These are table salt crystals on a 60 mesh sieve. It has an opening of 250 micro meters (or microns). Half of the crystals passed this sieve, half are retained. Notice on the right, several crystals are in the openings, about to fall through. Imagine that a particle (or crystal) of bentonite or ball clay can be sub-micron in diameter, they can actually be 2500 times smaller on a side than these salt crystals! One-tenth-micron ultimate particles would thus fit 2500x2500 on the flat side of a salt crystal. And, since the clay crystal is much thinner than wide, perhaps ten could stack to the same dimension. That means theoretically 2500x2500x25000 (or 1 with eleven zeros) could pack into a grain of salt!
| Glossary |
Sieve
Sieves are important in ceramics for removing particulates and agglomerates from glaze, engobe and body slurries. |
| Glossary |
Ultimate Particles
Utlimate particles of ceramic materials are finer than can be measured even on a 325 mesh screen. These particles are the key players in the physical presence of the material. |
| Glossary |
Particle Size Distribution
Knowing the distribution of particle sizes in a ceramic material is often very important in assessing its function and suitability for an application. |
| Glossary |
Particle Sizes
Knowledge of the physical and ultimate particles sizes in ceramic minerals and materials is an important part of understanding them, predicting their usefulness and explaining their behavior. |