? The first step is to create a new recipe record in my Insight-Live account, and find their production date code stamp on the bag. Hmmm. It does not have one! OK, then I need to record the date on which we received it. We need to save a bag on every pallet and sieve 50 grams through 100 mesh (to spot contamination). Then we'll make test bars (of all the samples mixed) to fire across a range of temperatures (to compare fired maturity with past shipments). We do a drying performance disk also to assess soluble salts.
| Articles |
Simple Physical Testing of Clays
Learn to test your clay bodies and clay materials and record the results in an organized way, understanding the purpose of each test and how to relate its results to changes that need to be made in process, recipe and materials. |
Buy me a coffee and we can talk